daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Current Research on Extraction of Mo from Wulfenite AITranslate

School of Chemistry, Central South University;School of Chemistry, Central South University;School of Chemistry, Central South University;School of Chemistry, Central South University;School of Chemistry, Central South University;School of Chemistry, Central South University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The characteristics of wulfenite and latest development of wulfenite extractive metallurgy were reviewed. Na2 S-leaching process, microbe-leaching process and mechanochemistry directly leaching process were introduced and compared, the result showed that Mo leaching ratio could reach 99% by mechanochemistry directly leaching process for wulfenite, in which process energy consumption was the lowest, and least equipment was needed,the newly developed process was the best way to recover Mo from wulfenite.

KeyWords AITranslate

wulfenite leaching Na2 S mechanochemist ry

1Gupta C K.Extractive metallurgy of molybdenum[M].London:CRC Press,1992.

2赵天丛.有色金属提取冶金手册·总论[M].北京:冶金工业出版社,1992.

3亚历山大·苏图洛夫.钼与铼[M].庄著学,译.西安:西安交通大学出版社,1991.

4Sasaki I.Method for regenerating molybdenum-containing oxide fluidized-bed catalyst[P].US Pat:6559085,2003-05-06.

5王滢.钼冶金进展[M].西安:西安冶金建筑学院,1980.

6张文钲.钼冶金[M].西安:西安交通大学出版社,1991..

7戴元宁.彩钼铅矿的化学分选方法[P].中国专利:1074486,1993-07-21.

8邹著适.用钼铅矿制取钼酸铵的试验[J].广州化工,1993,21(2):44-48. 被引量:5

9戴元宁.彩钼铅矿化学分选的研究[J].云南化工,1993,20(3):6-10. 被引量:7

10刘明力.生物浸出-萃取法分选彩钼铅矿的方法[P].中国专利:1614042A,2005-05-11.

1马飞,赵中伟,曹才放,张刚,霍广生,陈爱良,李洪桂.硫化钠分解彩钼铅矿热力学研究[J].中国钼业,2008,32(1):44-47. 被引量:9

2张文朴.加强钼资源综合利用与再生研发 促进我国生态钼业建设[J].中国钼业,2010,34(2):13-18. 被引量:3

3曹耀华,刘红召,高照国,杨绍文.低品位氧化钼精矿高压浸出新工艺[J].有色金属:冶炼部分,2011(1):5-8. 被引量:7

4曹耀华,吕良,刘红召,岳铁兵.小秦岭地区某低品位氧化钼铅矿选冶新技术研究[J].金属矿山,2012(9):72-75. 被引量:2

5曹耀华,刘红召,高照国,杨绍文.从高压碱浸液中提取钼钨新工艺[J].有色金属:冶炼部分,2012(10):27-29. 被引量:2

6曹耀华,王洪杰,刘红召,高照国.氧化钼钨粗精矿高压浸出液提取钼钨新工艺[J].稀有金属与硬质合金,2013,41(1):17-19. 被引量:2

7胡真,宋宝旭,邹坚坚,李汉文,汪泰,王成行,李秀娟.某稀土矿床中伴生彩钼铅矿的综合回收试验研究[J].有色金属:选矿部分,2013(B12):124-128. 被引量:5

8陈平炬,吴彦波,李艳,孔建河.小秦岭含金氧化钼铅矿选矿工艺实验研究[J].化工设计通讯,2017,43(2):59-59.

