Research on the Phenomena of Grain Growth during the Sintering of WC-Co Hard Alloy AITranslate
Abstract AITranslate
The mechanism of the grain growth is analyzed. During the sintering of WC-Co powder, grain is grown in normal way and abnormally way. WC grain begins to grow at the early sintering. The measures to inhibit the WC grain growth are proposed.
KeyWords AITranslate
1Almond E A,Roebuck B.Very fine-grained hard metals[J].Int J Refract M Hard Mat,1987,6(3):137-144.
2高勇,唐振方,黄景清,郑家概,凌育远,钟红海.纳米WC-Co复合材料制备及其烧结过程[J].硬质合金,2000,17(1):18-20. 被引量:35
3范景莲,李志希,缪群,黄伯云,吴恩熙.超细纳米硬质合金及晶粒长大抑制剂的研究[J].粉末冶金技术,2004,22(5):259-265. 被引量:35
4Yoon B K,Lee B A,Kang S L.Growth behavior of rounded (Ti,W)C and faceted WC grains in a Co matrix during liquid phase sintering[J].Acta Mater,2005,53:4 677-4 685.
5Sommer M,Schubert W D,Zobetz P,et al.On the formation of very large WC crystals during sintering of ultrafine WC-Co alloys[J].Int J Refract M Hard Mat,2002,20(1):41-45.
6Kang S L,Han S M.Grain growth in Si3N4-based materials[J].MRS Bull,1995,20:33.
7Kang S L.Sintering:densification,grain growth and microstructure[M].London:Elsevier,2005.
8Park Y J,Hwang N M,Yoon D Y.Abnormal growth of faceted (WC) grainsin a (Co) liquid matrix[J].Metall Mater Trans A,1996,27A:2 809-2 819.
9Kang M K,Kim D Y,Hwang N M,et al.Ostwald ripening kinetics of angular grains dispersed in a liquid phase by two-dimensional nucleation and abnormal grain growth[J].J Eur Ceram Soc,2002,22:603-612.
10Rohrer G S,Rohrer C L,Mullins W W.Coarsening of faceted crystals[J].J Am Ceram Soc,2002,85:675.
1刘雪梅,宋晓艳,刘文彬,赵世贤,张久兴,殷福星.热压和放电等离子烧结对硬质合金材料微观组织和性能的影响[J].电子显微学报,2009,28(1):1-5. 被引量:3
2雷贻文,吴恩熙.VC/Cr_3C_2添加剂与烧结温度对超细WC-12Co硬质合金的影响[J].材料科学与工艺,2010,18(3):405-409. 被引量:7
3袁明健,顾金宝.氢气脱蜡工艺与原料WC碳量的选择[J].硬质合金,2010,27(5):293-297. 被引量:2
4饶承毅.不同烧结温度下超细合金烧结体的密度、钴磁和晶粒度[J].硬质合金,2011,28(3):143-147. 被引量:4
5蔡海燕.矿用硬质合金WC晶粒均匀性及板状形貌异常长大的控制[J].硬质合金,2014,31(4):230-235. 被引量:4
6石丽秋,王晓灵,熊超伟.球磨时间对双晶结构的WC-TiC-Co/Ni硬质合金组织及性能的影响[J].硬质合金,2015,32(3):155-163. 被引量:4
7李金普,丁存光,李一,柳学全,李楠,李发长.低压烧结温度对YG15粗晶硬质合金性能的影响[J].硬质合金,2016,33(1):33-37. 被引量:4
8樊小琴,贺端威,王培,李东,刘银娟,杜雁春.低钴粗晶硬质合金的高压融渗法制备[J].高压物理学报,2017,31(1):8-14.
9刘志芳,梁瑜,钟腾飞,郭永忠,覃伟坚,汤昌仁.WC粉末碳化工艺与球磨时间对亚微晶硬质合金显微组织与性能的影响[J].中国钨业,2019,34(6):48-53. 被引量:5
10马赛.细晶碳化钨粉末特性对硬质合金晶粒异常长粗的影响[J].数码设计,2020,9(5):44-46.
