An Organic Retinomorphic Sensor An Organic Retinomorphic Sensor AITranslate
Abstract AITranslate
Inspired by the way retinal cells respond to light, retinomorphic sensors are hoped to enable rapid identification of moving objects. Unlike conventional optical sensors, these sensors are designed to produce a signal in response to changes in illumination but not under constant illumination. This report represents the first demonstration of a retinomorphic sensor employing organic semiconductors as the absorber. The sensor exhibits stability under constant measurement conditions up to a period of 1 h and characteristic decay times that are tunable through a choice of external resistor, demonstrated down to 10 μs, roughly 10 000 times faster than previous devices.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsaelm.1c00955
Chinese Library Classification Number:
Citation Information:
Inspired by the way retinal cells respond to light, retinomorphic sensors are hoped to enable rapid identification of moving objects. Unlike conventional optical sensors, these sensors are designed to produce a signal in response to changes in illumination but not under constant illumination. This report represents the first demonstration of a retinomorphic sensor employing organic semiconductors as the absorber. The sensor exhibits stability under constant measurement conditions up to a period of 1 h and characteristic decay times that are tunable through a choice of external resistor, demonstrated down to 10 μs, roughly 10 000 times faster than previous devices.
quote
| GB/T 7714-2015 | [1] Cinthya Trujillo Herrera, John G. Labram. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.1c00955. |
| MLA | [1] Cinthya Trujillo Herrera, and John G. Labram. ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.1c00955. |
| APA | [1] Cinthya Trujillo Herrera, & John G. Labram. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.1c00955 |
| IEEE | [1] Cinthya Trujillo Herrera and John G. Labram, ACS Applied Electronic Materials, no. 4, 2022, doi: 10.1021/acsaelm.1c00955. keywords: {retinomorphic neuromorphic eventdriven organic semiconductor optical sensor} |