Effect of Arsenic on the Preparation and Carbonization Process of Violet Tungsten Oxide AITranslate

School of Materials Science and Engineering,Nanchang University;School of Materials Science and Engineering,Nanchang University;School of Materials Science and Engineering,Nanchang University;School of Materials Science and Engineering,Nanchang University;School of Materials Science and Engineering,Nanchang University;School of Materials Science and Engineering,Nanchang University;School of Materials Science and Engineering,Nanchang University;School of Materials Science and Engineering,Nanchang University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Arsenic (As) is a common impurity element in scheelite,and needs to be removed in the metallurgical process. However, the effect of arsenic on the subsequent tungsten products is not clear. APT-As composite powders with As mass content of 1% was prepared by using ammonium tungstate and As element as raw materials. After the treatment of calcination and carbonization, violet tungsten oxide(W18O49-As) and tungsten carbide (WC-As) containing arsenic were obtained, respectively.X-ray diffractometer, scanning electron microscope, high-resolution transmission electron microscope and differential scanning calorimeter were used to analyse the morphology and structure of W18O49-As and WC-As. The results show that As element mainly exists in the surface of the bar W18O49-As in the form of W2O3 (AsO4)2 phase,making bar W18O49-As easily break. The initial reaction temperatures of reduction and carbonization of W18O49-As are lower than those of W18O49. The phase of W2O3 (AsO4)2 is distributed between W18O49 powders,hindering substance migration and diffusion in the process of W18O49 carbonization and inhibiting aggregation and growth of fine WC particles,so the uniform WC-As powders are obtained.

KeyWords AITranslate

arsenic violet tungsten oxide tungsten carbide uniformity

1谭敦强,李亚蕾,杨欣,陆磊,陆德平.杂质元素对钨产品结构及性能的影响[J].材料导报,2013,27(17):98-100. 被引量:5

2李洪桂,孙培梅,李运姣,起中伟,苏鹏抟,刘茂盛.选择性沉淀法从钨酸盐溶液中除钼、砷、锑、锡等杂质的研究[J].中国钨业,1998,13(4):17-19. 被引量:19

3张湘.直接碳化技术制备碳化钨粉的研究[J].硬质合金,2013,30(2):73-78. 被引量:2

4张永会,傅声华,李飞.紫色氧化钨的制备及工艺研究[J].中国钨业,2011,26(3):47-49. 被引量:8

5王岗,李海华,黄忠伟,陈美华,王庆康,钟伟良.蓝钨与紫钨氢还原法生产超细钨粉的比较[J].稀有金属材料与工程,2009,38(A01):548-552. 被引量:17

6宋志华,郭亨群,吴冲浒,吴其山.以紫钨为原料制备纳米钨粉体的研究[J].稀有金属材料与工程,2011,40(12):2216-2220. 被引量:9

7张久兴,张国珍,张利平,王澈,宋晓艳,周美玲,钟涛兴.氧化钨/碳SPS原位合成WC硬质合金的XPS研究[J].稀有金属材料与工程,2006,35(6):937-940. 被引量:4

1魏庭民,李志锋,林钊,张永会,陈伟豪.紫色氧化钨制备工艺研究[J].世界有色金属,2022(20):163-165.

1袁卓敏,李继林,王孟君,刘明阳,李永杰.超声波和均匀化处理对Al-Mg-Si-Sn合金铸态组织的影响[J].铸造技术,2018,39(12):2861-2865. 被引量:1

2刘觐,易志强,张琳,黄红华,谭敦强,陆磊.化学沉淀法制备超细仲钨酸铵粉末的研究[J].江西科学,2019,37(3):405-408. 被引量:2

3赵经纬,刘贞山,曹以恒,赵丕植.冷轧率与退火工艺对汽车用5754铝合金组织演变的影响[J].材料导报,2018,32(A02):365-370. 被引量:1

4王玥,陈杉杉,马丽丽,林高安.不同单斜仲钨酸铵在惰性气体中的热分解研究[J].中国钨业,2019,34(1):58-63. 被引量:4

5曹宇,邓松云,朱玉涛,李睿,赵解扬,周文标,王华春.3C电子产品用高强度Al-Mg铝合金薄板热处理工艺研究[J].热加工工艺,2019,48(2):199-201. 被引量:2

