Naphthalimide-Fused Subphthalocyanines: Electron-Deficient Materials Prepared by Cascade Annulation AITranslate
Abstract AITranslate
Imide-fused porphyrinoids are becoming key components in the area of molecular materials. Herein we report the synthesis of naphthalimide (NMI)-annulated subphthalocyanines (SubPcs) designed as an NIR-absorbing n-type organic semiconductor. Two different synthetic pathways could be applied for the preparation of NMI-fused SubPcs. The first consists of a [3 + 2] annulation between SubPc boronic ester and dibromo-NMI. This annulation, which involves the first CH activation reaction of a SubPc derivative reported so far, is totally regioselective to the β-position. Density functional theory (DFT) indicated that such position is favored both kinetically and thermodynamically. On the other hand, the second method relies on a cyclotrimerization of NMI-fused phthalonitrile. Electrochemical measurements and DFT calculations revealed that these NMI-fused SubPcs have low-lying LUMO energy levels suitable for electron charge transport. The N-alkyl substituted derivative (NMI-SubPc 2) was successfully applied as an nonfullerene acceptor (NFA) in combination with donor polymer PM6 in bulk-heterojunction (BHJ) organic solar cells (OSCs) with a highest power conversion efficiency (PCE) of 7.0%. This value is comparable to the record PCE of SubPc derivatives in BHJ-OSCs. Our results open a new vista in the preparation of π-extended contracted porphyrinoids and substantiate the potential of this new class of strong-absorbing electron-acceptor materials for applications in optoelectronic devices.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsmaterialslett.2c01132
Chinese Library Classification Number:
Citation Information:
Imide-fused porphyrinoids are becoming key components in the area of molecular materials. Herein we report the synthesis of naphthalimide (NMI)-annulated subphthalocyanines (SubPcs) designed as an NIR-absorbing n-type organic semiconductor. Two different synthetic pathways could be applied for the preparation of NMI-fused SubPcs. The first consists of a [3 + 2] annulation between SubPc boronic ester and dibromo-NMI. This annulation, which involves the first CH activation reaction of a SubPc derivative reported so far, is totally regioselective to the β-position. Density functional theory (DFT) indicated that such position is favored both kinetically and thermodynamically. On the other hand, the second method relies on a cyclotrimerization of NMI-fused phthalonitrile. Electrochemical measurements and DFT calculations revealed that these NMI-fused SubPcs have low-lying LUMO energy levels suitable for electron charge transport. The N-alkyl substituted derivative (NMI-SubPc 2) was successfully applied as an nonfullerene acceptor (NFA) in combination with donor polymer PM6 in bulk-heterojunction (BHJ) organic solar cells (OSCs) with a highest power conversion efficiency (PCE) of 7.0%. This value is comparable to the record PCE of SubPc derivatives in BHJ-OSCs. Our results open a new vista in the preparation of π-extended contracted porphyrinoids and substantiate the potential of this new class of strong-absorbing electron-acceptor materials for applications in optoelectronic devices.
quote
| GB/T 7714-2015 | [1] Jorge Labella, Kazutaka Shoyama, David Guzmán, et al. ACS Materials Letters, 2023(5). DOI:10.1021/acsmaterialslett.2c01132. |
| MLA | [1] Jorge Labella, et al., ACS Materials Letters, no. 5, 2023, https://doi.org/10.1021/acsmaterialslett.2c01132. |
| APA | [1] Jorge Labella, Kazutaka Shoyama, David Guzmán, Tim Schembri, Matthias Stolte, Tomás Torres, & Frank Würthner. (2023). ACS Materials Letters(5). https://doi.org/10.1021/acsmaterialslett.2c01132 |
| IEEE | [1] Jorge Labella, Kazutaka Shoyama, David Guzmán, Tim Schembri, Matthias Stolte, Tomás Torres, and Frank Würthner, ACS Materials Letters, no. 5, 2023, doi: 10.1021/acsmaterialslett.2c01132. |