Recent Progress on Environmentally Friendly Humidity Sensor: A Mini Review Recent Progress on Environmentally Friendly Humidity Sensor: A Mini Review AITranslate

Wuhan Textile University; Wuhan Textile University; Harbin Institute of Technology (Shenzhen)
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Due to the impact of the epidemic, human health is seriously threatened so that the technology of human health detection is increasingly important, and humidity sensors for detecting human health have been studied extensively. A number of humidity sensors made of a variety of different materials and based on multiple principles have been prepared, which can be classified into numerous categories. This article starts out by introducing sensor materials according to environmentally friendliness. Following that, a variety of structures for humidity sensors, the mechanisms for sensing, and different power supply types are discussed. This study summarizes the review of current research in this field as well as challenges that exist, indicating the focus of possible future research and application prospects. This work may pave the way to understanding the overview of humidity sensing.

KeyWords AITranslate

humidity sensors environmentally friendliness moisture flexible electronics sensing mechanism
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.3c00653

Chinese Library Classification Number:

Citation Information:

Due to the impact of the epidemic, human health is seriously threatened so that the technology of human health detection is increasingly important, and humidity sensors for detecting human health have been studied extensively. A number of humidity sensors made of a variety of different materials and based on multiple principles have been prepared, which can be classified into numerous categories. This article starts out by introducing sensor materials according to environmentally friendliness. Following that, a variety of structures for humidity sensors, the mechanisms for sensing, and different power supply types are discussed. This study summarizes the review of current research in this field as well as challenges that exist, indicating the focus of possible future research and application prospects. This work may pave the way to understanding the overview of humidity sensing.

quote

GB/T 7714-2015 [1] Cheng Huang, Ming Jiang, Feihua Liu. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.3c00653.
MLA [1] Cheng Huang, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.3c00653.
APA [1] Cheng Huang, Ming Jiang, & Feihua Liu. (2023). ACS Applied Electronic Materials(5). https://doi.org/10.1021/acsaelm.3c00653
IEEE [1] Cheng Huang, Ming Jiang, and Feihua Liu, ACS Applied Electronic Materials, no. 5, 2023, doi: 10.1021/acsaelm.3c00653. keywords: {humidity sensors environmentally friendliness moisture flexible electronics sensing mechanism}