daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Preparation of WC Powder Containing Yttrium by Co-precipitation AITranslate

School of Materials Science and Engineering,Nanchang University;School of Materials Science and Engineering,Nanchang University;School of Materials Science and Engineering,Nanchang University;School of Materials Science and Engineering,Nanchang University;School of Materials Science and Engineering,Nanchang University;School of Materials Science and Engineering,Nanchang University;School of Materials Science and Engineering,Nanchang University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The process of doping yttrium by co-precipitation with yttrium nitrate aqueous solution added during evaporation crystallization of ammonium tungstate was studied. Yttrium-doped ammonium paratungstate powder was prepared by the above process,and then tungsten carbide powder containing yttrium was prepared by redox,carbon distribution and carbonization.The results show that yttrium in APT pow der prepared by co-precipitation has relatively uniform distribution, and exists mainly in the form of Y(OH)3. The average particle sizes of tungsten carbide powders doped with 0.5%Y and 1%Y is 0.37μm and 0. 28μm,respectively.Yttrium doping has the effect of refining tungsten carbide powder.

KeyWords AITranslate

tungsten carbide powder yttrium doping co-precipitation ammonium paratungstate ammonium tungstate yttrium nitrate

1李洪全,郑树凯,丁帮福,闫小兵.钇掺杂亚稳相γ-Bi_2O_3的合成及光催化性能[J].中国粉体技术,2018,24(6):19-24. 被引量:1

2刘觐,易志强,张琳,黄红华,谭敦强,陆磊.化学沉淀法制备超细仲钨酸铵粉末的研究[J].江西科学,2019,37(3):405-408. 被引量:2

3朱锋,曾执一.电力企业的碳权性质和碳权的会计确认时间研究[J].广西电业,2019,0(3):43-46.

4杨丽.对钨酸铵蒸发结晶反应槽的改造的探讨[J].信息记录材料,2019,20(4):60-61. 被引量:1

5姜建辉,邓臣强,曹钰,刘永召,熊伟.Y和Si共掺杂纳米TiO2的制备及光催化性能[J].硅酸盐学报,2019,47(7):942-950. 被引量:12

6李颖,陈侠,苗淑兰,廖恩鑫.磷钨酸铵复合材料对铷铯吸附性能的研究[J].无机盐工业,2019,51(6):34-37. 被引量:1

7张文海,吉庆华,兰华春,李静.BiOCl-(NH_4)_3PW_(12)O_(40)复合光催化剂制备及其光催化降解污染物机制[J].环境科学,2019,40(3):1295-1301. 被引量:6

8樊国栋,郭萌.钇掺杂的铕三元配合物的制备及其性能研究[J].应用化工,2018,47(11):2394-2397. 被引量:5

9王玥,陈杉杉,马丽丽,林高安.不同单斜仲钨酸铵在惰性气体中的热分解研究[J].中国钨业,2019,34(1):58-63. 被引量:4

10刘铭哲,李斌川,韩庆,陈建设,刘奎仁.超细碳化钨粉末制备工艺研究进展[J].稀有金属与硬质合金,2019,47(2):74-81. 被引量:7

Basic Information:

DOI:

Chinese Library Classification Number:TG146.411[金属学及工艺—金属材料]

Citation Information:

The process of doping yttrium by co-precipitation with yttrium nitrate aqueous solution added during evaporation crystallization of ammonium tungstate was studied. Yttrium-doped ammonium paratungstate powder was prepared by the above process,and then tungsten carbide powder containing yttrium was prepared by redox,carbon distribution and carbonization.The results show that yttrium in APT pow der prepared by co-precipitation has relatively uniform distribution, and exists mainly in the form of Y(OH)3. The average particle sizes of tungsten carbide powders doped with 0.5%Y and 1%Y is 0.37μm and 0. 28μm,respectively.Yttrium doping has the effect of refining tungsten carbide powder.

quote

GB/T 7714-2015 [1] DENG Chong, TAN Dun-qiang, ZHU Hong-bo, et al. Preparation of WC Powder Containing Yttrium by Co-precipitation[J]. Rare Metals and Cemented Carbides, 2019(3): 31-35.
MLA [1] DENG Chong, et al., "Preparation of WC Powder Containing Yttrium by Co-precipitation." Rare Metals and Cemented Carbides, no. 3, 2019, pp. 31-35.
APA [1] DENG Chong, TAN Dun-qiang, ZHU Hong-bo, WANG Xiao-ru, HE Wen, YI Zhi-qiang, & KUANG Hai. (2019). Preparation of WC Powder Containing Yttrium by Co-precipitation. Rare Metals and Cemented Carbides(3), 31-35.
IEEE [1] DENG Chong, TAN Dun-qiang, ZHU Hong-bo, WANG Xiao-ru, HE Wen, YI Zhi-qiang, and KUANG Hai, "Preparation of WC Powder Containing Yttrium by Co-precipitation," Rare Metals and Cemented Carbides, no. 3, pp. 31-35, 2019. keywords: {tungsten carbide powder;yttrium doping;co-precipitation;ammonium paratungstate;ammonium tungstate;yttrium nitrate}