Study of Ln_2O_3/X-13 Sieve as Catalyst for Esterification AITranslate
Abstract AITranslate
Ln2O3/X-13 sieve sorption (Ln= Nd,Sm,Tm,Lu, Dy ),prepared by immersioncalcination method,with 0.83% ~0. 93% RE oxides, has been proved to be quite effective as catalyst for esterification of aromatic phthalic acid or aliphatic acid with primary 2-ethylhexyl alcohol. For example. the conversion percentage of catalyst-bearing DOP is ~10% and 8% higher than that of catalyst-free DOP and X-13. And the conversion percentage of catalystbearing lOP is ~7% and ~4 % higher respectively than that of catalyst-free lOP and X-13. Furthermore, Ln2O3/X-13 sieve sorption contains ~25% less rare earth than Ln2O3/Al2O3 type esterification catalyst and esterification temperature is ~ 10℃ lower. It can be seen from the above that Ln2O3/X-13 sieve sorption is a very good esterification catalyst.
KeyWords AITranslate
1陈其瑞,张凤美,罗明润,焦肇林.混合镨钕氧化物催化合成DOP、DOM和DOA[J].稀有金属与硬质合金,1994,22(2):1-4. 被引量:5
2陈其瑞,张凤美,罗明润,焦肇林.Ln_2O_3/Al_2O_3催化酯化合成邻苯二甲酸二辛酯[J].催化学报(英文),1994,15(3):236-238. 被引量:20
3陈其瑞,罗明润,焦肇林,潘慧芳.提高稀土氧化物催化酯化活性的新方法[J].催化学报(英文),1991,12(6):494-497. 被引量:12
4陈其瑞,焦肇林,罗明润,潘慧芳.混合镨钕氧化物作为酯化催化剂的研究[J].稀土,1990,11(5):66-68. 被引量:13
5区兆华,陈子涛.分子筛催化酯化反应[J]科学通报,1985(06).
1江琦,李向召,高智勤.稀土在催化中的应用研究进展[J].信阳师范学院学报:自然科学版,2005,18(4):467-470. 被引量:7
2李永梅,徐勇军.稀土分子筛的合成与应用研究进展[J].广东化工,2009,36(3):47-50. 被引量:7
3陈其瑞,邵明霞.Ln_2O_3/ZrO_2催化合成DOP、DOM和DOA[J].稀有金属与硬质合金,2001,29(3):23-26. 被引量:1
1苏琼,陈辉,陆善祥.催化裂化催化剂的酸性调变方法[J].现代化工,2011,31(S1):43-46. 被引量:4
2赵永和,黄绍重,徐启杰,时文中.纳米固体酸催化聚合松香酯化反应的研究[J].信阳师范学院学报:自然科学版,2007,20(4):465-467. 被引量:2
3郑修成,叶文豪,袁程远,苏运来,王向宇.合成条件对硅基介孔分子筛结构的影响[J].信阳师范学院学报:自然科学版,2007,20(2):204-206. 被引量:4
4任彦瑾,施力.铈、铌改性镁铝尖晶石作为催化降烯烃助剂的研究[J].中国稀土学报,2008,26(1):1-5. 被引量:3
5王会嫣,汤恩旗,刘希东.稀土修饰的丝光沸石分子筛催化剂结构及性能研究[J].天津工业大学学报,2009,28(2):56-58. 被引量:1
6王艳,聂光华,但悠梦,杨一心.稀土配合物Nd(C5H8NO3)2(C3H5N2)2Cl3·4H2O的合成、表征及性能研究[J].信阳师范学院学报:自然科学版,2009,22(2):261-264. 被引量:1
7冯宜绥,刘洋.提高REY分子筛馏出口合格率[J].湖南农机:学术版,2010,37(4):45-45. 被引量:2
8冯宜绥.浅析降低REY分子筛原材料氯化稀土的单耗[J].甘肃科技,2011,27(10):34-35. 被引量:2
9蔡进军,丁伟,刘从华,黄校亮,滕秋霞.ZSM-5分子筛的复合改性及催化裂化性能[J].工业催化,2012,20(12):41-44. 被引量:8
10江甜,刘华伟,孔渝华.甲醇芳构化制对二甲苯催化剂的研究进展[J].化工设计通讯,2015,41(6):5-8. 被引量:3
1王守柱,陈其瑞.Ln_2O_3/x-13分子筛担载型催化剂的制备及其在合成DOP中的催化活性[J].安徽机电学院学报,1999(2):69-71.
