Biodegradable Sucrose Ester-Based Cationic Lipids as Novel Vectors for Efficient and Safe Delivery of IGF-1R siRNA AITranslate

Dalian Minzu University; Dalian Minzu University; Dalian Minzu University; Dalian Minzu University; Dalian Minzu University; Dalian Medical University; Dalian Medical University; Dalian Medical University; Dalian Minzu University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites
111111

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The key to the success of siRNA therapy depends on the use of siRNA delivery agents that effectively penetrate tumor cells and simultaneously protect siRNA from RNase attacks. Sucrose esters (SEs) are found to have tremendous potential applications in siRNA delivery because of their biocompatibility and low toxicity. However, the esterification of sucrose yields complex mixtures that greatly limit their progress in this field. We synthesized a series of novel sucrose monoester-based cationic lipids (SECLs) by using 1′,4,6′-trichlorogalactosucrose (TGS) to achieve monoesterification of sucrose. SECL-based liposomes formed from these lipids and colipids [dioleoylphosphatidylethanolamine (DOPE) or cholesterol (Chol)] could effectively condense genes into nanocomplexes, which exhibited significantly higher uptake rates and gene silencing efficiency than 1,2-dioleoyl-3-trimethylammonium-propane (DOTAP) liposome. Furthermore, SECL-based liposomes containing cholesterol-mediated IGF-1R siRNA delivery could inhibit tumor growth by the downregulation of Bcl-2 and the upregulation of Bax. Most importantly, these liposomes displayed low cytotoxicity in vitro and in vivo because they could be degraded under tumor acidic pH environments. Our study establishes a novel method for the synthesis of SEs from TGS and demonstrates the applicability of SECLs for gene delivery with the potential for clinical therapy.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsmaterialslett.2c00994

Chinese Library Classification Number:

Citation Information:

The key to the success of siRNA therapy depends on the use of siRNA delivery agents that effectively penetrate tumor cells and simultaneously protect siRNA from RNase attacks. Sucrose esters (SEs) are found to have tremendous potential applications in siRNA delivery because of their biocompatibility and low toxicity. However, the esterification of sucrose yields complex mixtures that greatly limit their progress in this field. We synthesized a series of novel sucrose monoester-based cationic lipids (SECLs) by using 1′,4,6′-trichlorogalactosucrose (TGS) to achieve monoesterification of sucrose. SECL-based liposomes formed from these lipids and colipids [dioleoylphosphatidylethanolamine (DOPE) or cholesterol (Chol)] could effectively condense genes into nanocomplexes, which exhibited significantly higher uptake rates and gene silencing efficiency than 1,2-dioleoyl-3-trimethylammonium-propane (DOTAP) liposome. Furthermore, SECL-based liposomes containing cholesterol-mediated IGF-1R siRNA delivery could inhibit tumor growth by the downregulation of Bcl-2 and the upregulation of Bax. Most importantly, these liposomes displayed low cytotoxicity in vitro and in vivo because they could be degraded under tumor acidic pH environments. Our study establishes a novel method for the synthesis of SEs from TGS and demonstrates the applicability of SECLs for gene delivery with the potential for clinical therapy.

quote

GB/T 7714-2015 [1] Defu Zhi, Jian Shi, Shaohui Cui, et al. ACS Materials Letters, 2023(5). DOI:10.1021/acsmaterialslett.2c00994.
MLA [1] Defu Zhi, et al., ACS Materials Letters, no. 5, 2023, https://doi.org/10.1021/acsmaterialslett.2c00994.
APA [1] Defu Zhi, Jian Shi, Shaohui Cui, Ting Yang, Jian Yang, Wei Wang, Pengfei Ma, Yuhong Zhen, & Shubiao Zhang. (2023). ACS Materials Letters(5). https://doi.org/10.1021/acsmaterialslett.2c00994
IEEE [1] Defu Zhi, Jian Shi, Shaohui Cui, Ting Yang, Jian Yang, Wei Wang, Pengfei Ma, Yuhong Zhen, and Shubiao Zhang, ACS Materials Letters, no. 5, 2023, doi: 10.1021/acsmaterialslett.2c00994.