Effect of Trace Oxygen Content on Microstructure and Mechanical Properties of Ti-3Zr Alloy AITranslate

College of Materials Science and Technology,Nanjing University of Aeronautics and A stronautics;College of Materials Science and Technology,Nanjing University of Aeronautics and A stronautics;College of Materials Science and Technology,Nanjing University of Aeronautics and A stronautics;College of Materials Science and Technology,Nanjing University of Aeronautics and A stronautics;College of Materials Science and Technology,Nanjing University of Aeronautics and A stronautics
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The effect of trace oxygen content on phase transition temperature,microstructure and mechanical properties of Ti-3 Zr alloy was discussed by differential scanning calorimetry,X-ray diffractometry,metallographic microscope,transmission electron microscope,universal testing machine and Vickers hardness tester.The experimental results show that with the increase of oxygen content,the phase transition temperature of Ti-3 Zr-xO alloys increases,and their microstructure greatly changes,transforming from Widmanstatten structure into basket-waved structure,then into bimodal structure and finally into equiaxed structure.The tensile strength and yield strength of the alloys are significantly increased with the increase of oxygen,attributed to the solid solution strengthening of oxygen.The plasticity of the alloys shows a decline trend on the whole.Ti-3 Zr-0.05 O has lower plasticity than adjacent alloys due to the presence of a certain number of dislocation cells and ultrafine crystals in its substructure.The plasticity of Ti-3 Zr-0.25 O alloy is significantly improved by the toughening mechanism of nano-twin crystals.Ti-3 Zr-0.25 O alloy has the best comprehensive mechanical properties.

KeyWords AITranslate

oxygen content Ti-3Zr alloy microstructure mechanical property nano-twin crystal

1张国宝,彭楚峰,吴鹤.超细晶/纳米晶钛合金的研究与进展[J].材料导报,2007,21(F11):9-10. 被引量:2

2秦川.钛和钛合金铸件在牙科医疗上的应用[J].稀有金属与硬质合金,2002,30(4):54-56. 被引量:3

3孟丽君,梁伟,赵兴国,李秀杰.应变速率对纯铁位错胞尺寸的影响[J].电子显微学报,2005,24(4):295-295. 被引量:4

4缪润杰,汪涛,钱海梅,何庆贤,郑长天.氧含量对Ti-4Zr-xO合金组织与力学性能的影响[J].稀有金属,2017,41(11):1196-1201. 被引量:2

5王凯旋,曾卫东,赵永庆,周义刚.钛合金显微组织与性能定量关系的模型[J].稀有金属材料与工程,2011,40(5):784-787. 被引量:9

6卢磊,卢柯.纳米孪晶金属材料[J].金属学报,2010,46(11):1422-1427. 被引量:41

7朱康平,祝建雯,曲恒磊.国外生物医用钛合金的发展现状[J].稀有金属材料与工程,2012,41(11):2058-2063. 被引量:63

1罗红萍.EVA/MBS/稀土三元共混改性PVC性能研究[J].广东化工,2019,46(20):29-30. 被引量:5

2吴汐玥,陈志勇,程超,刘建荣,徐东生,王清江.热处理对Ti65钛合金板材的显微组织、织构及拉伸性能的影响[J].材料研究学报,2019,33(10):785-793. 被引量:10

3李婧雅.PDCA循环在提高母婴分离产妇母乳采集储存正确率中的应用[J].当代护士:中旬刊,2020,27(1):59-61. 被引量:1

4翟大军,税玥,袁满,张燕燕,何跃斌.α相含量及形态对TC4钛合金组织和力学性能的影响[J].金属热处理,2019,44(10):129-134. 被引量:8

5程小伟,张高寅,马志超,李斌,辜涛.页岩气水平井油井水泥的原位增韧技术研究[J].西南石油大学学报:自然科学版,2019,41(6):68-74. 被引量:5

6孙为民.孙为民 苏宁的全场景智慧零售 会在六个方向持续成长[J].中外管理,2019,0(12):62-63. 被引量:1

7朱红,孙捷,凌敏.锻造工艺对BT25钛合金组织和性能影响[J].热加工工艺,2019,48(21):102-104.

8陈霞,张丁非,邓天宇,赵阳,冯靖凯,蒋斌,潘复生.Ca和Sn对ZM61合金微观组织和性能的影响[J].材料热处理学报,2019,40(12):13-18.

9丁青军,郑勇,柯峥,严永林,周伟.不同细WC添加量对板状硬质合金显微组织和力学性能各向异性的影响[J].硬质合金,2019,36(6):414-422.

10王洪涛.乙醇-空气混合气激光点火火焰形成过程研究[J].科学技术创新,2019,0(34):20-21.

Basic Information:

DOI:

Chinese Library Classification Number:TG146.23[金属学及工艺—金属材料]

Citation Information:

The effect of trace oxygen content on phase transition temperature,microstructure and mechanical properties of Ti-3 Zr alloy was discussed by differential scanning calorimetry,X-ray diffractometry,metallographic microscope,transmission electron microscope,universal testing machine and Vickers hardness tester.The experimental results show that with the increase of oxygen content,the phase transition temperature of Ti-3 Zr-xO alloys increases,and their microstructure greatly changes,transforming from Widmanstatten structure into basket-waved structure,then into bimodal structure and finally into equiaxed structure.The tensile strength and yield strength of the alloys are significantly increased with the increase of oxygen,attributed to the solid solution strengthening of oxygen.The plasticity of the alloys shows a decline trend on the whole.Ti-3 Zr-0.05 O has lower plasticity than adjacent alloys due to the presence of a certain number of dislocation cells and ultrafine crystals in its substructure.The plasticity of Ti-3 Zr-0.25 O alloy is significantly improved by the toughening mechanism of nano-twin crystals.Ti-3 Zr-0.25 O alloy has the best comprehensive mechanical properties.

quote

GB/T 7714-2015 [1] FEI Yang, WANG Tao, MIAO Run-jie, et al. Effect of Trace Oxygen Content on Microstructure and Mechanical Properties of Ti-3Zr Alloy[J]. Rare Metals and Cemented Carbides, 2019(6): 52-58.
MLA [1] FEI Yang, et al., "Effect of Trace Oxygen Content on Microstructure and Mechanical Properties of Ti-3Zr Alloy." Rare Metals and Cemented Carbides, no. 6, 2019, pp. 52-58.
APA [1] FEI Yang, WANG Tao, MIAO Run-jie, WANG Qian, & YUAN Jie. (2019). Effect of Trace Oxygen Content on Microstructure and Mechanical Properties of Ti-3Zr Alloy. Rare Metals and Cemented Carbides(6), 52-58.
IEEE [1] FEI Yang, WANG Tao, MIAO Run-jie, WANG Qian, and YUAN Jie, "Effect of Trace Oxygen Content on Microstructure and Mechanical Properties of Ti-3Zr Alloy," Rare Metals and Cemented Carbides, no. 6, pp. 52-58, 2019. keywords: {oxygen content;Ti-3Zr alloy;microstructure;mechanical property;nano-twin crystal}