Study of Processability of Low-Re Mo Alloy AITranslate
Abstract AITranslate
The processability of low-Re Mo alloy manufactured by PM is studied. It was observed that the tensile strength and initial recrystallization temperature of the said alloy were increased wiht the incresae of Re content. The relation between tensile strength and annealing temperature conformed to linear regressing equations for the wire specimens with 1%,3%,and 5% Re at 900 to 1400℃ annealing temperatures.
KeyWords AITranslate
1刘沙.亚(过)共晶合金次生相的简便计算[J].稀有金属与硬质合金,1997,25(3):52-53. 被引量:1
1辛甜,李延超,林小辉,常恬,高选乔,梁静.不同铼含量对钼铼合金性能影响研究概述[J].中国钼业,2022,46(6):1-8.
1刘沙.粉末冶金法制取低铼钼合金的研究[J].稀有金属与硬质合金,1997,25(4):26-29.
2刘沙,曹昱,舒金波.低铼钼合金高温烧结过程的研究[J].稀有金属与硬质合金,1999,27(4):18-20. 被引量:3
Basic Information:
DOI:
Chinese Library Classification Number:TF125.241[冶金工程—粉末冶金]
Citation Information:
The processability of low-Re Mo alloy manufactured by PM is studied. It was observed that the tensile strength and initial recrystallization temperature of the said alloy were increased wiht the incresae of Re content. The relation between tensile strength and annealing temperature conformed to linear regressing equations for the wire specimens with 1%,3%,and 5% Re at 900 to 1400℃ annealing temperatures.
quote
| GB/T 7714-2015 | [1] LIU Sha. Study of Processability of Low-Re Mo Alloy[J]. Rare Metals and Cemented Carbides, 1998(1): 33-36. |
| MLA | [1] LIU Sha. "Study of Processability of Low-Re Mo Alloy." Rare Metals and Cemented Carbides, no. 1, 1998, pp. 33-36. |
| APA | [1] LIU Sha. (1998). Study of Processability of Low-Re Mo Alloy. Rare Metals and Cemented Carbides(1), 33-36. |
| IEEE | [1] LIU Sha, "Study of Processability of Low-Re Mo Alloy," Rare Metals and Cemented Carbides, no. 1, pp. 33-36, 1998. keywords: {low-Re Mo alloy;PM;processability} |