Cyclometalated Platinum(II) Complexes Simultaneously Catalyze the Cross-Linking of Polysiloxanes and Function as Luminophores AITranslate

Saint Petersburg State University;Saint Petersburg State University;Saint Petersburg State University;Saint Petersburg State University;Saint Petersburg State University; 199034 Russian Federation|South Ural State University;Saint Petersburg State University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

A family of the C,N-cyclometalated species [Pt(ppy)Cl(PPh3)], [Pt(ppy)Cl(CNCy)], [Pt(ppy)(CNCy)(PPh3)](OTf), and [Pt(ppy)(CNCy)2](BF4) (ppy = 2-phenylpyridinato-C2,N; Cy = cyclohexyl) was generated from [Pt(ppy)(μ-Cl)]2, CNCy, and PPh3. The obtained platinum(II) complexes were characterized by high-resolution ESI+-MS, IR, and 1D (1H, 13C{1H}, 195Pt{1H}) and 2D (1H,1H-NOESY; 1H,13C-HSQC; 1H,13C-HMBC) NMR spectroscopy, and the latter three complexes were investigated by X-ray diffraction. All four platinum species were examined as hydrosilylation catalysts (c 10–4–10–3 M; 80–120 °C; [Pt(ppy)Cl(PPh3)] exhibited the highest catalytic activity) for the cross-linking of vinyl-terminated polydimethylsiloxane and polymethylhydrosiloxane to achieve luminescent silicone rubbers. Each solid complex and the appropriate silicone rubber exhibited the same emission spectra in the green region and strong phosphorescence with a solid-state quantum yield of up to 12.5% (measured for the silicone elastomer obtained with the [Pt(ppy)(CNCy)2](BF4) catalyst). The resulting luminescent silicone rubbers can be potentially used for protective coatings (to facilitate the thickness control) and as a component for phosphor-converted white light-emitting diodes (to transform a UV part of the LED emission to the visible spectrum).

KeyWords AITranslate

crosslinking hydrosilylation luminescent silicones catalysis platinum complexes isocyanides
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.0c01190

Chinese Library Classification Number:

Citation Information:

A family of the C,N-cyclometalated species [Pt(ppy)Cl(PPh3)], [Pt(ppy)Cl(CNCy)], [Pt(ppy)(CNCy)(PPh3)](OTf), and [Pt(ppy)(CNCy)2](BF4) (ppy = 2-phenylpyridinato-C2,N; Cy = cyclohexyl) was generated from [Pt(ppy)(μ-Cl)]2, CNCy, and PPh3. The obtained platinum(II) complexes were characterized by high-resolution ESI+-MS, IR, and 1D (1H, 13C{1H}, 195Pt{1H}) and 2D (1H,1H-NOESY; 1H,13C-HSQC; 1H,13C-HMBC) NMR spectroscopy, and the latter three complexes were investigated by X-ray diffraction. All four platinum species were examined as hydrosilylation catalysts (c 10–4–10–3 M; 80–120 °C; [Pt(ppy)Cl(PPh3)] exhibited the highest catalytic activity) for the cross-linking of vinyl-terminated polydimethylsiloxane and polymethylhydrosiloxane to achieve luminescent silicone rubbers. Each solid complex and the appropriate silicone rubber exhibited the same emission spectra in the green region and strong phosphorescence with a solid-state quantum yield of up to 12.5% (measured for the silicone elastomer obtained with the [Pt(ppy)(CNCy)2](BF4) catalyst). The resulting luminescent silicone rubbers can be potentially used for protective coatings (to facilitate the thickness control) and as a component for phosphor-converted white light-emitting diodes (to transform a UV part of the LED emission to the visible spectrum).

quote

GB/T 7714-2015 [1] Mikhail V. Dobrynin, Elina V. Sokolova, Mikhail A. Kinzhalov, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.0c01190.
MLA [1] Mikhail V. Dobrynin, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.0c01190.
APA [1] Mikhail V. Dobrynin, Elina V. Sokolova, Mikhail A. Kinzhalov, Andrey S. Smirnov, Galina L. Starova, Vadim Yu. Kukushkin, & Regina M. Islamova. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.0c01190
IEEE [1] Mikhail V. Dobrynin, Elina V. Sokolova, Mikhail A. Kinzhalov, Andrey S. Smirnov, Galina L. Starova, Vadim Yu. Kukushkin, and Regina M. Islamova, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.0c01190. keywords: {crosslinking;hydrosilylation;luminescent silicones;catalysis;platinum complexes;isocyanides}