Determination of Tungsten in Tantalum-niobium Ores by Inductively Coupled Plasma Mass Spectrometry AITranslate
Abstract AITranslate
Currently,spectrophotometry method and ICP-AES method are generally used to determine low content tungsten in ores .With the continuous development and innovation of analytical techniques,ICP- MS method has obvious advantages in the field of trace analysis.In this paper,ICP-MS as a new instrument analysis and detection method with the advantages of high-resolution,high sensitivity,low detection limit and rapid analysis is established to meet the requirements of rapid analysis of low content tungsten in tantalum-niobium ores in industrial production,which is superior to current analytical methods developed by industry standards.After testing,the analytical results of ICP-AES are accurate and reliable,and can be applied in practice.
KeyWords AITranslate
1陈登云,Tye Christopher.ICP-MS技术及其应用[J].现代仪器,2001(4):8-11. 被引量:36
2蔡彦明.无机痕量元素分析的好帮手:安捷伦ICP-MS 7500i[J].农业环境与发展,2006,23(4):19-21. 被引量:1
3刘宁平,刘建章,孙洪志,郭让民,郝红卫.钽铌工业生产及其展望[J].稀有金属快报,2005,24(9):1-6. 被引量:13
4周礼仙.硫氰酸盐分光光度法测定镍基合金中钨[J].冶金分析,2017,37(8):78-82. 被引量:5
5白小叶,佡云,迟爱玲.硫氰酸盐光度法测定钼精矿中的钨[J].有色矿冶,2015,30(6):49-51. 被引量:5
6刁憬平,秦宗兴,高银香.电感耦合等离子体发射光谱法测定钨矿中的钨[J].化学工程与装备,2011(7):180-181. 被引量:7
7邹龙,刘荣丽,易师.电感耦合等离子体原子发射光谱法测定铝钨合金中钨[J].冶金分析,2014,34(11):65-68. 被引量:3
8赵建平.硫氰酸盐分光光度法测定岩矿中钨量的改进[J].新疆有色金属,2016,39(1):69-69. 被引量:1
9何蔓,胡斌,江祖成.用于研究ICP-MS中基体效应的逐级稀释法[J].高等学校化学学报,2004,25(12):2232-2237. 被引量:33
1冯先进.电感耦合等离子体质谱分析技术在国内矿石矿物分析中的应用[J].冶金分析,2020,40(6):21-36. 被引量:8
2张众,李明华.ICP-OES法测定钽铌矿石中钨铜钛含量[J].湖南有色金属,2023,39(2):87-90.
3陈世航,刘莉,邓志伟,郝中骐,史久林,何兴道.基于单激光构造的DP-LIBS对钽铌矿的检测研究[J].激光与光电子学进展,2023,60(13):291-296.
1李彤,沈康俊,朱亚冠,闵红,李晨,刘曙.高分辨电感耦合等离子体质谱分析地质样品中痕量元素的应用进展[J].冶金分析,2021,41(4):9-19. 被引量:7
2刘曙,干兆祥,闵红.电感耦合等离子体质谱分析中金属元素的基体效应[J].冶金分析,2021,41(12):79-86. 被引量:5
3张元,王文东,卢兵,赵文志,杨园,吕胜男.碱熔-阳离子交换树脂分离ICP-MS法测定厚覆盖区地球化学调查样品中硼锗溴钼锡碘钨[J].岩矿测试,2022,41(1):99-108. 被引量:2
4王斌,郑少锋,李伟才,钟康华,甘久林,杨中民,宋武元.高基体样品进样系统-电感耦合等离子体质谱法测定进口铜精矿中稀土元素的含量[J].光谱学与光谱分析,2022,42(6):1822-1826. 被引量:4
5乔雅楠.质谱分析法在化学分析中的应用[J].化学工程与装备,2022(6):221-222. 被引量:1
6王夺.镍锍试金-微波消解法联合测定汽车三元催化剂中铑[J].有色矿冶,2023,39(2):59-61.
