Residual Molecular Groups’ Adsorption in Tuning the Transport Properties of Carbon Nanotubes Residual Molecular Groups’ Adsorption in Tuning the Transport Properties of Carbon Nanotubes AITranslate

Xiangtan University; Xiangtan University; University of Electronic Science and Technology of China
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Carbon nanotubes (CNTs) have attracted much attention due to their unique electronic structures and transport properties for the application of carbon-based sensor components. It is doubtful in experiments that if the adsorbates, such as the groups of conjugated polymers, hinder the performance of transport on CNTs. Here, we systemically studied the transport properties of common groups (−CH3, −C6H5, −NH2, −OH) adsorbed on (7, 0)-CNT by first-principles calculations. Our results show that the adsorption of surface groups will lead to different impurity states near the Fermi level. The localized electrons at the Fermi level limit the electrical transport properties of CNTs. The electron transport capacity of CNTs becomes weaker with increase in the impurity concentration and the carrier mobility becomes lower. Our research provides an instructive theoretical foundation for fabricating high-performance carbon-based sensor devices.

KeyWords AITranslate

carbon nanotubes conjugated polymers electronic structure carrier mobility firstprinciples
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.3c00072

Chinese Library Classification Number:

Citation Information:

Carbon nanotubes (CNTs) have attracted much attention due to their unique electronic structures and transport properties for the application of carbon-based sensor components. It is doubtful in experiments that if the adsorbates, such as the groups of conjugated polymers, hinder the performance of transport on CNTs. Here, we systemically studied the transport properties of common groups (−CH3, −C6H5, −NH2, −OH) adsorbed on (7, 0)-CNT by first-principles calculations. Our results show that the adsorption of surface groups will lead to different impurity states near the Fermi level. The localized electrons at the Fermi level limit the electrical transport properties of CNTs. The electron transport capacity of CNTs becomes weaker with increase in the impurity concentration and the carrier mobility becomes lower. Our research provides an instructive theoretical foundation for fabricating high-performance carbon-based sensor devices.

quote

GB/T 7714-2015 [1] Xiaoling Li, Juexian Cao, Yanning Zhang. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.3c00072.
MLA [1] Xiaoling Li, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.3c00072.
APA [1] Xiaoling Li, Juexian Cao, & Yanning Zhang. (2023). ACS Applied Electronic Materials(5). https://doi.org/10.1021/acsaelm.3c00072
IEEE [1] Xiaoling Li, Juexian Cao, and Yanning Zhang, ACS Applied Electronic Materials, no. 5, 2023, doi: 10.1021/acsaelm.3c00072. keywords: {carbon nanotubes conjugated polymers electronic structure carrier mobility firstprinciples}