Study on Solvothermal Synthesis and Photocatalytic Properties ofβ-In2Se3 AITranslate
Abstract AITranslate
β-In2Se3 is widely used in various fields due to its good mobility and excellent photoresponse.However,Due to the fact that In2Se3 has multiple complex crystal structures and indium is prone to hydro-lysis,it is difficult to prepare layeredβ-In2Se3 in solution.Using InCl3,Se powder and ethylenediamine as raw materials,β-In2Se3 powder was prepared by the solvothermal method.The structure,morphology and optical properties of the powder were characterized by Raman spectrometer,Fourier infrared spectrometer,thermogravimetric analyzer,scanning electron microscope and fluorescence spectrophotometer.The photocatalytic properties of the powders were investigated using methyl orange solution as the degradation substance.The results show that the main component of the prepared powder isβ-In2Se3 with a layered structure.The powder has good absorption in the UV and visible light regions,with an optical bandgap of approximately 2.01 eV,and has excellent fluorescent properties.β-In2Se3 powder exhibits photocatalytic activity towards methyl orange,and after 5 h of UV irradiation,the degradation rate of methyl orange can reach 81%.The result expands the application ofβ-In2Se3 for the degradation of organic pollutants.
KeyWords AITranslate
Basic Information:
DOI:
Chinese Library Classification Number:TQ426.62[化学工程]
Citation Information:
β-In2Se3 is widely used in various fields due to its good mobility and excellent photoresponse.However,Due to the fact that In2Se3 has multiple complex crystal structures and indium is prone to hydro-lysis,it is difficult to prepare layeredβ-In2Se3 in solution.Using InCl3,Se powder and ethylenediamine as raw materials,β-In2Se3 powder was prepared by the solvothermal method.The structure,morphology and optical properties of the powder were characterized by Raman spectrometer,Fourier infrared spectrometer,thermogravimetric analyzer,scanning electron microscope and fluorescence spectrophotometer.The photocatalytic properties of the powders were investigated using methyl orange solution as the degradation substance.The results show that the main component of the prepared powder isβ-In2Se3 with a layered structure.The powder has good absorption in the UV and visible light regions,with an optical bandgap of approximately 2.01 eV,and has excellent fluorescent properties.β-In2Se3 powder exhibits photocatalytic activity towards methyl orange,and after 5 h of UV irradiation,the degradation rate of methyl orange can reach 81%.The result expands the application ofβ-In2Se3 for the degradation of organic pollutants.
quote
| GB/T 7714-2015 | [1] LYU Bao-hua, JIA Rong, JING Xiao-xia, et al. Study on Solvothermal Synthesis and Photocatalytic Properties ofβ-In2Se3[J]. Rare Metals and Cemented Carbides, 2024(4): 78-83. |
| MLA | [1] LYU Bao-hua, et al., "Study on Solvothermal Synthesis and Photocatalytic Properties ofβ-In2Se3." Rare Metals and Cemented Carbides, no. 4, 2024, pp. 78-83. |
| APA | [1] LYU Bao-hua, JIA Rong, JING Xiao-xia, GUO Gui-zheng, & WANG Yu-chun. (2024). Study on Solvothermal Synthesis and Photocatalytic Properties ofβ-In2Se3. Rare Metals and Cemented Carbides(4), 78-83. |
| IEEE | [1] LYU Bao-hua, JIA Rong, JING Xiao-xia, GUO Gui-zheng, and WANG Yu-chun, "Study on Solvothermal Synthesis and Photocatalytic Properties ofβ-In2Se3," Rare Metals and Cemented Carbides, no. 4, pp. 78-83, 2024. keywords: {β-InSe;layered structure;solvothermal method;optical property;photocatalysis} |