Research Progress of Lithium Manganese Iron Phosphate as Cathode Material for Lithium Ion Batteries AITranslate
Abstract AITranslate
At present,the energy density of lithium iron phosphate,the mainstream cathode material for lithium ion batteries in the market,has almost reached its limit,while lithium manganese iron phosphate is expected to break this bottleneck.Lithium ion batteries with lithium manganese iron phosphate as the ca-thode material offer advantages of high voltage,high energy density,and better low-temperature stability.This paper describes the characteristics of structure and performance of lithium manganese iron phosphate,introduces the latest research progress in its preparation methods,and discusses the deficiencies of these methods.Finally,this paper looks ahead to the future development directions and application prospects of lithium manganese iron phosphate.
KeyWords AITranslate
Basic Information:
DOI:
Chinese Library Classification Number:TB34[一般工业技术—材料科学与工程]
Citation Information:
At present,the energy density of lithium iron phosphate,the mainstream cathode material for lithium ion batteries in the market,has almost reached its limit,while lithium manganese iron phosphate is expected to break this bottleneck.Lithium ion batteries with lithium manganese iron phosphate as the ca-thode material offer advantages of high voltage,high energy density,and better low-temperature stability.This paper describes the characteristics of structure and performance of lithium manganese iron phosphate,introduces the latest research progress in its preparation methods,and discusses the deficiencies of these methods.Finally,this paper looks ahead to the future development directions and application prospects of lithium manganese iron phosphate.
quote
| GB/T 7714-2015 | [1] HUANG Zong-peng, TAN Xin, LI Chuan-zong, et al. Research Progress of Lithium Manganese Iron Phosphate as Cathode Material for Lithium Ion Batteries[J]. Rare Metals and Cemented Carbides, 2024(4): 84-89. |
| MLA | [1] HUANG Zong-peng, et al., "Research Progress of Lithium Manganese Iron Phosphate as Cathode Material for Lithium Ion Batteries." Rare Metals and Cemented Carbides, no. 4, 2024, pp. 84-89. |
| APA | [1] HUANG Zong-peng, TAN Xin, LI Chuan-zong, CHEN Yu-yang, ZHOU Yong, & PENG Jun. (2024). Research Progress of Lithium Manganese Iron Phosphate as Cathode Material for Lithium Ion Batteries. Rare Metals and Cemented Carbides(4), 84-89. |
| IEEE | [1] HUANG Zong-peng, TAN Xin, LI Chuan-zong, CHEN Yu-yang, ZHOU Yong, and PENG Jun, "Research Progress of Lithium Manganese Iron Phosphate as Cathode Material for Lithium Ion Batteries," Rare Metals and Cemented Carbides, no. 4, pp. 84-89, 2024. keywords: {lithium manganese iron phosphate;lithium ion battery;cathode material;preparation method;research progress} |