Analysis of The Formation of The SHSTiC Crystalline Structure AITranslate
Abstract AITranslate
This paper briefly introduces the common feature of the SHS process and the SHS's materials; reveals the effects of initial temperature, fast cooling, additives and other factors on microstructure of SHSTiC: analyzes the SHSTiC crystal with discussion about mechanisms of the synthesis and the structure formation.
KeyWords AITranslate
1李劲风,张昭,张鉴清.Ti-W-C体系燃烧合成产物颗粒形貌分析[J].粉末冶金技术,2002,20(2):71-74.
2李奎,潘复生,汤爱涛.TiC、TiN、Ti(C、N)粉末制备技术的现状及发展[J].重庆大学学报:自然科学版,2002,25(6):135-138. 被引量:28
3白鑫涛,王锦霞,谢宏伟,崔富辉,翟玉春.非传统TiC合成研究进展[J].有色金属科学与工程,2015,6(1):59-65. 被引量:2
1汤波.TiC基金属陶瓷的性能与发展[J].湖南冶金,2004,32(5):7-10. 被引量:8
2李素平,孙洪巍,钟香崇.铝热还原氮化法制备TiN-Al_2O_3复合粉体[J].金刚石与磨料磨具工程,2004,24(6):40-42.
3杨锦,李芳,刘颖,涂铭旌.Ti(C,N)粉末制备技术的研究及进展[J].硬质合金,2005,22(1):51-54. 被引量:6
4周永贵,郑江.Ti(C,N)基金属陶瓷制备工艺研究[J].硬质合金,2005,22(3):156-160. 被引量:1
5马玉平,向道辉,陈明,孙方宏.微小孔加工试验及刀具磨损机理[J].南京航空航天大学学报,2005,37(B11):8-11. 被引量:3
6马玉平,李铸宇,钟敬文,陈明.钛合金微小孔钻削试验研究[J].机械工程材料,2005,29(11):11-13. 被引量:1
7吴锋,李志坚,陈俊红,亓华涛.碳热还原氮化合成TiN的研究[J].耐火材料,2006,40(2):89-91. 被引量:10
8卢红宪,胡水,蒋明学.Al_2O_3基金属陶瓷的研究现状及发展趋势[J].陶瓷,2006(6):5-8.
9甘明亮,李亚伟,聂建华,金胜利,李远兵,杨大兵,高运明.反应气氛对铝热还原氧化钛合成氮化钛的影响[J].武汉科技大学学报,2007,30(1):33-36. 被引量:2
10聂建华,李亚伟,甘明亮,李远兵,颜浩.还原气氛下铝热还原法合成TiN-Al_2O_3复合材料[J].耐火材料,2007,41(4):241-244.
1严有为,魏伯康,林汉同,蔡启舟.SHS基础研究的现状及展望[J].汽车工艺与材料,1996(12):5-9. 被引量:4
2刘纪德,李伟,孙伟成.重力分离SHS过程的预测[J].沈阳工业学院学报,2003,22(3):72-74.
3金华军,唐立平.Ti-C-3Ni-Al体系SHS反应热力学分析[J].钛工业进展,2009,26(3):38-40.
4张荣法(发).“宜兴窑艺”青瓷的表征与研制[J].江苏陶瓷,2016,49(4):17-20.
5张艳丽,徐世帅,刘红燕,梁宝岩.铝对3Ti/SiC/C体系自蔓延高温合成Ti_3SiC_2的影响[J].中国陶瓷,2015,51(6):26-29. 被引量:2
6曾晓春,孙国雄,张树格.自蔓延高温合成法制备Al_2O_3-Cr金属陶瓷[J].硅酸盐学报,1999,27(1):98-102. 被引量:2
7豆志河,张廷安,刘燕,郭永楠,赫冀成.Preparation of CeB_6 nano-powders by self-propagating high-temperature synthesis(SHS)[J].稀土学报:英文版,2011,29(10):986-990. 被引量:1
8周玉梅,张凤林,王成勇.金刚石对Ni-Al自蔓延反应过程的影响[J].金刚石与磨料磨具工程,2010,30(2):44-48. 被引量:4
9梁宝岩,王艳芝,张旺玺,徐世帅.金刚石颗粒表面形成氧化铝晶须的研究[J].中国陶瓷,2015,51(12):31-34. 被引量:1
10张化宇,韩杰才,赫晓东,杜善义,张宇民.自蔓延高温合成MgO-B_4C微观组织研究[J].宇航材料工艺,2000,30(2):25-28. 被引量:6
Basic Information:
DOI:
Chinese Library Classification Number:TQ127.12[化学工程—无机化工];TQ134.11[化学工程—无机化工]
Citation Information:
This paper briefly introduces the common feature of the SHS process and the SHS's materials; reveals the effects of initial temperature, fast cooling, additives and other factors on microstructure of SHSTiC: analyzes the SHSTiC crystal with discussion about mechanisms of the synthesis and the structure formation.
quote
| GB/T 7714-2015 | [1] XIA Bin-hua, LV Hai-bo, LUO Xu-ming, et al. Analysis of The Formation of The SHSTiC Crystalline Structure[J]. Rare Metals and Cemented Carbides, 1996(3): 6-12. |
| MLA | [1] XIA Bin-hua, et al., "Analysis of The Formation of The SHSTiC Crystalline Structure." Rare Metals and Cemented Carbides, no. 3, 1996, pp. 6-12. |
| APA | [1] XIA Bin-hua, LV Hai-bo, LUO Xu-ming, & JIANG Ci-jin. (1996). Analysis of The Formation of The SHSTiC Crystalline Structure. Rare Metals and Cemented Carbides(3), 6-12. |
| IEEE | [1] XIA Bin-hua, LV Hai-bo, LUO Xu-ming, and JIANG Ci-jin, "Analysis of The Formation of The SHSTiC Crystalline Structure," Rare Metals and Cemented Carbides, no. 3, pp. 6-12, 1996. keywords: {SHSTiC;crystal;crystalline structure;grain size} |