Application of Fe78Si9B13 Amorphous Catalyst in Industrial Wastewater Pretreatment AITranslate
Abstract AITranslate
Industrial production wastewater has high chemical oxygen demand (COD) value and complex composition,which precludes effective treatment via a single unit operation. Direct discharge into the natural environment without treatment will cause environmental pollution,damage the ecosystem and threaten human health. Therefore,it is particularly important to seek an advanced and efficient process for the treatment of industrial wastewater.Heterogeneous catalytic ozonation,as a kind of advanced oxidation processes (AOPs),has attracted more and more attention from researchers due to its strong oxidizability and the ability to decompose ozone into reactive oxygen species to attack pollutants. However,the development of environmentally friendly and efficient cheap catalysts to promote ozone decomposition still faces enormous challenges. In this paper,actual high-COD flame retardant manufacturing wastewater collected from Xurui Industrial Wastewater Treatment Plant was used as the treatment target to investigate the COD removal performance of ozone catalytic oxidation over Fe-based amorphous alloy catalysts and its underlying reaction mechanism. Firstly,the master alloy rod was prepared by vacuum magnetron tungsten arc melting furnace,and then the master alloy rod was heated and spun into amorphous ribbon by high vacuum single roller-spinning and spray casting system to obtain the catalyst. X-ray diffraction (XRD),ultraviolet spectrophotometer,scanning electron microscopy (SEM) and electron spin resonance (ESR) were used to systematically analyze the structure,catalytic performance,surface morphology change,and the type and contribution of free radicals of the catalyst. In addition,the effects of ozone concentration and pH value on the efficiency of ozone catalytic oxidation were also discussed. The results showed that compared with the ozone oxidation method without obvious COD removal effect,the combination of amorphous alloy catalyst and ozone could effectively improve COD removal rate. Among Fe78Si9B13,(CoFe)80B20,(CoFeNi)80B20,(CoFeMn)80B20 and zero-valent iron (ZVI) samples,Fe78Si9B13 showed the best catalytic efficiency,and COD of wastewater could be removed by 15.28% within 2 h. (CoFe)80B20,(CoFeNi)80B20,(CoFeMn)80B20 and ZVI couldonly remove COD of wastewater by 11.61%,7.9%,4.19% and 3.23%,respectively. In particular,it was observed during the experiment that ZVI powder was easily adhered to the inner wall of the reactor,resulting in a poor catalytic effect.As the reaction progresses,a large number of holes and corrosion pits appeared on the surface of Fe78Si9B13,constantly exposing new substrates,and gradually evolving into a three-dimensional nanoflower-like structure,increasing active sites,promoting ozone decomposition to produce free radicals to attack pollutants. Secondly,the optimal ozone concentration was explored. The experimental results showed that COD removal ratios at ozone concentrations of 4,24,34,39,42 and 44 mg·L-1 were 17.95%,22.09%,30.95%,31.58%,32.09% and 32.19%,respectively. Among them,when O2 flow rate was 1.5 L·min-1,that was,the ozone concentration was 34.0 mg·L-1,COD removal effect hadreached 30.95%.When the ozone concentration continued to increase,COD removal rate did not increase much. In view of the cost and environmental friendliness,34.0 mg·L-1 was selected as the optimal ozone concentration. Similarly,the reaction time was investigated,revealing a COD removal efficiency of 30.9% at 2 h. Prolonging the reaction time only marginally improved the removal efficiency. Therefore,2 h was selected as the optimal reaction time to balance efficiency and cost-effectiveness.The lower pH,the better COD removal effect of ozone catalytic oxidation.When pH was 3,5,7,and 9,COD of wastewater could be removed by 35.67%,31.02%,30.58% and 15.51%,respectively. This might be