Development of Cemented Carbide Technologyin China and Abroad AITranslate
Abstract AITranslate
The development of foreign cemen ted carbide technology isreviewed. the general description of the development of China 's cementedcarbide technology is made. Some suggestions are made for speeding-upthe development of China's cemented carbide industry.
KeyWords AITranslate
1林伯颖,李沐山.发挥引进技术优势 推进企业科技进步[J].中国钨业,1993,0(8):4-7. 被引量:1
1张文毓.硬质合金技术研究进展[J].材料开发与应用,2011,26(1):61-65. 被引量:3
2张少华,鲍立强.浅析WC—Co硬质合金研究现状[J].中国科技博览,2013(31):607-607.
1孙晓莉.量块材质特性比较[J].工业计量,2012,22(S1):264-265. 被引量:1
2黄华龙,李益民,潘文强.基于黏弹性理论液相共烧结模型的建立及应用研究[J].有色金属科学与工程,2014,5(6):71-79. 被引量:1
3王娟梅,仝晓楠,高源.高性能煤化工浆料输出用硬质合金喷嘴的制备试验[J].机械研究与应用,2020,33(2):138-139.
12006上海国际硬质合金工业及生产技术与应用展览会[J].硬质合金,2005,22(4):231-231.
2亓家钟.世界硬质合金工业的最新发展[J].国外金属材料,1992(4):25-30.
3李沐山.世界硬质合金工业现状与发展趋势[J].世界有色金属,1993(10):2-7.
4王春荣.成分对高硼白口耐磨铸铁组织与性能的影响[J].热加工工艺,2014,43(1):19-21. 被引量:1
5王定武.国外不锈钢生产的发展趋势和我国不锈钢发展的建议[J].特殊钢,1996,17(5):30-33. 被引量:5
6周大伟,许晨阳,李晋,吴智鹏.镁合金激光表面改性研究新进展[J].轻金属,2007(4):39-42. 被引量:6
7冯光纯.控轧控冷技术的现状与发展[J].四川冶金,1996,18(1):73-75. 被引量:9
8王孟君,黄电源,姜海涛.汽车用铝合金的研究进展[J].金属热处理,2006,31(9):34-38. 被引量:93
9冯光纯.发展冷弯型钢[J].四川冶金,1997,19(1):55-58. 被引量:2
10林伯颖.关于我国硬质合金工业科技进步的研讨[J].硬质合金,1994,11(4):246-251. 被引量:2
Basic Information:
DOI:
Chinese Library Classification Number:TG135.5[一般工业技术—材料科学与工程]
Citation Information:
The development of foreign cemen ted carbide technology isreviewed. the general description of the development of China 's cementedcarbide technology is made. Some suggestions are made for speeding-upthe development of China's cemented carbide industry.
quote
| GB/T 7714-2015 | [1] SHEN Dai-xiu, LI Mu-shan. Development of Cemented Carbide Technologyin China and Abroad[J]. Rare Metals and Cemented Carbides, 1995(1): 52-56. |
| MLA | [1] SHEN Dai-xiu, and LI Mu-shan. "Development of Cemented Carbide Technologyin China and Abroad." Rare Metals and Cemented Carbides, no. 1, 1995, pp. 52-56. |
| APA | [1] SHEN Dai-xiu, & LI Mu-shan. (1995). Development of Cemented Carbide Technologyin China and Abroad. Rare Metals and Cemented Carbides(1), 52-56. |
| IEEE | [1] SHEN Dai-xiu and LI Mu-shan, "Development of Cemented Carbide Technologyin China and Abroad," Rare Metals and Cemented Carbides, no. 1, pp. 52-56, 1995. keywords: {cemented carbide. technical dtvelopment, suggestion} |