Development of remaining life prediction of crankshaft remanufacturing core AITranslate

Science and Technology on Remanufacturing Laboratory;Science and Technology on Remanufacturing Laboratory;Science and Technology on Remanufacturing Laboratory;Science and Technology on Remanufacturing Laboratory;Science and Technology on Remanufacturing Laboratory
AITranslate
Publisher: Springer Nature
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

This paper reviewed the main research work in the field of remaining life prediction of crankshaft remanufacturing core by Science and Technology on Remanufacturing Laboratory. Based on the results of finite element analysis, the R angle zone of crankshaft was determined as a major measuring position. A special measuring probe is developed, and bending fatigue bench tests were carried out to collect electromagnetic damage information during fatigue process. A neural network model was established to identify damage degree of crankshaft core, and a damage evaluation equipment for crankshaft core was developed.

KeyWords AITranslate

Remanufacturing Remaining life Crankshaft Metal magnetic memory Multifrequency eddy current
No data

Basic Information:

DOI:https://doi.org/10.1007/s40436-013-0004-7

Chinese Library Classification Number:

Citation Information:

This paper reviewed the main research work in the field of remaining life prediction of crankshaft remanufacturing core by Science and Technology on Remanufacturing Laboratory. Based on the results of finite element analysis, the R angle zone of crankshaft was determined as a major measuring position. A special measuring probe is developed, and bending fatigue bench tests were carried out to collect electromagnetic damage information during fatigue process. A neural network model was established to identify damage degree of crankshaft core, and a damage evaluation equipment for crankshaft core was developed.

quote

GB/T 7714-2015 [1] LiHong Dong, BinShi Xu, Nan Xue, et al. Advances in Manufacturing, 2013(1). DOI:10.1007/s40436-013-0004-7.
MLA [1] LiHong Dong, et al., Advances in Manufacturing, no. 1, 2013, https://doi.org/10.1007/s40436-013-0004-7.
APA [1] LiHong Dong, BinShi Xu, Nan Xue, HuiPeng Wang, & HaoYu Li. (2013). Advances in Manufacturing(1). https://doi.org/10.1007/s40436-013-0004-7
IEEE [1] LiHong Dong, BinShi Xu, Nan Xue, HuiPeng Wang, and HaoYu Li, Advances in Manufacturing, no. 1, 2013, doi: 10.1007/s40436-013-0004-7. keywords: {Remanufacturing;Remaining life;Crankshaft;Metal magnetic memory;Multifrequency eddy current}