due to the acidic environment to promote the consumption of the catalyst,thereby promoting the production of more free radicals and degrading pollutants. However,no acid-base adjustment treatment of neutral wastewater could avoid additional cost increase,and the removal efficiency at pH 7 was only about 5% different from that at pH3,which still had a good COD removal ratio.The removal effect of wastewater with different COD values was also studied. The production wastewater with COD values of 5600,7500,16000,36000,40000 and 44000 mg·L-1 were selected as the degradation target. The experiment was carried out under the conditions of ozone concentration of 34.0 mg·L-1,catalyst dosage of 1 g·L-1,pH 7 and room temperature. COD removal ratios after 2 h were 45.21%,31.04%,16.86%,10.47%,17.63% and 9.09%,respectively. With the increase of COD value,the removal ratio of COD decreased as a whole,but the removal rate of wastewater with COD of 40000 mg·L-1 increased instead,which might be due to the fact that the organic pollutants in this kind of wastewater were more easily degraded. In addition,although the removal ratiowas reduced,COD degradation amount increased with the increase of COD value of the raw water,indicating that the ozone catalytic oxidation had a good degradation effect on COD of the raw water,and could better adapt to different concentrations of production wastewater.Throughout nine consecutive cycling tests,Fe78Si9B13 catalyst consistently maintained a removal efficiency exceeding 26%,demonstrating its excellent cycling stability. Electron paramagnetic resonance tests showed that a large amount of hydroxyl radical (·OH) radicals could be produced in the ozone catalytic oxidation system,but this result was not observed in the ozone oxidation system,which further emphasized the role of the catalyst. In addition,the active site Fe in Fe78Si9B13 had a variety of valence states,which could further promote the electron transfer of O3 molecules and promote the reaction.
KeyWords AITranslate
[1](陈虹雨,王庆刚,胡林,孙宏杰. 功能材料在工业废水治理中的研究进展 [J]. 复合材料学报,2024,41(11):5924.)
H Y Chen,Q G Wang,L Hu,H J Sun. Recent research progress of functional materials in industrial wastewater treatment [J]. Acta Materiae Compositae Sinica,2024,41(11):5924.
[2]Wei J,Jia J,Liao T. Highly selective adsorption of dyes by functional hypercrosslinked-polymers prepared in a facile and chemically stable manner [J]. Journal of Environmental Chemical Engineering,2023,11:110555.
[3]Dutta D,Arya S,Kumar S. Industrial wastewater treatment:current trends,bottlenecks,and best practices [J]. Chemosphere,2021,285:131245.
[4](张盼盼,宋永辉,廖龙,周佳梦,王一帆. 过硫酸盐氧化处理氰化废水过程中添加量的影响研究 [J]. 稀有金属,2025,49(2):212.)
P P Zhang,Y H Song,L Liao,J M Zhou,Y F Wang. Treatment of cyanide gold extraction wastewater by adding different concentrations of persulfate oxidation [J]. Chinese Journal of Rare Metals,2025,49(2):212.
[5](徐昊,樊丽,郑冬. 应用CNN对紫外-可见光谱工业废水进行分类研究 [J]. 科技创新与应用,2025,15(17):49.)
H Xu,L Fan,D Zheng. Classification study on ultraviolet-visible spectral industrial wastewater using CNN [J]. Technology Innovation and Application,2025,15(17):49.
[6]Grégorio C,Eric L. Advantages and disadvantages of techniques used for wastewater treatment [J]. Environmental Chemistry Letters,2019,17(1):145.
[7](陈鑫,曹立坤. 污水处理厂COD和TOC分析的相关性研究 [J]. 工业用水与废水,2025,56(3):71.)
X Chen,L K Cao. Study on relevance between COD and TOC in sewage treatment plant [J]. Industrial Water & Wastewater,2025,56(3):71.
[8](姚恩亲,桂和荣. UV/TiO2降解矿井水CODcr中SO42-,HCO3-和Cl-的影响及动力学研究 [J]. 稀有金属,2008,32(2):224.)
E Q Yao,H R Gui. Kinetics and effect of SO42-,HCO3- and Cl- in coal mine water on degradation of mine water CODcr by UV/TiO2 [J]. Chinese Journal of Rare Metals,2008,32(2):224.
[9]Asghar A,Lutze H V,Tuerk J,Schmidt T C. Influence of water matrix on the degradation of organic micropollutants by ozone based processes:a review on oxidant scavenging mechanism [J]. Journal of Hazardous Materials,2022,429:128189.
