daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Sustainable Electrospun Affinity Membranes for Water Remediation by Removing Metal and Metal Oxide Nanoparticles AITranslate

University of Bayreuth; Zhejiang University; University of Bayreuth
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Nanoparticles (NPs) as part of engineered nanomaterials (ENMs) possess outstanding properties. Thus, they are more frequently integrated into various products resulting in high annual production quantities. The consequence can be the unintentional release into the environment where NPs could accumulate and pose a threat to human health. Therefore, the strong need becomes apparent for the remediation of environmental media. Electrospun nonwovens, which are defined here as membranes, could efficiently remove these released NPs. In this paper, electrospun membranes are utilized to flow filtration of metal and metal oxide NP, such as gold, silver, copper oxide, zinc oxide, iron oxide, and titanium dioxide. The membrane–NP interaction was analyzed and the correlation between NP size, NP ligand, ligand concentration, and the membrane surface functional group was investigated systematically. Finally, a membrane combining two functional groups was designed, which is able to adsorb up to 100% of the filtered NPs. The highest adsorption capacity was provided by AuNPs with 0.14 mg NP/mg membrane. To enhance their lifetime and gain sustainability, the membranes were then regenerated three times by rinsing with low concentrated acids. No significant efficiency loss was recorded, which allowed reusability of the electrospun membranes. We believe that the results shown here are of general relevance for other metals, metal oxides, and microplastic particles as well.

KeyWords AITranslate

electrospun membrane affinity separation ligands metal nanoparticles membrane regeneration
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c00990

Chinese Library Classification Number:

Citation Information:

Nanoparticles (NPs) as part of engineered nanomaterials (ENMs) possess outstanding properties. Thus, they are more frequently integrated into various products resulting in high annual production quantities. The consequence can be the unintentional release into the environment where NPs could accumulate and pose a threat to human health. Therefore, the strong need becomes apparent for the remediation of environmental media. Electrospun nonwovens, which are defined here as membranes, could efficiently remove these released NPs. In this paper, electrospun membranes are utilized to flow filtration of metal and metal oxide NP, such as gold, silver, copper oxide, zinc oxide, iron oxide, and titanium dioxide. The membrane–NP interaction was analyzed and the correlation between NP size, NP ligand, ligand concentration, and the membrane surface functional group was investigated systematically. Finally, a membrane combining two functional groups was designed, which is able to adsorb up to 100% of the filtered NPs. The highest adsorption capacity was provided by AuNPs with 0.14 mg NP/mg membrane. To enhance their lifetime and gain sustainability, the membranes were then regenerated three times by rinsing with low concentrated acids. No significant efficiency loss was recorded, which allowed reusability of the electrospun membranes. We believe that the results shown here are of general relevance for other metals, metal oxides, and microplastic particles as well.

quote

GB/T 7714-2015 [1] AnnKathrin Müller, ZhiKang Xu, Andreas Greiner. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c00990.
MLA [1] AnnKathrin Müller, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c00990.
APA [1] AnnKathrin Müller, ZhiKang Xu, & Andreas Greiner. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c00990
IEEE [1] AnnKathrin Müller, ZhiKang Xu, and Andreas Greiner, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.1c00990. keywords: {electrospun membrane;affinity separation;ligands;metal nanoparticles;membrane regeneration}