Selective Laser Sintering for Electrically Conductive Poly(dimethylsiloxane) Composites with Self-Healing Lattice Structures AITranslate

Sichuan University; Sichuan University; Sichuan University; Sichuan University; Sichuan University; Sichuan University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Developing flexible elastomer composites for sensors and effective fabrication methods is of great significance. Single-walled carbon nanotubes (SWCNTs)-wrapped poly(dimethylsiloxane) covalent adaptable networks (PDMS-CANs) composite powders were prepared through a liquid-phase deposition and adsorption process and used for selective laser sintering (SLS) three-dimensional (3D) printing. The electrically conductive PDMS composite parts with self-healing lattice structures were printed. Ingeniously utilizing the quasi-static processing characteristic of SLS printing, the conductive segregated SWCNT networks are in situ formed in PDMS-CANs during the printing process, showing an ultralow percolation threshold of 0.007 wt %. Due to the photothermal and electrothermal effects of SWCNTs, the composites possess multifunctions including crack diagnosis and self-healing triggered by heat, electricity, or light. To demonstrate the potential application, the SLS-printed SWCNTs@PDMS-CANs strain sensors with various lattice structures were designed and SLS-printed. Their strain sensitivity is compared and analyzed by finite element modeling. The results show that the TPMS Schwartz structure possesses the highest sensitivity due to the concentrated localized strain.

KeyWords AITranslate

SLS 3D printing PDMS electrical conductive selfhealing lattice
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c00138

Chinese Library Classification Number:

Citation Information:

Developing flexible elastomer composites for sensors and effective fabrication methods is of great significance. Single-walled carbon nanotubes (SWCNTs)-wrapped poly(dimethylsiloxane) covalent adaptable networks (PDMS-CANs) composite powders were prepared through a liquid-phase deposition and adsorption process and used for selective laser sintering (SLS) three-dimensional (3D) printing. The electrically conductive PDMS composite parts with self-healing lattice structures were printed. Ingeniously utilizing the quasi-static processing characteristic of SLS printing, the conductive segregated SWCNT networks are in situ formed in PDMS-CANs during the printing process, showing an ultralow percolation threshold of 0.007 wt %. Due to the photothermal and electrothermal effects of SWCNTs, the composites possess multifunctions including crack diagnosis and self-healing triggered by heat, electricity, or light. To demonstrate the potential application, the SLS-printed SWCNTs@PDMS-CANs strain sensors with various lattice structures were designed and SLS-printed. Their strain sensitivity is compared and analyzed by finite element modeling. The results show that the TPMS Schwartz structure possesses the highest sensitivity due to the concentrated localized strain.

quote

GB/T 7714-2015 [1] Xue Li, Hao Ouyang, Shaojie Sun, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c00138.
MLA [1] Xue Li, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c00138.
APA [1] Xue Li, Hao Ouyang, Shaojie Sun, Jinzhi Wang, Guoxia Fei, & Hesheng Xia. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c00138
IEEE [1] Xue Li, Hao Ouyang, Shaojie Sun, Jinzhi Wang, Guoxia Fei, and Hesheng Xia, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c00138. keywords: {SLS;3D printing;PDMS;electrical conductive;selfhealing lattice}