daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Effect of Porogen on Acid-Activated Rare Earth Tailings-Based Molded NH3-SCR Denitration Catalyst AITranslate

Collaborative Innovation Center of Integrated Exploitation of Bayan Obo Multi-Metal Resources,Key Laboratory of Green Extraction&Efficient Utilization of Light Rare-Earth Resources of Ministry of Education,School of Energy and Environment,Inner Mongolia University of Science and Technology;Collaborative Innovation Center of Integrated Exploitation of Bayan Obo Multi-Metal Resources,Key Laboratory of Green Extraction&Efficient Utilization of Light Rare-Earth Resources of Ministry of Education,School of Energy and Environment,Inner Mongolia University of Science and Technology;Collaborative Innovation Center of Integrated Exploitation of Bayan Obo Multi-Metal Resources,Key Laboratory of Green Extraction&Efficient Utilization of Light Rare-Earth Resources of Ministry of Education,School of Energy and Environment,Inner Mongolia University of Science and Technology;Collaborative Innovation Center of Integrated Exploitation of Bayan Obo Multi-Metal Resources,Key Laboratory of Green Extraction&Efficient Utilization of Light Rare-Earth Resources of Ministry of Education,School of Energy and Environment,Inner Mongolia University of Science and Technology;Collaborative Innovation Center of Integrated Exploitation of Bayan Obo Multi-Metal Resources,Key Laboratory of Green Extraction&Efficient Utilization of Light Rare-Earth Resources of Ministry of Education,School of Energy and Environment,Inner Mongolia University of Science and Technology;Collaborative Innovation Center of Integrated Exploitation of Bayan Obo Multi-Metal Resources,Key Laboratory of Green Extraction&Efficient Utilization of Light Rare-Earth Resources of Ministry of Education,School of Energy and Environment,Inner Mongolia University of Science and Technology;Collaborative Innovation Center of Integrated Exploitation of Bayan Obo Multi-Metal Resources,Key Laboratory of Green Extraction&Efficient Utilization of Light Rare-Earth Resources of Ministry of Education,School of Energy and Environment,Inner Mongolia University of Science and Technology;Collaborative Innovation Center of Integrated Exploitation of Bayan Obo Multi-Metal Resources,Key Laboratory of Green Extraction&Efficient Utilization of Light Rare-Earth Resources of Ministry of Education,School of Energy and Environment,Inner Mongolia University of Science and Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites Download PDF

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

To enhance the denitration performance of acid-activated molded NH3-SCR denitration catalysts,using rare earth tailings as raw materials,various porogens(starch,polyethylene glycol,ammonium carbonate,activated carbon)were added to the sulfuric acid-activated and microwave-treated powdered catalyst,and then NH3-SCR denitration catalysts were prepared by extrusion molding.The effects of different types and dosages of porogens on the denitration activity,compressive strength,specific surface area,pore structure,phase composition,and redox capacity of the catalysts were investigated using NH3-SCR tests,Xray diffraction,specific surface area measurement,and H2 temperature-programmed reduction.The optimal type and dosage of porogen were determined accordingly.The results show that adding 5.0%by mass of polyethylene glycol results in the relatively optimal denitration performance of the molded catalyst,which exhibits a specific surface area of 3.70 m2/g,a total pore volume of 0.0308 cm3/g,and a denitration efficiency of 74.0%at 350℃.It also demonstrates high N2 selectivity,compressive strength,and redox capacity.Compared to the catalyst without any porogen,the denitration performance is significantly improved.

KeyWords AITranslate

porogen acid-activation rare earth tailings NH3-SCR catalyst denitration polyethylene glycol
No data

Basic Information:

DOI:

Chinese Library Classification Number:TQ426.98[化学工程]

Citation Information:

To enhance the denitration performance of acid-activated molded NH3-SCR denitration catalysts,using rare earth tailings as raw materials,various porogens(starch,polyethylene glycol,ammonium carbonate,activated carbon)were added to the sulfuric acid-activated and microwave-treated powdered catalyst,and then NH3-SCR denitration catalysts were prepared by extrusion molding.The effects of different types and dosages of porogens on the denitration activity,compressive strength,specific surface area,pore structure,phase composition,and redox capacity of the catalysts were investigated using NH3-SCR tests,Xray diffraction,specific surface area measurement,and H2 temperature-programmed reduction.The optimal type and dosage of porogen were determined accordingly.The results show that adding 5.0%by mass of polyethylene glycol results in the relatively optimal denitration performance of the molded catalyst,which exhibits a specific surface area of 3.70 m2/g,a total pore volume of 0.0308 cm3/g,and a denitration efficiency of 74.0%at 350℃.It also demonstrates high N2 selectivity,compressive strength,and redox capacity.Compared to the catalyst without any porogen,the denitration performance is significantly improved.

quote

GB/T 7714-2015 [1] HOU Li-min, WANG Xin-zhan, YE Yu-qiao, et al. Effect of Porogen on Acid-Activated Rare Earth Tailings-Based Molded NH3-SCR Denitration Catalyst[J]. Rare Metals and Cemented Carbides, 2025(5): 51-58.
MLA [1] HOU Li-min, et al., "Effect of Porogen on Acid-Activated Rare Earth Tailings-Based Molded NH3-SCR Denitration Catalyst." Rare Metals and Cemented Carbides, no. 5, 2025, pp. 51-58.
APA [1] HOU Li-min, WANG Xin-zhan, YE Yu-qiao, LI Jia-ming, SUN Xian-kang, LU Lin-bo, CHEN Han, & WU Wen-fei. (2025). Effect of Porogen on Acid-Activated Rare Earth Tailings-Based Molded NH3-SCR Denitration Catalyst. Rare Metals and Cemented Carbides(5), 51-58.
IEEE [1] HOU Li-min, WANG Xin-zhan, YE Yu-qiao, LI Jia-ming, SUN Xian-kang, LU Lin-bo, CHEN Han, and WU Wen-fei, "Effect of Porogen on Acid-Activated Rare Earth Tailings-Based Molded NH3-SCR Denitration Catalyst," Rare Metals and Cemented Carbides, no. 5, pp. 51-58, 2025. keywords: {porogen;acid-activation;rare earth tailings;NH-SCR;catalyst;denitration;polyethylene glycol}