Investigation into the Common Quality Defect in the Processing of W-Ce Ingot AITranslate

Beijing Tungsten and Molybdenum Materials Factory
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Brief description and analysis are made with respect to the quality defects (ie cracks, split and corewrapping) during W-Ce ingot processing. Preliminary investigation is made into the ways to prevent the defects and to improve the product quality.

KeyWords AITranslate

W-Ce electrode ingot processing quality defects

1李鹏.钨铈坯条深度加工工艺研究[J].稀有金属与硬质合金,1997,25(4):29-31.

2莫智桓.浅谈10kV配网工程常见质量缺陷及其防治对策[J].大科技,2012(6):71-72.

3王为.钨铈电极生产过程中氧化铈某些行为的浅析[J].有色金属与稀土应用,1994(4):38-46.

4朱清.混铁车结盖分析[J].宝钢技术,1997(5):8-11.

5张钰,张俊,王聪,朱敏娃,慎月强.电线电缆质量比对方案[J].科技视界,2015(22):331-332.

6曹武民.浅谈系列按键开关的结构改进[J].机电元件,2001,21(4):8-12.

7张业昭.电容式电压互感器故障分析[J].科协论坛:下半月,2012(12):25-26. 被引量:3

8阙兴正.钨铈电极的研制[J].稀有金属与硬质合金,1999(1):20-23. 被引量:3

9唐辉,牛燕光,廉波,陆助瑛,董梅.1~#、3~#750m^3高炉炉前开口机改造[J].莱钢科技,2005(2):13-15.

10王志刚.发电机失磁保护研析[J].机电信息,2005(3):33-36.

Basic Information:

DOI:

Chinese Library Classification Number:TF125.24[冶金工程—粉末冶金];TM24[一般工业技术—材料科学与工程]

Citation Information:

Brief description and analysis are made with respect to the quality defects (ie cracks, split and corewrapping) during W-Ce ingot processing. Preliminary investigation is made into the ways to prevent the defects and to improve the product quality.

quote

GB/T 7714-2015 [1] ZHANG Wen-lu. Investigation into the Common Quality Defect in the Processing of W-Ce Ingot[J]. Rare Metals and Cemented Carbides, 1998(1): 37-39.
MLA [1] ZHANG Wen-lu. "Investigation into the Common Quality Defect in the Processing of W-Ce Ingot." Rare Metals and Cemented Carbides, no. 1, 1998, pp. 37-39.
APA [1] ZHANG Wen-lu. (1998). Investigation into the Common Quality Defect in the Processing of W-Ce Ingot. Rare Metals and Cemented Carbides(1), 37-39.
IEEE [1] ZHANG Wen-lu, "Investigation into the Common Quality Defect in the Processing of W-Ce Ingot," Rare Metals and Cemented Carbides, no. 1, pp. 37-39, 1998. keywords: {W-Ce electrode;ingot processing;quality defects}