1邓四文.相同硬度的高钴和低钴含量硬质合金性能比较[J].理化检验:物理分册,2022,58(6):21-25.
2迟静,李惠琪,王淑峰,李敏.矿用WC硬质合金的研究进展与趋势[J].矿山机械,2010,38(8):23-28. 被引量:7
3赵声志,张忠健.工艺条件对WC-12%Co超细硬质合金性能的影响[J].硬质合金,2012,29(3):141-145. 被引量:10
4陈颢,李剑波,羊建高.硬质合金回收研究进展及发展趋势[J].有色金属科学与工程,2012,3(5):18-22. 被引量:17
5姜中涛,李力,陈慧,刘兵,陈巧旺.一步还原法制备超细碳化钒铬粉末[J].粉末冶金材料科学与工程,2013,18(4):522-526. 被引量:2
6屈广林,颜练武,张卫兵,何惧.碳化钨和碳化钒在固相钴中的固溶研究[J].硬质合金,2014,31(1):8-14. 被引量:6
7赵然,马立民,郭福,胡扬端瑞,舒雨田.高优值系数In_4Se_3多晶的制备及其热电输运特性[J].无机材料学报,2015,30(3):249-255.
8张豪,叶金文,刘颖,马世卿.开放体系下碳热还原氮化法制备(Cr,Ta)_2CN固溶体粉末的研究[J].功能材料,2015,46(B06):71-74.
9涂彦坤,郑勇,赵毅杰,朱林正,黄琦.固相烧结阶段的升温速率对板状WC晶粒硬质合金的显微组织和力学性能的影响[J].硬质合金,2015,32(4):221-229. 被引量:2
10李韶雨,易健宏,李凤仙.烧结参数对超细晶铁粉的SPS烧结的影响[J].热加工工艺,2016,45(18):69-72. 被引量:4
1平冈裕,罗丽.Mo—0.2Ti合金的晶粒长大行为[J].钨钼材料,1997(4):8-10.
2余式昌,吴申庆,宫友军,宫元生,练明生.6Cr21Mn10MoVNbN气阀钢晶粒长大及其动力学研究[J].钢铁,2006,41(6):71-76. 被引量:5
3张春华,郭亨群,王国立,宋志华,吴冲浒,吴其山.纳米碳化钨粉的制备和晶粒粗化动力学研究[J].材料导报:纳米与新材料专辑,2009,23(2):129-131.
Basic Information:
DOI:
Chinese Library Classification Number:TG135.5[一般工业技术—材料科学与工程]
Citation Information:
The mechanism of the grain growth is analyzed. During the sintering of WC-Co powder, grain is grown in normal way and abnormally way. WC grain begins to grow at the early sintering. The measures to inhibit the WC grain growth are proposed.
quote
| GB/T 7714-2015 | [1] SUN Lan, JIA Cheng-chang, CAO Rui-jun, et al. Research on the Phenomena of Grain Growth during the Sintering of WC-Co Hard Alloy[J]. Rare Metals and Cemented Carbides, 2007(1): 44-47. |
| MLA | [1] SUN Lan, et al., "Research on the Phenomena of Grain Growth during the Sintering of WC-Co Hard Alloy." Rare Metals and Cemented Carbides, no. 1, 2007, pp. 44-47. |
| APA | [1] SUN Lan, JIA Cheng-chang, CAO Rui-jun, & LIU Zong. (2007). Research on the Phenomena of Grain Growth during the Sintering of WC-Co Hard Alloy. Rare Metals and Cemented Carbides(1), 44-47. |
| IEEE | [1] SUN Lan, JIA Cheng-chang, CAO Rui-jun, and LIU Zong, "Research on the Phenomena of Grain Growth during the Sintering of WC-Co Hard Alloy," Rare Metals and Cemented Carbides, no. 1, pp. 44-47, 2007. keywords: {WC-Co hard alloy;sintering process;grain growth} |