Study on Preparation and Photocatalytic Properties of TiO2-ZnO Composite Materials AITranslate

Engineering Experiment Training Center,Yuncheng University;Engineering Experiment Training Center,Yuncheng University;Engineering Experiment Training Center,Yuncheng University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Using titanium dioxide(TiO2)and zinc oxide(ZnO)powders as precursors,the TiO2-ZnO composite powders with different ZnO molar fraction(x)were synthesized via the solid phase method.The structure,morphology and properties of the composite materials were characterized by X-ray diffraction(XRD),scanning electron microscope(SEM)and ultraviolet-visible(UV-Vis)absorption spectrometer,respectively.The effects of different ZnO molar fraction and calcination temperature on the structure and morphology of TiO2-ZnO composites were investigated,and the photocatalytic activity of the composites for degradation of methyl orange was also studied.The results show that the calcination temperature has a great influence on the structure and morphology of the composites.With t=600℃ and x=0.440,the TiO2-ZnO powder is composed of wurtzite ZnO,anatase TiO2 and a small amount of Ti3Zn3O0.5,and the interface particles are closely contacted.The combination of ZnO and TiO2 not only enhances the absorption of the composites in the ultraviolet region,but also enhances the absorption in the visible region.In addition,the TiO2-ZnO composite(x=0.440)exhibits good photocatalytic activity for organic dye methyl orange,and the degradation rate of methyl orange reaches 95.7% after UV irradiation for 120 min.

KeyWords AITranslate

TiO2-ZnO solid phase method photocatalysis ZnO molar fraction calcination temperature

1王艳香,高智丹,赵学国,范学运,杨志胜,黄丽群,李家科,孙健.水热法制备ZnO/TiO_2复合粉体及其电池性能[J].陶瓷学报,2016,37(2):163-168. 被引量:4

2孙梦龙,王红波,聂祥龙,马大衍,马飞,徐可为.ZnO-TiO_2核壳纳米线结构及其热稳定性研究[J].稀有金属材料与工程,2015,44(12):3073-3077. 被引量:1

3冯汉坤,蔡宗英,李杰,李运刚.ZnO-TiO_2体系的固相合成与表征[J].有色金属科学与工程,2016,7(4):22-26. 被引量:2

4朱堂龙,王黎明,沈勇,汪萍,沈洋洋.纳米ZnO/TiO_2复合体系的制备及应用[J].印染,2016,42(2):1-6. 被引量:6

5吕宝华,李玉珍,宋维阳,姚陈忠.Ti^(4+)掺杂ZnO复合材料的制备及其光学性能研究[J].稀有金属,2014,38(6):1055-1059. 被引量:6

6季玉晓,贾瑛,王幸运,李明,侯立安,贺亚南.锐钛矿型TiO_2/ZnO纳米复合颗粒的制备及光学性能研究[J].化工新型材料,2016,44(8):148-150. 被引量:3

1林金梅,张晗.ZnO/TiO_(2)复合纳米材料的制备及其乙醇气敏性能研究[J].广州化工,2021,49(13):53-55. 被引量:1

1邹利婷,赵薇,邹望辉.基于rGO-SnO_(2)复合材料的丙酮气体传感器制备与特征分析[J].传感器与微系统,2023,42(4):27-30.

1刘红.纳米氧化锌的制备方法及其优缺点[J].山东化工,2019,48(24):114-114. 被引量:3

2王林香,赵海琴,孙德方.Mg2+、Zn2+掺杂CaWO4∶Eu3+荧光粉的发光性质[J].发光学报,2020,41(1):23-30. 被引量:5

3罗祖云,冯振亮,洪若瑜.二氧化钛空心微球的可控制备及其处理染料废水性能研究[J].水处理技术,2019,45(11):72-75. 被引量:2

4朱显会,张婷婷,李光益.以甘蔗渣为基质硝酸回流法制备碳量子点及其性能表征[J].江西化工,2019,0(6):64-66. 被引量:1

5李小芳.一种新型硅藻土负载物对甲基橙染料废水的吸附性能[J].天水师范学院学报,2019,39(5):120-122. 被引量:2

6俞双林,黄寿标,吴妮,李春碧,蒙卓玮,曾建民.分光光度法对锰矿中铁含量分析的研究[J].冶金工程,2019,6(4):180-184.

7陆文涛,赵青南,王晓宏,常潇,董玉红,赵杰.可见光照射下Fe3+掺杂量对玻璃基TiO2薄膜亲水性能的影响[J].硅酸盐通报,2019,38(10):3293-3301.

8李德华.拉曼光谱检测甲基苯丙胺类毒品的应用研究[J].化工设计通讯,2019,45(11):124-125. 被引量:3

9赵建强,张玥,王冠蕾.偶氮苯的合成与研究进展[J].化工管理,2020,0(1):94-95. 被引量:1

10张磊,张海霞,何佳,薛康,格日乐,石磊,鲍秀珍,丁铁柱.退火温度对(STO/YSZ/GDC)4超晶格电解质薄膜的影响[J].稀土,2019,40(6):42-48.

Basic Information:

DOI:

Chinese Library Classification Number:TQ134.1[化学工程—无机化工]

Citation Information:

Using titanium dioxide(TiO2)and zinc oxide(ZnO)powders as precursors,the TiO2-ZnO composite powders with different ZnO molar fraction(x)were synthesized via the solid phase method.The structure,morphology and properties of the composite materials were characterized by X-ray diffraction(XRD),scanning electron microscope(SEM)and ultraviolet-visible(UV-Vis)absorption spectrometer,respectively.The effects of different ZnO molar fraction and calcination temperature on the structure and morphology of TiO2-ZnO composites were investigated,and the photocatalytic activity of the composites for degradation of methyl orange was also studied.The results show that the calcination temperature has a great influence on the structure and morphology of the composites.With t=600℃ and x=0.440,the TiO2-ZnO powder is composed of wurtzite ZnO,anatase TiO2 and a small amount of Ti3Zn3O0.5,and the interface particles are closely contacted.The combination of ZnO and TiO2 not only enhances the absorption of the composites in the ultraviolet region,but also enhances the absorption in the visible region.In addition,the TiO2-ZnO composite(x=0.440)exhibits good photocatalytic activity for organic dye methyl orange,and the degradation rate of methyl orange reaches 95.7% after UV irradiation for 120 min.

quote

GB/T 7714-2015 [1] LI Yu-zhen, LV Bao-hua, YAO Chen-zhong. Study on Preparation and Photocatalytic Properties of TiO2-ZnO Composite Materials[J]. Rare Metals and Cemented Carbides, 2019(6): 48-51.
MLA [1] LI Yu-zhen, et al., "Study on Preparation and Photocatalytic Properties of TiO2-ZnO Composite Materials." Rare Metals and Cemented Carbides, no. 6, 2019, pp. 48-51.
APA [1] LI Yu-zhen, LV Bao-hua, & YAO Chen-zhong. (2019). Study on Preparation and Photocatalytic Properties of TiO2-ZnO Composite Materials. Rare Metals and Cemented Carbides(6), 48-51.
IEEE [1] LI Yu-zhen, LV Bao-hua, and YAO Chen-zhong, "Study on Preparation and Photocatalytic Properties of TiO2-ZnO Composite Materials," Rare Metals and Cemented Carbides, no. 6, pp. 48-51, 2019. keywords: {TiO2-ZnO;solid phase method;photocatalysis;ZnO molar fraction;calcination temperature}