Meta-Aerogels: Auxetic Shape-Memory Polyurethane Aerogels AITranslate

NASA Glenn Research Center, 21000 Brookpark Road; Missouri University of Science and Technology; The University of Texas at Dallas; The University of Texas at Dallas; Missouri University of Science and Technology; Missouri University of Science and Technology; The University of Texas at Dallas;NASA Glenn Research Center, 21000 Brookpark Road; Missouri University of Science and Technology; Missouri University of Science and Technology; The University of Texas at Dallas
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Shape-memory poly(isocyanurate–urethane) (PIR–PUR) aerogels are low-density monolithic nanoporous solids that remember and return to their permanent shape through a heating actuation step. Herein, through structural design at the macro scale, the shape-memory response is augmented with an auxetic effect manifested by a negative Poisson’s ratio of approximately −0.8 at 15% compressive strain. Thus, auxetic shape-memory PIR–PUR monoliths experience volume contraction upon compression at a temperature above the glass transition temperature of the base polymer (Tg ≈ 30 °C), and they can be stowed indefinitely in that temporary shape by cooling below Tg. By heating back above Tg, the compressed/shrunk form expands back to their original shape/size. This technology is relevant to a broad range of industries spanning the commercial, aeronautical, and aerospace sectors. The materials are referred to as meta-aerogels, and their potential applications include minimally invasive medical devices, soft robotics, and situations where volume is at a premium, as for example for storage of deployable space structures and planetary habitats during transport to the point of service.

KeyWords AITranslate

shape memory polymer aerogel auxetic metamaterial negative Poisson’s ratio
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c00987

Chinese Library Classification Number:

Citation Information:

Shape-memory poly(isocyanurate–urethane) (PIR–PUR) aerogels are low-density monolithic nanoporous solids that remember and return to their permanent shape through a heating actuation step. Herein, through structural design at the macro scale, the shape-memory response is augmented with an auxetic effect manifested by a negative Poisson’s ratio of approximately −0.8 at 15% compressive strain. Thus, auxetic shape-memory PIR–PUR monoliths experience volume contraction upon compression at a temperature above the glass transition temperature of the base polymer (Tg ≈ 30 °C), and they can be stowed indefinitely in that temporary shape by cooling below Tg. By heating back above Tg, the compressed/shrunk form expands back to their original shape/size. This technology is relevant to a broad range of industries spanning the commercial, aeronautical, and aerospace sectors. The materials are referred to as meta-aerogels, and their potential applications include minimally invasive medical devices, soft robotics, and situations where volume is at a premium, as for example for storage of deployable space structures and planetary habitats during transport to the point of service.

quote

GB/T 7714-2015 [1] Sadeq Malakooti, A. B. M. Shaheen ud Doulah, Yao Ren, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c00987.
MLA [1] Sadeq Malakooti, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c00987.
APA [1] Sadeq Malakooti, A. B. M. Shaheen ud Doulah, Yao Ren, Vijay N. Kulkarni, Rushi U. Soni, Vaibhav A. Edlabadkar, Runyu Zhang, Stephanie L. Vivod, Chariklia SotiriouLeventis, Nicholas Leventis, & Hongbing Lu. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c00987
IEEE [1] Sadeq Malakooti, A. B. M. Shaheen ud Doulah, Yao Ren, Vijay N. Kulkarni, Rushi U. Soni, Vaibhav A. Edlabadkar, Runyu Zhang, Stephanie L. Vivod, Chariklia SotiriouLeventis, Nicholas Leventis, and Hongbing Lu, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.1c00987. keywords: {shape memory;polymer;aerogel;auxetic;metamaterial;negative Poisson’s ratio}