[10]Wang J L,Chen H. Catalytic ozonation for water and wastewater treatment:recent advances and perspective [J]. Science of the Total Environment,2020,704:135249.
[11]Zhang T,Li C J,Ma J,Tian H,Qiang Z M. Surface hydroxyl groups of synthetic α-FeOOH in promoting ·OH generation from aqueous ozone:Property and activity relationship [J]. Applied Catalysis B:Environmental,2008,82:131.
[12]Zhu S M,Dong B Z,Yu Y H,Bu L J,Deng J,Zhou S Q. Heterogeneous catalysis of ozone using ordered mesoporous Fe3O4 for degradation of atrazine [J]. Chemical Engineering Journal,2017,328:527.
[13]Zhu H,Ma W C,Han H J,Han Y X,Ma W W. Catalytic ozonation of quinoline using nano-MgO:efficacy,pathways,mechanisms and its application to real biologically pretreated coal gasification wastewater [J]. Chemical Engineering Journal,2017,327:91.
[14]He C,Wang Y C,Li Z Y,Huang Y J,Liao Y H,Xia D H,Lee S C. Facet engineered α-MnO2 for efficient catalytic ozonation of odor CH3SH:oxygen vacancy-induced active centers and catalytic mechanism [J]. Environmental Science & Technology,2020,54:12771.
[15]Li Y Q,Fu M Q,Zhang X X,He C,Chen D S,Xiong Y,Guo L Q,Tian S H. Enhanced catalytic ozonation performance by CuOx nanoclusters/TiO2 nanotube and an insight into the catalytic mechanism [J]. Journal of Colloid and Interface Science,2023,651:589.
[16]You N,Deng S H,He H Y,Hu J Y. Ferromanganese oxide-functionalized TiO2 for rapid catalytic ozonation of PPCPs through a coordinated oxidation process with adjusted composition and strengthened generation of reactive oxygen species [J]. Water Research,2024,258:121813.
[17](李春燕,杨陇鹏,翟文正,李春玲,李晓诚,寇生中. 非晶合金污水处理研究现状 [J]. 稀有金属,2025,49(1):91.)
C Y Li,L P Yan,W Z Zhai,C L Li,X C Li,S Z Kou. Research status of amorphous alloy wastewater treatment [J]. Chinese Journal of Rare Metals,2025,49(1):91.
[18]Wang J Q,Liu Y H,Chen M W,Xie G Q,Louzguine-Luzgin D V,Inoue A,Perepezko J H. Rapid degradation of azo dye by Fe based metallic glass powder [J]. Advanced Functional Materials,2012,22:2567.
[19]Si JJ,Gu J L,Luan H W,Yang X L,Shi L X,Shao Y,Yao K F. Porous composite architecture bestows Fe-based glassy alloy with high and ultra-durable degradation activity in decomposing azo dye [J]. Journal of Hazardous Materials,2020,388:122043.
[20]Jjia Z,Jiang J L,Sun L G,Zhang L C,Wang Q,Liang S X,Qin P,Li D F,Lu J,Kruzic J J. Role of boron in enhancing electron delocalization to improve catalytic activity of Fe-based metallic glasses for persulfate-based advanced oxidation [J]. ACS Applied Materials & Interfaces,2020,12:44789.
[21]Jia Z,Duan X G,Qin P,Zhang W C,Wang W M,Yang C,Sun H Q,Wang S B,Zhang L C. Disordered atomic packing structure of metallic glass:toward ultrafast hydroxyl radicals production rate and strong electron transfer ability in catalytic performance [J]. Advanced Functional Materials,2017,27:1702258.
[22]Wang Q Q,Chen M X,Shao L L,Ge Y W,Lin P H,Chu C L,Shen B L. Effects of structural relaxation on the dye degradation ability of FePC amorphous alloys [J]. Journal of Non-Crystalline Solids,2019,525:119671.
[23](徐武军,张国臣,郑明霞,陈健,王凯军. 臭氧氧化技术处理含抗生素废水 [J]. 化学进展,2010,22(5):1002.)
