Study on Phase Transformation During the Reduction of Molybdenum AITranslate
Abstract AITranslate
Molybdenum powders have been made by directly reducing of ammonium molybdate and three-step reduction of ammonium molybdate. The rules of phase transformation taking place during reduction have been investigated by X-ray diffraction analysis and the effects of unstable phase of Mo4O11 on the reduction of molybdenum have also been discussed.
KeyWords AITranslate
1刘仁智,李晶,安耿,付静波,卜春阳.层片状二氧化钼还原过程模型化研究[J].中国钼业,2009,33(3):37-40. 被引量:4
2刘国玺,顾明俊,韩剑锋,常永威,燕东明,高晓菊,乔光利.钼粉的研究进展及应用[J].材料导报:纳米与新材料专辑,2011,25(2):143-147. 被引量:7
3刘秋萍.MoO_3-MoO_2氢还原过程中的速率控制[J].中国钨业,2012,27(5):25-28. 被引量:4
4陈艳芳,谢敬佩,苌清华,马窦琴.钼粉制备技术的研究进展[J].材料热处理学报,2020,41(7):14-24. 被引量:3
5张瑞华,郝振华,车玉思,舒永春,孙院军,何季麟.钼粉的制备方法及研究进展[J].稀有金属,2022,46(4):510-522.
6王新刚,唐利侠.高纯三氧化钼激光粒度分布的测定与分析[J].中国钼业,2003,27(2):67-70. 被引量:3
7李晶,左羽飞.钼粉还原过程的形貌演变[J].稀有金属,2007,31(S1):73-76. 被引量:5
8秦文峰,彭金辉,樊希安,向守义,杨晓青,袁茂强.微波煅烧钼酸铵制取高纯三氧化钼新工艺[J].新技术新工艺,2004(4):42-44. 被引量:10
9刘伟,周美玲,王金淑,陈以欣,李娜.溶胶-凝胶法制备稀土钼超细粉末[J].中国有色金属学报,2004,14(5):820-824. 被引量:4
1闫洪.2004年云南金属材料与加工年评[J].云南冶金,2005,34(2):40-49.
2杨晓青,秦文峰,罗振中,贺跃辉.微波加热技术在钼工业中的应用[J].中国钼业,2005,29(2):43-46. 被引量:12
3谢复青,张志.微波技术在无机化学中的应用进展[J].广西梧州师范高等专科学校学报,2005,21(2):92-94. 被引量:3
4周雪梅.北师大出版社隆重推出《当代中国心理学家文库》[J].大学出版,2006(2):46-46.
5杨晓青,罗振中,郭荣辉,关鑫.稀土掺杂钼制品研究进展[J].中国钼业,2006,30(4):33-35. 被引量:12
6张文朴.微波加热技术在冶金工业中的应用研发进展[J].中国钼业,2007,31(6):20-23. 被引量:7
7张文朴.微波在稀贵金属冶金中的应用研究进展[J].稀有金属与硬质合金,2008,36(2):49-53. 被引量:11
8冯兆滨,刘秀梅,刘光荣,邹绍文,张树清,张建峰,王玉军,张夫道.两种改性磷矿粉的制备与表征[J].植物营养与肥料学报,2008,14(4):792-796. 被引量:8
9罗会龙,彭金辉,张利波,郭胜惠,刘秉国.高温微波反应器工业化应用部分关键问题分析[J].现代化工,2009(5):76-79. 被引量:2
10刘拼拼,范景莲,成会朝,李勇明,田家敏.稀土La对钼合金组织和性能的影响[J].粉末冶金技术,2009,27(3):185-188. 被引量:21
1李军,刘心宇,成锐.钼还原过程研究[J].中南工业大学学报,1997,28(4):370-372. 被引量:3
2秦玉楠.离子交换法自含铜钼精矿生产纯MoO_3新工艺[J].中国钼业,1996,20(1):47-50.
3绪小鹏.优质钼酸铵是钼条生产的质量保证[J].中国钼业,1997,21(2):107-108. 被引量:8
4陈庭章,周勤俭,银瑰.从萃取钼余液中回收铜[J].中国钼业,1997,21(2):80-82. 被引量:4
5顾珩,李洪桂,刘茂盛.热球磨苏打法处理钼渣新工艺研究[J].中国钼业,1997,21(4):16-18. 被引量:5
6程立,黎嫚.高压溶出贵州铝土矿时硅钛矿物的相变化[J].轻金属,1991(6):18-22. 被引量:8
7桂明玺.氮化硅铁在高炉出铁口用炮泥料中的性状[J].国外耐火材料,1998,23(12):41-44. 被引量:12
8王献科,王德勇.利用中频感应电炉生产硅铝铁合金[J].中国钼业,1999,23(2):11-13.
9董桑林.美国钼工业的现状与发展[J].稀有金属,1993,17(6):455-459. 被引量:1
10Sebe.,RF,陈安庆.流化床还原器内保持流态化的方法[J].钨钼材料,1995(4):9-13.
Basic Information:
DOI:
Chinese Library Classification Number:TF841.2[冶金工程—有色金属冶金]
Citation Information:
Molybdenum powders have been made by directly reducing of ammonium molybdate and three-step reduction of ammonium molybdate. The rules of phase transformation taking place during reduction have been investigated by X-ray diffraction analysis and the effects of unstable phase of Mo4O11 on the reduction of molybdenum have also been discussed.
quote
| GB/T 7714-2015 | [1] WEI Yong, LIU Xin-yu, LI Yi-fu, et al. Study on Phase Transformation During the Reduction of Molybdenum[J]. Rare Metals and Cemented Carbides, 1996(3): 13-18. |
| MLA | [1] WEI Yong, et al., "Study on Phase Transformation During the Reduction of Molybdenum." Rare Metals and Cemented Carbides, no. 3, 1996, pp. 13-18. |
| APA | [1] WEI Yong, LIU Xin-yu, LI Yi-fu, & SU Xiao. (1996). Study on Phase Transformation During the Reduction of Molybdenum. Rare Metals and Cemented Carbides(3), 13-18. |
| IEEE | [1] WEI Yong, LIU Xin-yu, LI Yi-fu, and SU Xiao, "Study on Phase Transformation During the Reduction of Molybdenum," Rare Metals and Cemented Carbides, no. 3, pp. 13-18, 1996. keywords: {molybdenum;powder;reduction;phase composition} |