Synthesis of 2-ethylhexoic Acid Rare Earth and its Application in Coating AITranslate
Abstract AITranslate
High-Content rare earth of 2-ethylhexoic acid has been synthesized by complex extraction method. The optimum synthetic conditions: the saponification rate of 2ethylhexoic acid is about 80%;the mole ratio of 2-ethylhexoic acid to rare earth is 3. 4: ;the reaction lasts 30 mins at 80℃. Its application in alchoholic acid paint proved its properties are up to or superior to the traditional drier standard.
KeyWords AITranslate
1成本诚,李祖光.稀土有机化学品的应用及其发展趋势[J].稀有金属与硬质合金,1995,23(2):42-46. 被引量:2
2倪文康,陈雨平.合成脂肪酸稀土催干剂在醇酸清漆中的应用[J].涂料工业,1991(3):16-18. 被引量:3
3李会宁,刘梅玲,刘国杰.涂料用稀土催干剂系列研究(Ⅰ)——代钴稀土催干剂合成过程中络合萃取的研究[J].涂料工业,1991(1):7-10. 被引量:7
4翟应离,谭民裕,李斯加,张连启,刘国杰,张筱兰,李大鸣.涂料催干剂羧酸稀土络合物的合成[J]涂料工业,1983(06).
1詹志洪.稀土在塑料和涂料制品中的应用与展望[J].稀土,2004,25(6):80-83. 被引量:3
2张玉玺,唐黎明,曹鸿璋.稀土在涂料工业中的应用[J].涂料工业,2009,39(3):61-63. 被引量:8
3吴茂英,刘正堂,崔英德.稀土高分子材料助剂开发研究进展[J].稀土,2004,25(1):63-67. 被引量:10
1刘新海,赵莹,王笃金,刘智,孙贤育,吴瑾光,徐端夫.聚氨酯与乙酰丙酮铽复合物的相互作用[J].高等学校化学学报,2006,27(10):1974-1977. 被引量:4
2吴茂英.硬脂酸稀土和硬脂酸钙对PVC热稳定特性的比较研究[J].聚氯乙烯,2007,35(10):30-33. 被引量:16
3邱凤仙,史成亮,陈丽琴,杨冬亚.稀土钕/聚氨酯光致发光材料的合成与性能研究[J].化工新型材料,2008,36(3):34-35. 被引量:2
4任艳军,关长斌.改性三氧化二钇填充橡胶应力松弛行为研究[J].世界橡胶工业,2008,35(12):22-25.
5张玉玺,唐黎明,曹鸿璋.稀土在涂料工业中的应用[J].涂料工业,2009,39(3):61-63. 被引量:8
6汪怀远,冯新,史以俊,陆小华.Effects of Treated Nano-Lanthanum Oxide on the Mechanical and Tribological Properties of PTFE Nanocomposites[J].稀土学报:英文版,2007,0(S2):40-44.
7戴越,陈逸珺,张孟群.微波消解-电感耦合等离子体原子发射光谱法测定催干剂中金属元素含量[J].理化检验:化学分册,2010,46(4):371-373. 被引量:4
8杨华.稀土元素的配位化合物及应用概述[J].稀土,2010,31(3):87-92. 被引量:9
9张技术.针织T恤衫二次设计中稀土夜光材料的应用[J].针织工业,2010(10):51-53. 被引量:1
10杨永清,齐暑华,吴江涛.稀土在高分子材料中的应用[J].中国塑料,2011,25(6):87-91. 被引量:7
1夏清平.新型异辛酸稀土催干剂[J].上海化工,1992,17(4):19-21. 被引量:1
2贺晓慧,邹建国,孙,吴琴芬,刘燕燕,付平汉,汪楠.稀土催干剂的制备及应用研究[J].江西化工,1995,11(4):3-6. 被引量:7
3张征林,王惠荣.环烷酸异辛酸稀土的合成和应用[J].江苏化工,1992,20(2):7-9. 被引量:2
4周继鑫.环境友好型催干剂异辛酸锆的合成工艺[J].现代涂料与涂装,2005,8(2):30-31. 被引量:1
5张素英.稀土催干剂及其应用[J].辽宁化工,1991(2):25-27. 被引量:4
6任致伟.稀土催干剂合成和应用[J].云南化工,1999(2):41-42. 被引量:1
7郭延秀.浅谈稀土催干剂在油漆中的应用[J].西宁科技,1991(2):9-11.
8刘国杰.稀土催干剂的特性及发展前景[J].中国涂料,1992(3):31-34. 被引量:1
9孙日圣,贺晓慧,邹建国,吴琴芬,刘燕燕.异辛酸稀土合成工艺条件的研究[J].精细化工,1996,13(3):35-37. 被引量:7
10韩利,石玉香.新型高效催干剂异辛酸锆的研制[J].涂料技术与文摘,2002,23(1):76-79. 被引量:2
Basic Information:
DOI:
Chinese Library Classification Number:TQ630.492[化学工程—精细化工]
Citation Information:
High-Content rare earth of 2-ethylhexoic acid has been synthesized by complex extraction method. The optimum synthetic conditions: the saponification rate of 2ethylhexoic acid is about 80%;the mole ratio of 2-ethylhexoic acid to rare earth is 3. 4: ;the reaction lasts 30 mins at 80℃. Its application in alchoholic acid paint proved its properties are up to or superior to the traditional drier standard.
quote
| GB/T 7714-2015 | [1] CHENG Ben-cheng, XIE Wen-lin. Synthesis of 2-ethylhexoic Acid Rare Earth and its Application in Coating[J]. Rare Metals and Cemented Carbides, 1997(4): 15-18. |
| MLA | [1] CHENG Ben-cheng, and XIE Wen-lin. "Synthesis of 2-ethylhexoic Acid Rare Earth and its Application in Coating." Rare Metals and Cemented Carbides, no. 4, 1997, pp. 15-18. |
| APA | [1] CHENG Ben-cheng, & XIE Wen-lin. (1997). Synthesis of 2-ethylhexoic Acid Rare Earth and its Application in Coating. Rare Metals and Cemented Carbides(4), 15-18. |
| IEEE | [1] CHENG Ben-cheng and XIE Wen-lin, "Synthesis of 2-ethylhexoic Acid Rare Earth and its Application in Coating," Rare Metals and Cemented Carbides, no. 4, pp. 15-18, 1997. keywords: {2-ethylhexoic acid, rare earth, coating, rare earth drier} |