Objective microstructure classification by support vector machine (SVM) using a combination of morphological parameters and textural features for low carbon steels AITranslate
Abstract AITranslate
Highlights • SVM-based classification of steelusing textural features and morphological parameters. • A combination of different parameter groups leads to the highest classification result. • Significant parameters could show the same range of accuracy as the whole dataset. The variety of modern steels is growing steadily. In order to meet the ever tighter tolerance ranges for the properties of these steels, it is important to both understand the manufacturing process as accurately as possible and to be able to correctly classify the microstructure. The microstructure acts as a link between the production and the properties, which acts as an information storage, which must be read out and understood in the best way to develop new steels. For this reason, it is of utmost importance to have an objective and reproducible microstructure classification available. The present study demonstrates that using a support vector machine in combination with pixel-based and morphology-based parameters allows a reliable classification based on microstructural images. In order to determine the parameters correlative microscopy is used to collect a large variety of information about the different steel structures. The significance of the different parameter groups for the classification success and the correlation of the parameters with each other are investigated. The minimum number of parameters required for a reliable classification is determined by evolutionary feature selection. Graphical abstract Download : Download high-res image (190KB) Download : Download full-size image
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1016/j.commatsci.2019.01.006
Chinese Library Classification Number:
Citation Information:
Highlights • SVM-based classification of steelusing textural features and morphological parameters. • A combination of different parameter groups leads to the highest classification result. • Significant parameters could show the same range of accuracy as the whole dataset. The variety of modern steels is growing steadily. In order to meet the ever tighter tolerance ranges for the properties of these steels, it is important to both understand the manufacturing process as accurately as possible and to be able to correctly classify the microstructure. The microstructure acts as a link between the production and the properties, which acts as an information storage, which must be read out and understood in the best way to develop new steels. For this reason, it is of utmost importance to have an objective and reproducible microstructure classification available. The present study demonstrates that using a support vector machine in combination with pixel-based and morphology-based parameters allows a reliable classification based on microstructural images. In order to determine the parameters correlative microscopy is used to collect a large variety of information about the different steel structures. The significance of the different parameter groups for the classification success and the correlation of the parameters with each other are investigated. The minimum number of parameters required for a reliable classification is determined by evolutionary feature selection. Graphical abstract Download : Download high-res image (190KB) Download : Download full-size image
quote
| GB/T 7714-2015 | [1] Jessica Gola, Johannes Webel, Dominik Britz, et al. Computational Materials Science, 2019(160). DOI:10.1016/j.commatsci.2019.01.006. |
| MLA | [1] Jessica Gola, et al., Computational Materials Science, no. 160, 2019, https://doi.org/10.1016/j.commatsci.2019.01.006. |
| APA | [1] Jessica Gola, Johannes Webel, Dominik Britz, Agustina Guitar, Thorsten Staudt, Marc Winter, & Frank Mücklich. (2019). Computational Materials Science(160). https://doi.org/10.1016/j.commatsci.2019.01.006 |
| IEEE | [1] Jessica Gola, Johannes Webel, Dominik Britz, Agustina Guitar, Thorsten Staudt, Marc Winter, and Frank Mücklich, Computational Materials Science, no. 160, 2019, doi: 10.1016/j.commatsci.2019.01.006. |