Ketocoumarins are attractive and distinct photosensitizers due to their high molar extinction coefficients, high intersystem crossing coefficients, and high photochemical stability. As a classic commercial ketocoumarin-based two-photon initiator, 7-diethylamino-3-thenoylcoumarin (DETC) was widely used in two-photon lithography. However, the large fluorescence quantum yield and low two-photon absorption cross section value greatly limit its application in high-throughput nanofabrication. In this work, a series of DETC derivatives were developed by extending the length of the alkyl chain and integrating different donor and acceptor groups. These ketocoumarin-based initiators, namely, compounds 1–7, were designed, synthesized, and unambiguously characterized. Compared with DETC, these compounds exhibit higher molar extinction coefficient, lower fluorescence quantum yield, higher two-photon absorption cross section, and improved sensitivity in two-photon lithography. Among these molecules, compound 7 with expanded π-electron systems and structures with enhanced intramolecular charge transfer exhibits the best sensitivity in two-photon lithography. With compound 7-based photoresist, many kinds of complex three-dimensional patterns can be fabricated using two-photon lithography at a writing speed of up to 60 mm s–1. The high two-photon initiation sensitivity makes these compounds promising candidates for commercialization and provides a new design concept for the development of new initiators.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.3c00141
Chinese Library Classification Number:
Citation Information:
Ketocoumarins are attractive and distinct photosensitizers due to their high molar extinction coefficients, high intersystem crossing coefficients, and high photochemical stability. As a classic commercial ketocoumarin-based two-photon initiator, 7-diethylamino-3-thenoylcoumarin (DETC) was widely used in two-photon lithography. However, the large fluorescence quantum yield and low two-photon absorption cross section value greatly limit its application in high-throughput nanofabrication. In this work, a series of DETC derivatives were developed by extending the length of the alkyl chain and integrating different donor and acceptor groups. These ketocoumarin-based initiators, namely, compounds 1–7, were designed, synthesized, and unambiguously characterized. Compared with DETC, these compounds exhibit higher molar extinction coefficient, lower fluorescence quantum yield, higher two-photon absorption cross section, and improved sensitivity in two-photon lithography. Among these molecules, compound 7 with expanded π-electron systems and structures with enhanced intramolecular charge transfer exhibits the best sensitivity in two-photon lithography. With compound 7-based photoresist, many kinds of complex three-dimensional patterns can be fabricated using two-photon lithography at a writing speed of up to 60 mm s–1. The high two-photon initiation sensitivity makes these compounds promising candidates for commercialization and provides a new design concept for the development of new initiators.
quote
| GB/T 7714-2015 | [1] Jin Tang, Xiaoyi Xu, Xiaoming Shen, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c00141. |
| MLA | [1] Jin Tang, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c00141. |
| APA | [1] Jin Tang, Xiaoyi Xu, Xiaoming Shen, Cuifang Kuang, Hongzheng Chen, Minmin Shi, & Ning Huang. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c00141 |
| IEEE | [1] Jin Tang, Xiaoyi Xu, Xiaoming Shen, Cuifang Kuang, Hongzheng Chen, Minmin Shi, and Ning Huang, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c00141. keywords: {twophoton lithography;twophoton photoinitiator;ketocoumarin;DETC;highspeed nanolithography} |