2陈其瑞,罗明润,焦肇林,潘慧芳.稀土氧化物作为酯化反应催化剂的改进[J].应用化学,1991,8(1):92-94. 被引量:4
3翟智卫,杨双花.酯化反应研究进展[J].洛阳理工学院学报:自然科学版,2009,19(1):18-21. 被引量:3
4周文富,康为炜,陈从凤,孙金华,陈芳琴,陈水生.一种新型的酯化反应催化剂──三氯化钛催化合成柠檬酸三丁酯的研究[J].漳州师范学院学报:自然科学版,1999,12(3):49-54.
5朱传征,戴立益,赵泓,李伟,杨宝林,艾仁云.SO_4^(2-)/MO_2超强酸体系催化酯化性能研究[J].华东师范大学学报:自然科学版,1995(3):61-64.
6刘福安,李耀先,张景文,徐之雒,黄化民.高分子负载的二元羧酸酯化反应催化剂聚氯乙烯-三氯化铝·氯化锌[J].吉林大学自然科学学报,1991(1):120-122. 被引量:2
7于大勇.催化合成水杨酸甲酯的研究与表征[J].分析仪器,2006(4):45-48. 被引量:7
8厦门大学推出新型酯化反应催化剂[J].石油炼制与化工,2008,39(8):20-20.
9涂华民,李铭岫.含水硝酸盐作为酯化反应催化剂的研究[J].河北师范学院学报:自然科学版,1991(2):74-78.
10陈其瑞,张凤美,郑爱华,焦肇林.稀土氧化物作为酯化反应催化剂的改进[J].稀土,1997,18(1):55-57. 被引量:3
Basic Information:
DOI:
Chinese Library Classification Number:O621.256.4[理学—有机化学];O643.36[理学—物理化学]
Citation Information:
Ln2O3/X-13 sieve sorption (Ln= Nd,Sm,Tm,Lu, Dy ),prepared by immersioncalcination method,with 0.83% ~0. 93% RE oxides, has been proved to be quite effective as catalyst for esterification of aromatic phthalic acid or aliphatic acid with primary 2-ethylhexyl alcohol. For example. the conversion percentage of catalyst-bearing DOP is ~10% and 8% higher than that of catalyst-free DOP and X-13. And the conversion percentage of catalystbearing lOP is ~7% and ~4 % higher respectively than that of catalyst-free lOP and X-13. Furthermore, Ln2O3/X-13 sieve sorption contains ~25% less rare earth than Ln2O3/Al2O3 type esterification catalyst and esterification temperature is ~ 10℃ lower. It can be seen from the above that Ln2O3/X-13 sieve sorption is a very good esterification catalyst.
quote
| GB/T 7714-2015 | [1] CHEN Qi-rui, SHAO Ming-xia. Study of Ln_2O_3/X-13 Sieve as Catalyst for Esterification[J]. Rare Metals and Cemented Carbides, 1997(4): 11-14. |
| MLA | [1] CHEN Qi-rui, and SHAO Ming-xia. "Study of Ln_2O_3/X-13 Sieve as Catalyst for Esterification." Rare Metals and Cemented Carbides, no. 4, 1997, pp. 11-14. |
| APA | [1] CHEN Qi-rui, & SHAO Ming-xia. (1997). Study of Ln_2O_3/X-13 Sieve as Catalyst for Esterification. Rare Metals and Cemented Carbides(4), 11-14. |
| IEEE | [1] CHEN Qi-rui and SHAO Ming-xia, "Study of Ln_2O_3/X-13 Sieve as Catalyst for Esterification," Rare Metals and Cemented Carbides, no. 4, pp. 11-14, 1997. keywords: {RE oxide, supporting catalyst, catalytic esterification, X-13 molecular sieve} |