W J Xu,G C Zhang,M X Zheng,J Chen,K J Wang. Treatment of antibiotic wastewater by ozonation [J]. Progress in Chemistry,2010,22(5):1002.
[24]Zhang L C,Jia Z,Lyu F C,Liang S X,Lu J. A review of catalytic performance of metallic glasses in wastewater treatment:recent progress and prospects [J]. Progress in Materials Science,2019,105:100576.
[25]Chen S Q,Li M,Ji Q M,Feng T,Lan S,Yao K F. Effect of the chloride ion on advanced oxidation processes catalyzed by Fe-based metallic glass for wastewater treatment [J]. Journal of Materials Science & Technology,2022,117:49.
[26](白格,陈茂清,蔡楠,郭子维,张婷,郭鹏然. 高级氧化技术中自由基的检测技术和方法研究进展 [J]. 分析测试学报,2021,40(7):1109.)
G Bai,M Q Chen,N Cai,Z W Guo,T Zhang,P R Guo. Advances on determination methods of free radicals in advanced oxidation processes [J]. Journal of Instrumental Analysis,2021,40(7):1109.
Basic Information:
DOI:10.13373/j.cnki.cjrm.XY25060005
Chinese Library Classification Number:TG139+.8
Citation Information:
Industrial production wastewater has high chemical oxygen demand (COD) value and complex composition,which precludes effective treatment via a single unit operation. Direct discharge into the natural environment without treatment will cause environmental pollution,damage the ecosystem and threaten human health. Therefore,it is particularly important to seek an advanced and efficient process for the treatment of industrial wastewater.Heterogeneous catalytic ozonation,as a kind of advanced oxidation processes (AOPs),has attracted more and more attention from researchers due to its strong oxidizability and the ability to decompose ozone into reactive oxygen species to attack pollutants. However,the development of environmentally friendly and efficient cheap catalysts to promote ozone decomposition still faces enormous challenges. In this paper,actual high-COD flame retardant manufacturing wastewater collected from Xurui Industrial Wastewater Treatment Plant was used as the treatment target to investigate the COD removal performance of ozone catalytic oxidation over Fe-based amorphous alloy catalysts and its underlying reaction mechanism. Firstly,the master alloy rod was prepared by vacuum magnetron tungsten arc melting furnace,and then the master alloy rod was heated and spun into amorphous ribbon by high vacuum single roller-spinning and spray casting system to obtain the catalyst. X-ray diffraction (XRD),ultraviolet spectrophotometer,scanning electron microscopy (SEM) and electron spin resonance (ESR) were used to systematically analyze the structure,catalytic performance,surface morphology change,and the type and contribution of free radicals of the catalyst. In addition,the effects of ozone concentration and pH value on the efficiency of ozone catalytic oxidation were also discussed. The results showed that compared with the ozone oxidation method without obvious COD removal effect,the combination of amorphous alloy catalyst and ozone could effectively improve COD removal rate. Among Fe78Si9B13,(CoFe)80B20,(CoFeNi)80B20,(CoFeMn)80B20 and zero-valent iron (ZVI) samples,Fe78Si9B13 showed the best catalytic efficiency,and COD of wastewater could be removed by 15.28% within 2 h. (CoFe)80B20,(CoFeNi)80B20,(CoFeMn)80B20 and ZVI couldonly remove COD of wastewater by 11.61%,7.9%,4.19% and 3.23%,respectively. In particular,it was observed during the experiment that ZVI powder was easily adhered to the inner wall of the reactor,resulting in a poor catalytic effect.As the reaction progresses,a large number of holes and corrosion pits appeared on the surface of Fe78Si9B13,constantly exposing new substrates,and gradually evolving into a three-dimensional nanoflower-like structure,increasing active sites,promoting ozone decomposition to produce free radicals to attack pollutants. Secondly,the optimal ozone concentration was explored. The experimental results showed that COD removal ratios at ozone concentrations of 4,24,34,39,42 and 44 mg·L-1 were 17.95%,22.09%,30.95%,31.58%,32.09% and 