Amplifying Photoluminescence of Lanthanide-Doped Nanoparticles by Iridium Phosphonate Complex AITranslate
Abstract AITranslate
Amplifying the photoluminescence of lanthanide-doped nanoparticles by antenna materials can bridge the gap in properties between pristine nanoparticles and those required by practical applications. However, high-performance antennas with ideal stability are rather few. Here, we report a new type of iridium (Ir)-based phosphonate complex as an antenna to amplify the near-infrared luminescence of lanthanide-doped nanoparticles. Unlike conventional antennas, the Ir complex, with a quasi-spherical structure and pendent phosphonic groups, can resist the aggregation-caused quenching and firmly anchor on nanoparticles. Near-infrared luminescence of lanthanide-doped nanoparticles can be stably amplified up to 130 times by the complex, which should be due to short-range energy transfer from the triplet state of the complex to lanthanide ions. These findings may pave a new fundamental way to amplify the luminescence of lanthanide-doped nanoparticles and promote applications of the nanoparticles.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsmaterialslett.2c01125
Chinese Library Classification Number:
Citation Information:
Amplifying the photoluminescence of lanthanide-doped nanoparticles by antenna materials can bridge the gap in properties between pristine nanoparticles and those required by practical applications. However, high-performance antennas with ideal stability are rather few. Here, we report a new type of iridium (Ir)-based phosphonate complex as an antenna to amplify the near-infrared luminescence of lanthanide-doped nanoparticles. Unlike conventional antennas, the Ir complex, with a quasi-spherical structure and pendent phosphonic groups, can resist the aggregation-caused quenching and firmly anchor on nanoparticles. Near-infrared luminescence of lanthanide-doped nanoparticles can be stably amplified up to 130 times by the complex, which should be due to short-range energy transfer from the triplet state of the complex to lanthanide ions. These findings may pave a new fundamental way to amplify the luminescence of lanthanide-doped nanoparticles and promote applications of the nanoparticles.
quote
| GB/T 7714-2015 | [1] Kui Xu, Chen Lin, MingFeng Qin, et al. ACS Materials Letters, 2023(5). DOI:10.1021/acsmaterialslett.2c01125. |
| MLA | [1] Kui Xu, et al., ACS Materials Letters, no. 5, 2023, https://doi.org/10.1021/acsmaterialslett.2c01125. |
| APA | [1] Kui Xu, Chen Lin, MingFeng Qin, Ze Yuan, Ye Tao, SongSong Bao, Runfeng Chen, Xiaoji Xie, & LiMin Zheng. (2023). ACS Materials Letters(5). https://doi.org/10.1021/acsmaterialslett.2c01125 |
| IEEE | [1] Kui Xu, Chen Lin, MingFeng Qin, Ze Yuan, Ye Tao, SongSong Bao, Runfeng Chen, Xiaoji Xie, and LiMin Zheng, ACS Materials Letters, no. 5, 2023, doi: 10.1021/acsmaterialslett.2c01125. |