Study on Reducing Fluorine Content in Ammonium Molybdate Solution by Active Magnesium Oxide AITranslate
Abstract AITranslate
The fluorine removal effects from ammonium molybdate solution by different magnesium salts and aluminum salts such as magnesium sulfate, active magnesium oxide, active alumina and aluminum sulfate were compared.And active magnesium oxide is determined to be the reagent for removing fluoride ions from ammonium molybdate solution.The effects of reaction temperature, addition amount of magnesium oxide, reaction time and solution pH on fluorine removal by active magnesium oxide were emphatically investigated.The results show that the fluorine content in ammonium molybdate solution can be reduced by more than 90% under the conditions as follows: solution pH of 7~7.5,reaction temperature of 60 ℃,magnesium oxide addition amount of 2.5 times the fluorine content, and stirring reaction time of 1 h.
KeyWords AITranslate
1肖连生.中国钨提取冶金技术的进步与展望[J].有色金属科学与工程,2013,4(5):6-10. 被引量:20
2罗军,袁喜振.溶剂萃取法提取钨研究现状[J].中国钨业,2017,32(2):56-59. 被引量:5
3王文强,赵中伟.钨提取冶金中钨钼分离研究进展——从“削足适履”到“量体裁衣”[J].中国钨业,2015,30(1):49-55. 被引量:7
4赵文迪,章晓林,王其宏,景满,申培伦.钨钼分离工艺及机理研究进展[J].有色金属工程,2019,9(4):41-48. 被引量:5
5陈杰山.国内除氟吸附剂的研究进展[J].广州化工,2015,43(19):18-20. 被引量:3
6王慧玲,张彦艳,徐微,花日茂,李学德.改性活性氧化镁的除氟效能及机制[J].环境工程学报,2015,9(5):2125-2130. 被引量:5
7吕亚娟,白林,严子春.活性氧化镁除氟条件的研究[J].甘肃高师学报,2010,15(5):22-24. 被引量:6
8赵炳翔,崔瑞璞,王晓凤,成杰民.活性氧化铝对水中F-的吸附特性及其影响因素[J].云南化工,2019,46(2):121-123. 被引量:5
9李德贵,王贤婷.硫酸铝改性活性氧化铝的除氟性能试验研究[J].材料研究与应用,2015,9(1):32-35. 被引量:11
10王文斌.硫酸铝除氟在金隆公司废水处理工艺中的应用[J].铜业工程,2019(1):101-103. 被引量:7
1齐海丽,吕云皓,杨双铭,江英.黑枸杞果醋发酵工艺条件优化[J].中国酿造,2021,40(12):204-210. 被引量:7
2尼格尔热依·亚迪卡尔,邓淑萍,白玉,古丽皮耶·吾普尔.超声辅助提取薰衣草总三萜的工艺优化及体外抗氧化活性研究[J].食品工业科技,2022,43(3):172-179. 被引量:4
3朱永红,范震宇,韩勇,吴雯仪,蔡亮亮.蒲公英根多糖硫酸酯化工艺条件优化及其对HepaRG细胞氧化损伤的保护作用[J].天然产物研究与开发,2021,33(12):2082-2089.
4鲁云风,张四普,牛佳佳,唐存多,杨永峰,江建荣.猕猴桃百香果酒工艺条件优化[J].食品研究与开发,2022,43(1):105-109. 被引量:5
5李双祁,刘国峰,王亚惠,赵肃清.灵芝发酵工艺条件优化及美白因子探析[J].湖南农业大学学报:自然科学版,2021,47(6):655-662. 被引量:2
6金海炎,王丰园,鲁云风,张四普,牛佳佳,唐存多,左卫芳,杨永峰.混菌发酵猕猴桃果酒工艺条件优化及抗氧化性研究[J].食品与发酵工业,2022,48(3):177-185. 被引量:20
7王吉坤.臭氧催化剂对煤化工高盐废水有机物去除性能研究[J].煤质技术,2022,37(1):39-45. 被引量:2
8刘宏,谢桂容.桐油酸改性苯-丙烯酸酯乳液合成工艺条件优化[J].广东化工,2022,49(2):9-11.
9杨桂磊,徐旭峰,徐志远,郭中权,杨洋,郑利祥,黄文先,崔东锋.含氟矿井水除浊除氟处理试验研究[J].能源环境保护,2022,36(1):66-71. 被引量:4
10章丽萍,吴二勇,姚瑞涵,安逸云,郭湘帅,刘金辰,闫晋蒙.高效除氟药剂对神东矿区含氟矿井水的处理研究[J].干旱区资源与环境,2022,36(2):84-90. 被引量:4
Basic Information:
DOI:
Chinese Library Classification Number:TF803.25[冶金工程—有色金属冶金]
Citation Information:
The fluorine removal effects from ammonium molybdate solution by different magnesium salts and aluminum salts such as magnesium sulfate, active magnesium oxide, active alumina and aluminum sulfate were compared.And active magnesium oxide is determined to be the reagent for removing fluoride ions from ammonium molybdate solution.The effects of reaction temperature, addition amount of magnesium oxide, reaction time and solution pH on fluorine removal by active magnesium oxide were emphatically investigated.The results show that the fluorine content in ammonium molybdate solution can be reduced by more than 90% under the conditions as follows: solution pH of 7~7.5,reaction temperature of 60 ℃,magnesium oxide addition amount of 2.5 times the fluorine content, and stirring reaction time of 1 h.
quote
| GB/T 7714-2015 | [1] DU Kai-liang, JING Shi-gun, JIA Wei, et al. Study on Reducing Fluorine Content in Ammonium Molybdate Solution by Active Magnesium Oxide[J]. Rare Metals and Cemented Carbides, 2021(6): 15-19. |
| MLA | [1] DU Kai-liang, et al., "Study on Reducing Fluorine Content in Ammonium Molybdate Solution by Active Magnesium Oxide." Rare Metals and Cemented Carbides, no. 6, 2021, pp. 15-19. |
| APA | [1] DU Kai-liang, JING Shi-gun, JIA Wei, LI Xiao-yu, WANG Xin-xin, CHEN Li-ge, ZHAO Si-fang, & JU Cheng-xin. (2021). Study on Reducing Fluorine Content in Ammonium Molybdate Solution by Active Magnesium Oxide. Rare Metals and Cemented Carbides(6), 15-19. |
| IEEE | [1] DU Kai-liang, JING Shi-gun, JIA Wei, LI Xiao-yu, WANG Xin-xin, CHEN Li-ge, ZHAO Si-fang, and JU Cheng-xin, "Study on Reducing Fluorine Content in Ammonium Molybdate Solution by Active Magnesium Oxide," Rare Metals and Cemented Carbides, no. 6, pp. 15-19, 2021. keywords: {ammonium molybdate solution;fluorine removal;active magnesium oxide;optimization of technical condition} |