32.19%,respectively. Among them,when O2 flow rate was 1.5 L·min-1,that was,the ozone concentration was 34.0 mg·L-1,COD removal effect hadreached 30.95%.When the ozone concentration continued to increase,COD removal rate did not increase much. In view of the cost and environmental friendliness,34.0 mg·L-1 was selected as the optimal ozone concentration. Similarly,the reaction time was investigated,revealing a COD removal efficiency of 30.9% at 2 h. Prolonging the reaction time only marginally improved the removal efficiency. Therefore,2 h was selected as the optimal reaction time to balance efficiency and cost-effectiveness.The lower pH,the better COD removal effect of ozone catalytic oxidation.When pH was 3,5,7,and 9,COD of wastewater could be removed by 35.67%,31.02%,30.58% and 15.51%,respectively. This might be due to the acidic environment to promote the consumption of the catalyst,thereby promoting the production of more free radicals and degrading pollutants. However,no acid-base adjustment treatment of neutral wastewater could avoid additional cost increase,and the removal efficiency at pH 7 was only about 5% different from that at pH3,which still had a good COD removal ratio.The removal effect of wastewater with different COD values was also studied. The production wastewater with COD values of 5600,7500,16000,36000,40000 and 44000 mg·L-1 were selected as the degradation target. The experiment was carried out under the conditions of ozone concentration of 34.0 mg·L-1,catalyst dosage of 1 g·L-1,pH 7 and room temperature. COD removal ratios after 2 h were 45.21%,31.04%,16.86%,10.47%,17.63% and 9.09%,respectively. With the increase of COD value,the removal ratio of COD decreased as a whole,but the removal rate of wastewater with COD of 40000 mg·L-1 increased instead,which might be due to the fact that the organic pollutants in this kind of wastewater were more easily degraded. In addition,although the removal ratiowas reduced,COD degradation amount increased with the increase of COD value of the raw water,indicating that the ozone catalytic oxidation had a good degradation effect on COD of the raw water,and could better adapt to different concentrations of production wastewater.Throughout nine consecutive cycling tests,Fe78Si9B13 catalyst consistently maintained a removal efficiency exceeding 26%,demonstrating its excellent cycling stability. Electron paramagnetic resonance tests showed that a large amount of hydroxyl radical (·OH) radicals could be produced in the ozone catalytic oxidation system,but this result was not observed in the ozone oxidation system,which further emphasized the role of the catalyst. In addition,the active site Fe in Fe78Si9B13 had a variety of valence states,which could further promote the electron transfer of O3 molecules and promote the reaction.
quote
| GB/T 7714-2015 | [1] Yonghui Wang, Liqiang Li, Jianye Li, et al. Application of Fe78Si9B13 Amorphous Catalyst in Industrial Wastewater Pretreatment[J]. Chinese Journal of Rare Metals, 2026, 50(7): 1063-1071. DOI:10.13373/j.cnki.cjrm.XY25060005. |
| MLA | [1] Yonghui Wang, et al., "Application of Fe78Si9B13 Amorphous Catalyst in Industrial Wastewater Pretreatment." Chinese Journal of Rare Metals, vol. 50, no. 7, 2026, pp. 1063-1071, https://doi.org/10.13373/j.cnki.cjrm.XY25060005. |
| APA | [1] Yonghui Wang, Liqiang Li, Jianye Li, Xiaobin Tang, & Sida Jiang. (2026). Application of Fe78Si9B13 Amorphous Catalyst in Industrial Wastewater Pretreatment. Chinese Journal of Rare Metals, 50(7), 1063-1071. https://doi.org/10.13373/j.cnki.cjrm.XY25060005 |
| IEEE | [1] Yonghui Wang, Liqiang Li, Jianye Li, Xiaobin Tang, and Sida Jiang, "Application of Fe78Si9B13 Amorphous Catalyst in Industrial Wastewater Pretreatment," Chinese Journal of Rare Metals, vol. 50, no. 7, pp. 1063-1071, 2026, doi: 10.13373/j.cnki.cjrm.XY25060005. keywords: {wastewatertreatment;amorphous alloys;ozone catalytic oxidation;free radical} |