6陆向科,王孟君,李新涛,康跃华,王顺成.超声波功率对半连续铸造6013铝合金组织与力学性能的影响[J].轻合金加工技术,2019,47(5):25-29. 被引量:7

7郭鹏杰,张星,李保成,任耀.AZ80镁合金第二相体积分数对其拉伸性能的影响[J].金属热处理,2019,44(3):46-49. 被引量:9

8韩杰.热处理对Ti微合金钢组织性能的影响[J].山东冶金,2019,41(3):20-22. 被引量:2

9陈爱华,李婷婷,李腾飞,李化龙.220 MPa级烘烤硬化钢的组织和力学性能研究[J].热加工工艺,2019,48(2):247-250. 被引量:1

10党军杰,胡竹松,郭军,田晨光,孙登琼,张浩,崔嵩.不同相结构和微观结构对氮化铝陶瓷性能的影响[J].真空电子技术,2019,0(3):59-63.

Basic Information:

DOI:

Chinese Library Classification Number:TG146.411[金属学及工艺—金属材料]

Citation Information:

Arsenic (As) is a common impurity element in scheelite,and needs to be removed in the metallurgical process. However, the effect of arsenic on the subsequent tungsten products is not clear. APT-As composite powders with As mass content of 1% was prepared by using ammonium tungstate and As element as raw materials. After the treatment of calcination and carbonization, violet tungsten oxide(W18O49-As) and tungsten carbide (WC-As) containing arsenic were obtained, respectively.X-ray diffractometer, scanning electron microscope, high-resolution transmission electron microscope and differential scanning calorimeter were used to analyse the morphology and structure of W18O49-As and WC-As. The results show that As element mainly exists in the surface of the bar W18O49-As in the form of W2O3 (AsO4)2 phase,making bar W18O49-As easily break. The initial reaction temperatures of reduction and carbonization of W18O49-As are lower than those of W18O49. The phase of W2O3 (AsO4)2 is distributed between W18O49 powders,hindering substance migration and diffusion in the process of W18O49 carbonization and inhibiting aggregation and growth of fine WC particles,so the uniform WC-As powders are obtained.

quote

GB/T 7714-2015 [1] YI Zhi-qiang, TU Dan, TAN Dun-qiang, et al. Effect of Arsenic on the Preparation and Carbonization Process of Violet Tungsten Oxide[J]. Rare Metals and Cemented Carbides, 2019(3): 25-30.
MLA [1] YI Zhi-qiang, et al., "Effect of Arsenic on the Preparation and Carbonization Process of Violet Tungsten Oxide." Rare Metals and Cemented Carbides, no. 3, 2019, pp. 25-30.
APA [1] YI Zhi-qiang, TU Dan, TAN Dun-qiang, WANG Xiao-ru, HE Wen, KUANG Hai, ZOU Zhi-hang, & DENG Chong. (2019). Effect of Arsenic on the Preparation and Carbonization Process of Violet Tungsten Oxide. Rare Metals and Cemented Carbides(3), 25-30.
IEEE [1] YI Zhi-qiang, TU Dan, TAN Dun-qiang, WANG Xiao-ru, HE Wen, KUANG Hai, ZOU Zhi-hang, and DENG Chong, "Effect of Arsenic on the Preparation and Carbonization Process of Violet Tungsten Oxide," Rare Metals and Cemented Carbides, no. 3, pp. 25-30, 2019. keywords: {arsenic;violet tungsten oxide;tungsten carbide;uniformity}