Functional polyurethanes have several important advanced applications. In this investigation, a dual-functional polyurethane (PU) elastomer having disulfide as well as furfuryl functionality was developed. For this purpose, a functional diol having furfuryl and disulfide functionality was synthesized and used as a chain extender for the synthesis of a PU elastomer based on polycaprolactone (PCL) diol and 4,4′-methylenebis (phenyl diisocyanate) (MDI). This dual functional PU elastomer was cross-linked using a bismaleimide (BM) via the Diels–Alder (DA) reaction with the furfuryl pendant group in PU. This dual functional PU having thermoreversible DA linkage and disulfide linkage showed excellent tensile strength (σ = 39.5 MPa) and, importantly, good self-healing characteristics (self-healing efficiency, Eσ ≈ 97%). This healable PU having a thermoresponsive as well as a double dynamic covalent system based on the DA reaction and the disulfide metathesis reaction will have potential applications in specialty paints, coatings, and various advanced materials.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.0c01179
Chinese Library Classification Number:
Citation Information:
Functional polyurethanes have several important advanced applications. In this investigation, a dual-functional polyurethane (PU) elastomer having disulfide as well as furfuryl functionality was developed. For this purpose, a functional diol having furfuryl and disulfide functionality was synthesized and used as a chain extender for the synthesis of a PU elastomer based on polycaprolactone (PCL) diol and 4,4′-methylenebis (phenyl diisocyanate) (MDI). This dual functional PU elastomer was cross-linked using a bismaleimide (BM) via the Diels–Alder (DA) reaction with the furfuryl pendant group in PU. This dual functional PU having thermoreversible DA linkage and disulfide linkage showed excellent tensile strength (σ = 39.5 MPa) and, importantly, good self-healing characteristics (self-healing efficiency, Eσ ≈ 97%). This healable PU having a thermoresponsive as well as a double dynamic covalent system based on the DA reaction and the disulfide metathesis reaction will have potential applications in specialty paints, coatings, and various advanced materials.
quote
| GB/T 7714-2015 | [1] Prasanta Kumar Behera, Sagar Kumar Raut, Prantik Mondal, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.0c01179. |
| MLA | [1] Prasanta Kumar Behera, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.0c01179. |
| APA | [1] Prasanta Kumar Behera, Sagar Kumar Raut, Prantik Mondal, Shrabana Sarkar, & Nikhil K. Singha. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.0c01179 |
| IEEE | [1] Prasanta Kumar Behera, Sagar Kumar Raut, Prantik Mondal, Shrabana Sarkar, and Nikhil K. Singha, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.0c01179. keywords: {selfhealing;polyurethane;disulfide metathesis;click chemistry;Diels−Alder reaction;dual dynamic} |