Ultrasmall Palladium Nanoparticles Confined within Dendronized Polymers as High-Efficiency Catalysts AITranslate

Xinjiang University; Xinjiang University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Palladium nanoparticles (PdNPs) have attracted considerable interest for years and have been extensively applied as nanocatalysts for hydrogenation and C–C cross-coupling reactions. In general, small PdNPs are highly active nanocatalysts. However, it is a challenge to prepare PdNP catalysts with a size of less than 1.0 nm. Here, ultrasmall PdNPs (ca. 1.0 nm) are prepared using the linear PG0 or dendronized PG1 and PG2 as stabilizers. The catalytic activity of G0-PdNPs (1.00 ± 0.4 nm), G1-PdNPs (0.99 ± 0.4 nm), and G2-PdNPs (0.98 ± 0.4 nm) is estimated and compared in the catalytic 4-nitrophenol reduction and Suzuki–Miyaura reactions. The G1-PdNPs are observed to show the highest catalytic activity for both the reactions. In the 4-nitrophenol reduction, G1-PdNPs had a rate constant of 4.25 × 10–2 s–1 and a turnover frequency of up to 18,750 h–1. In the Suzuki–Miyaura reactions, G1-PdNPs with an ultralow dosage (50 ppm) can reach approximately quantitative yields with a turnover frequency of 3166 h–1, and G1-PdNPs also exhibit good applicability and generality for different substrates. The current work provides a valuable reference for the design and preparation of ultrasmall PdNPs in catalysis.

KeyWords AITranslate

palladium nanoparticles nanocatalysts dendronized polymers 4nitrophenol reduction Suzuki–Miyaura reactions
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c01995

Chinese Library Classification Number:

Citation Information:

Palladium nanoparticles (PdNPs) have attracted considerable interest for years and have been extensively applied as nanocatalysts for hydrogenation and C–C cross-coupling reactions. In general, small PdNPs are highly active nanocatalysts. However, it is a challenge to prepare PdNP catalysts with a size of less than 1.0 nm. Here, ultrasmall PdNPs (ca. 1.0 nm) are prepared using the linear PG0 or dendronized PG1 and PG2 as stabilizers. The catalytic activity of G0-PdNPs (1.00 ± 0.4 nm), G1-PdNPs (0.99 ± 0.4 nm), and G2-PdNPs (0.98 ± 0.4 nm) is estimated and compared in the catalytic 4-nitrophenol reduction and Suzuki–Miyaura reactions. The G1-PdNPs are observed to show the highest catalytic activity for both the reactions. In the 4-nitrophenol reduction, G1-PdNPs had a rate constant of 4.25 × 10–2 s–1 and a turnover frequency of up to 18,750 h–1. In the Suzuki–Miyaura reactions, G1-PdNPs with an ultralow dosage (50 ppm) can reach approximately quantitative yields with a turnover frequency of 3166 h–1, and G1-PdNPs also exhibit good applicability and generality for different substrates. The current work provides a valuable reference for the design and preparation of ultrasmall PdNPs in catalysis.

quote

GB/T 7714-2015 [1] Xiong Liu, Fangfei Liu. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c01995.
MLA [1] Xiong Liu, and Fangfei Liu. ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c01995.
APA [1] Xiong Liu, & Fangfei Liu. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c01995
IEEE [1] Xiong Liu and Fangfei Liu, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c01995. keywords: {palladium nanoparticles;nanocatalysts;dendronized polymers;4nitrophenol reduction;Suzuki–Miyaura reactions}