Experimental Study on the Molybdenum Oxide Extraction From a Refractory Molybdenum Oxide Ore AITranslate

Zhengzhou Institute of Mineral Comprehensive Utilization of China Academy of Geological Sciences;Zhengzhou Institute of Mineral Comprehensive Utilization of China Academy of Geological Sciences;Zhengzhou Institute of Mineral Comprehensive Utilization of China Academy of Geological Sciences;Zhengzhou Institute of Mineral Comprehensive Utilization of China Academy of Geological Sciences
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The process of sump leaching with hydrochloric acid for two cycles was adopted to extract molybdenum oxide from a refractory molybdenum oxide ore produced in Inner Mongolia.The ore contains 1.20% Mo,and its particle size is 10~20 mm.The ratio of liquid to solid is controlled at 0.3 during leaching,and leaching duration of either cycle is 8 h.The HCl concentrations of leaching solutios are 200 g/L and 220 g/L,respectively for the first cycle and the second cycle.The results show that the average Mo leaching rate of the above process is 78.80%,the recovery of ammonia neutralization-precipitation process is 96.22%,and Mo content of the product is 43%.

KeyWords AITranslate

molybdenum oxide ore cycling leaching hydrochloric acid ammonia molybdenum trioxide

1q李洪桂.稀有金属冶金学[M].北京:冶金工业出版社,1990.

2符剑刚,钟宏,王晖,贾丽娟,魏志锋.石煤中钼资源的综合开发与利用[J].稀有金属与硬质合金,2007,35(2):40-43. 被引量:12

1康维刚,郭鹏志,邱沙,彭志兵.河北某难选钼矿石酸浸浸钼试验[J].金属矿山,2015,44(7):77-79. 被引量:2

2郑琦,韦悦周,何春林,隆万江,王帆.低品位氧化钼矿石常压酸/碱浸出试验[J].金属矿山,2018,47(8):92-97. 被引量:2

3付强,王均,贾木欣,温利刚,王清.一种新型钼矿床中钼的赋存状态及对选矿工艺的影响[J].矿产保护与利用,2022,42(1):123-128. 被引量:3

4王鑫尧,杨洪英,康建,赵涵.复杂钼钨矿石溶浸试验[J].有色金属:冶炼部分,2023(5):75-80.

5邵伟华,赵平,王洪杰,刘广学.某低品位氧化钼钨粗精矿精选试验研究[J].矿业研究与开发,2014,34(2):41-44. 被引量:3

1王宇斌,彭祥玉,张小波,李帅,雷大士.某难选混合钼矿选矿试验研究[J].矿业研究与开发,2016,36(4):47-50. 被引量:6

2汪义兰.某钨矿选矿工艺流程优化研究[J].中国钨业,2016,31(3):37-40. 被引量:1

3肖军辉,施哲,陈金花.含钼铜精矿氧化焙烧-浸出分离钼研究[J].重庆大学学报:自然科学版,2016,39(4):50-56. 被引量:2

4李慧,王宇斌,靳建平.某石英岩型高硫铜钼矿石选矿试验研究[J].中国矿业,2017,26(10):136-141. 被引量:5

5戴蔚,何春林,郑春慧,韦悦周,李杰.D296树脂从低品位氧化钼矿石的硫酸浸出液中吸附钼[J].现代矿业,2020,36(4):113-117.

6刘明宝,耿西侠,王哲文.钼矿废石中硫化钼的高效回收技术研究[J].商洛学院学报,2022,36(4):49-54.

7陈永琳,冯吉福,周奇明,周丽君.四川省某地碱性花岗岩氧化带中钼矿石工艺特性研究[J].矿产与地质,2022,36(4):776-780.

8张帅,彭祥玉,王宇斌,林星彤,王雯雯.基于AHP-模糊综合评价法的钼金属回收率评估[J].中国钼业,2023,47(1):31-36.

