Selective Crystallization of a Highly Radiation-Resistant Isonicotinic Acid-Based Metal–Organic Framework as a Primary Actinide Waste Form AITranslate

Institute of Nuclear Physics and Chemistry;Institute of Resource Ecology;Institute of Resource Ecology;Institute of Resource Ecology;Institute of Resource Ecology;Institute of Resource Ecology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Isonicotinic acid (INA), as a prototypical N,O-donor bifunctional ligand, has demonstrated its ability to differentiate Th4+ from representative ions for products in spent nuclear fuels (Cs+, Ba2+, Mn2+, Fe2+, Fe3+, Co2+, Ni2+, Cu2+, Pd2+, ReO4–, La3+, Ce3+, Ce4+, UO22+), yielding an actinide metal–organic framework, Th-INA-1, by selective crystallization. This unprecedented motif with the highest ligand-binding number (i.e., 16) shows promise as a primary waste form due to its structural integrity, especially exposed to β- or γ-irradiation to achieve doses of 6 MGy.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsmaterialslett.2c01087

Chinese Library Classification Number:

Citation Information:

Isonicotinic acid (INA), as a prototypical N,O-donor bifunctional ligand, has demonstrated its ability to differentiate Th4+ from representative ions for products in spent nuclear fuels (Cs+, Ba2+, Mn2+, Fe2+, Fe3+, Co2+, Ni2+, Cu2+, Pd2+, ReO4–, La3+, Ce3+, Ce4+, UO22+), yielding an actinide metal–organic framework, Th-INA-1, by selective crystallization. This unprecedented motif with the highest ligand-binding number (i.e., 16) shows promise as a primary waste form due to its structural integrity, especially exposed to β- or γ-irradiation to achieve doses of 6 MGy.

quote

GB/T 7714-2015 [1] Kai Lv, Michael Patzschke, Juliane März, et al. ACS Materials Letters, 2023(5). DOI:10.1021/acsmaterialslett.2c01087.
MLA [1] Kai Lv, et al., ACS Materials Letters, no. 5, 2023, https://doi.org/10.1021/acsmaterialslett.2c01087.
APA [1] Kai Lv, Michael Patzschke, Juliane März, Elena Bazarkina, Kristina O. Kvashnina, & Moritz Schmidt. (2023). ACS Materials Letters(5). https://doi.org/10.1021/acsmaterialslett.2c01087
IEEE [1] Kai Lv, Michael Patzschke, Juliane März, Elena Bazarkina, Kristina O. Kvashnina, and Moritz Schmidt, ACS Materials Letters, no. 5, 2023, doi: 10.1021/acsmaterialslett.2c01087.