9傅开彬,汤鹏成,秦天邦,徐信,彭铁峰,陈梦君.贵州某彩钼铅矿焙烧浸出工艺研究[J].应用化工,2018,47(7):1437-1440. 被引量:1

10王素,齐向红,葛阳阳,田江涛,危刚.河南某低品位混合钼矿选矿试验研究[J].有色金属:选矿部分,2019,0(6):37-42. 被引量:4

1张文朴.加强钼资源综合利用与再生研发 促进我国生态钼业建设[J].中国钼业,2010,34(2):13-18. 被引量:3

2曹耀华,刘红召,高照国,杨绍文.从高压碱浸液中提取钼钨新工艺[J].有色金属:冶炼部分,2012(10):27-29. 被引量:2

3曹耀华,王洪杰,刘红召,高照国.氧化钼钨粗精矿高压浸出液提取钼钨新工艺[J].稀有金属与硬质合金,2013,41(1):17-19. 被引量:2

4黄迎红,王亚雄.钒钼铅矿浸出与钒钼分离试验研究[J].湿法冶金,2013,32(3):147-150. 被引量:2

5鲁兴武,易超,何国才,蒲敬文,李冠军,张析,余江鸿.钼酸铵硫化沉淀过程中钼损失试验研究[J].湿法冶金,2013,32(4):259-261. 被引量:5

6张鸿彪,牟文宁,宋佩,卢媛嫄,孙雷雷.钼矿冶炼新工艺发展概论[J].材料导报:纳米与新材料专辑,2013,27(2):87-90. 被引量:5

7杨玉珠,周强.2013年云南选矿年评[J].云南冶金,2014,43(2):19-30.

8谢铿,王海北,张邦胜.低品位钼矿及钼二次资源加压浸出工艺的研究进展[J].稀有金属与硬质合金,2014,42(3):23-27. 被引量:3

9吕振福,冯安生.几种矿产资源综合利用率计算方法的探讨[J].矿产保护与利用,2014,34(2):6-8. 被引量:12

10曹耀华,李清,高照国,刘红召,王威.低品位金钼混合精矿提取金钼新工艺[J].有色金属:冶炼部分,2014(7):42-44. 被引量:1

1李庚进.氧化锰矿直接浸出工艺的应用[J].中国锰业,1989(5):35-38. 被引量:7

2廖元双,杨大锦,鲁顺利.钼铅矿提钼工艺研究[J].有色金属:冶炼部分,2006(4):26-27. 被引量:9

3刘建华,包燕平,李太全,韩丽娜,董献,杨伶俐.高级别管线钢精炼工艺分析[J].北京科技大学学报,2007,29(8):789-792. 被引量:11

4王勇,韩晓兰.从低品位钼铅矿中提取钼的试验研究[J].湿法冶金,2012,31(4):237-239. 被引量:5

5柳兰生,陆业大,罗云鹏,张岩.锌直接浸出工艺中废电解液螺旋板换热器探讨[J].中国有色冶金,2014,43(3):31-33. 被引量:2

6黄迎红,王亚雄.钒钼铅矿浸出与钒钼分离试验研究[J].湿法冶金,2013,32(3):147-150. 被引量:2

7罗朝巍,曾睿,徐光耀,张建飞.难选钼镍矿处理工艺现状及开发[J].中国有色冶金,2015,44(4):25-27. 被引量:1

8张春生.兰坪氧化锌矿直接浸出工艺探析[J].有色金属设计,2010,37(1):10-14. 被引量:1

9东元.奥达(Odda)锌厂边改造边生产[J].世界有色金属,2003(6):61-61.

10郭鸿发.我国早期综合利用红土矿试验的回顾[J].不锈:市场与信息,2015,0(10):16-16.

Basic Information:

DOI:

Chinese Library Classification Number:TF841.2[冶金工程—有色金属冶金]

Citation Information:

The characteristics of wulfenite and latest development of wulfenite extractive metallurgy were reviewed. Na2 S-leaching process, microbe-leaching process and mechanochemistry directly leaching process were introduced and compared, the result showed that Mo leaching ratio could reach 99% by mechanochemistry directly leaching process for wulfenite, in which process energy consumption was the lowest, and least equipment was needed,the newly developed process was the best way to recover Mo from wulfenite.

quote

GB/T 7714-2015 [1] FU Jian-gang, WANG Hui, ZHONG Hong, et al. Current Research on Extraction of Mo from Wulfenite[J]. Rare Metals and Cemented Carbides, 2007(1): 41-43.
MLA [1] FU Jian-gang, et al., "Current Research on Extraction of Mo from Wulfenite." Rare Metals and Cemented Carbides, no. 1, 2007, pp. 41-43.
APA [1] FU Jian-gang, WANG Hui, ZHONG Hong, CHANG Qing-wei, WEI Zhi-feng, & MA Sheng-tao. (2007). Current Research on Extraction of Mo from Wulfenite. Rare Metals and Cemented Carbides(1), 41-43.
IEEE [1] FU Jian-gang, WANG Hui, ZHONG Hong, CHANG Qing-wei, WEI Zhi-feng, and MA Sheng-tao, "Current Research on Extraction of Mo from Wulfenite," Rare Metals and Cemented Carbides, no. 1, pp. 41-43, 2007. keywords: {wulfenite;leaching;Na2 S;mechanochemist ry}