7刘芳美,甘聪,廖彬玲,罗小兵,赖秋祥.锍镍试金富集-电感耦合等离子体质谱法测定铜阳极泥中微量元素铱铑[J].岩矿测试,2023,42(2):298-306.
8冯先进,马丽.电感耦合等离子体质谱(ICP-MS)法在我国矿物中“四稀”元素检测的应用[J].中国无机分析化学,2023,13(8):802-812.
1文忠勇.刍议小学语文高效课堂的策略探究[J].文理导航:教育研究与实践,2019,0(1):75-75.
2李鹏彦.离子色谱法在水质分析中的运用[J].中国石油和化工标准与质量,2018,38(16):35-36. 被引量:1
3郑美华.农村数字普惠金融:发展模式与典型案例[J].农村经济,2019(3):96-104. 被引量:43
4张中华,赵玉焕,SU Bin,王浩.能源需求与碳排放驱动因素分解模型发展评述[J].生态经济,2019,35(4):13-19. 被引量:9
5《光谱学与光谱分析》投稿简则[J].光谱学与光谱分析,2019,39(4):1221-1221.
6添彩凤.计算机图像识别的智能化处理方法解读[J].电脑乐园,2018,0(3):351-351.
7沈英.基于Nordest准则的化学分析测量不确定度评估研究[J].中国标准化,2018(A01):197-201. 被引量:1
8赵卓婷,段峰峰.婚恋交友App面临的问题及策略研究[J].科技传播,2018,10(17):159-160.
9耿昊,李海,徐陈陈,董健健,陈燕,韩咏竹,韩永升,杨任民,程楠.肝豆汤对Wilson病模型铜负荷大鼠肝脏Wnt/β-catenin信号通路的调控作用[J].中国实验方剂学杂志,2019,25(7):75-81. 被引量:8
10刘星.融合局部语义信息的多模态舆情分析模型[J].信息安全研究,2019,5(4):340-345. 被引量:5
Basic Information:
DOI:
Chinese Library Classification Number:TF841.1[冶金工程—有色金属冶金]
Citation Information:
Currently,spectrophotometry method and ICP-AES method are generally used to determine low content tungsten in ores .With the continuous development and innovation of analytical techniques,ICP- MS method has obvious advantages in the field of trace analysis.In this paper,ICP-MS as a new instrument analysis and detection method with the advantages of high-resolution,high sensitivity,low detection limit and rapid analysis is established to meet the requirements of rapid analysis of low content tungsten in tantalum-niobium ores in industrial production,which is superior to current analytical methods developed by industry standards.After testing,the analytical results of ICP-AES are accurate and reliable,and can be applied in practice.
quote
| GB/T 7714-2015 | [1] WU Zhuo-kui, HUANG Shuang. Determination of Tungsten in Tantalum-niobium Ores by Inductively Coupled Plasma Mass Spectrometry[J]. Rare Metals and Cemented Carbides, 2019(1): 80-82. |
| MLA | [1] WU Zhuo-kui, and HUANG Shuang. "Determination of Tungsten in Tantalum-niobium Ores by Inductively Coupled Plasma Mass Spectrometry." Rare Metals and Cemented Carbides, no. 1, 2019, pp. 80-82. |
| APA | [1] WU Zhuo-kui, & HUANG Shuang. (2019). Determination of Tungsten in Tantalum-niobium Ores by Inductively Coupled Plasma Mass Spectrometry. Rare Metals and Cemented Carbides(1), 80-82. |
| IEEE | [1] WU Zhuo-kui and HUANG Shuang, "Determination of Tungsten in Tantalum-niobium Ores by Inductively Coupled Plasma Mass Spectrometry," Rare Metals and Cemented Carbides, no. 1, pp. 80-82, 2019. keywords: {ICP-MS;tantalum-niobium ores;tungsten;analysis and detection;application} |