9王鑫尧,杨洪英,康建,赵涵.复杂钼钨矿石溶浸试验[J].有色金属:冶炼部分,2023(5):75-80.

10梁耕宇,康绍辉,孟晋,王洪明,杨剑飞,武翠莲.某难处理钼矿浸出工艺研究[J].铀矿冶,2023,42(3):24-28.

1肖华利.铟浸出工艺探讨[J].稀有金属与硬质合金,2003,31(4):4-6. 被引量:8

2程裕钧,余修勤.土龙山金矿池浸提金工艺的改进[J].江西冶金,1990,10(3):40-42.

3李承元.江西稀土工业现状及展望[J].世界有色金属,1996,21(6):10-15. 被引量:1

4赵思佳,刘振楠,刘景槐.某低硫金矿全泥氰化浸出、池浸试验研究[J].湖南有色金属,2012,28(5):23-26. 被引量:2

5崔涛,赖浚,袁野,彭建蓉,和晓才,谢刚.低品位多金属矿石焙砂浸出铜锌工艺研究[J].湿法冶金,2015,34(5):369-372. 被引量:6

6张江娟,邓理龙,钟淑梅.提钪萃余液制取铁红的研究[J].湿法冶金,2005,24(1):17-18. 被引量:4

7蒋志建.从含钯、铜、银等贵金属废料中回收钯和银[J].湿法冶金,2003,22(3):155-158. 被引量:7

8陈红亮,王德美,郭建春,陈恒,郑娟.电解锰渣资源化利用研究进展[J].六盘水师范学院学报,2016,28(1):7-9. 被引量:5

9靳林,普世坤,李善吉.从高硅高碳钒矿中回收钒的工艺研究[J].稀有金属与硬质合金,2011,39(2):6-9.

10离子型稀土矿山开采方式的革新[J].稀土信息,1993(2):2-3.

Basic Information:

DOI:

Chinese Library Classification Number:TF841.2[冶金工程—有色金属冶金]

Citation Information:

The process of sump leaching with hydrochloric acid for two cycles was adopted to extract molybdenum oxide from a refractory molybdenum oxide ore produced in Inner Mongolia.The ore contains 1.20% Mo,and its particle size is 10~20 mm.The ratio of liquid to solid is controlled at 0.3 during leaching,and leaching duration of either cycle is 8 h.The HCl concentrations of leaching solutios are 200 g/L and 220 g/L,respectively for the first cycle and the second cycle.The results show that the average Mo leaching rate of the above process is 78.80%,the recovery of ammonia neutralization-precipitation process is 96.22%,and Mo content of the product is 43%.

quote

GB/T 7714-2015 [1] CAO Yao-hua, GAO Zhao-guo, LIU Hong-zhao, et al. Experimental Study on the Molybdenum Oxide Extraction From a Refractory Molybdenum Oxide Ore[J]. Rare Metals and Cemented Carbides, 2011(1): 1-3.
MLA [1] CAO Yao-hua, et al., "Experimental Study on the Molybdenum Oxide Extraction From a Refractory Molybdenum Oxide Ore." Rare Metals and Cemented Carbides, no. 1, 2011, pp. 1-3.
APA [1] CAO Yao-hua, GAO Zhao-guo, LIU Hong-zhao, & YANG Shao-wen. (2011). Experimental Study on the Molybdenum Oxide Extraction From a Refractory Molybdenum Oxide Ore. Rare Metals and Cemented Carbides(1), 1-3.
IEEE [1] CAO Yao-hua, GAO Zhao-guo, LIU Hong-zhao, and YANG Shao-wen, "Experimental Study on the Molybdenum Oxide Extraction From a Refractory Molybdenum Oxide Ore," Rare Metals and Cemented Carbides, no. 1, pp. 1-3, 2011. keywords: {molybdenum oxide ore;cycling leaching;hydrochloric acid;ammonia;molybdenum trioxide}