School of Metallurgy Engineering, Xi'an University of Architecture and Technology;School of Metallurgy Engineering, Xi'an University of Architecture and Technology;School of Metallurgy Engineering, Xi'an University of Architecture and Technology;School of Metallurgy Engineering, Xi'an University of Architecture and Technology;School of Metallurgy Engineering, Xi'an University of Architecture and Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Molten salt electrolysis was done on V-Ti-Fe alloy prepared by metallothermic reduction,and deoxidation process of the alloy was studied.The influence of electrolysis time on deoxidation degree was investigated.The results show that most of oxygen in V-Ti-Fe alloy can be removed by molten salt electrolysis.With the increase of electrolysis time,oxygen content in the alloy gradually decreases to about 0.2%after 240 min electrolysis.Hydrogen absorption and desorption performances of V-Ti-Fe alloy are improved by electro-deoxidation in molten salt.With the increase of electrolysis time,both the maximum hydrogen absorption capacity and the effective hydrogen desorption capacity increase as high as 2.65% and 1.01%,respectively.

KeyWords AITranslate

V-Ti-Fe hydrogen storage alloy deoxidation molten salt electrolysis hydrogen storage capacity

1Sydney F. Santos,Jacques Huot.Hydrogen storage in TiCr 1.2 (FeV) x BCC solid solutions[J]. Journal of Alloys and Compounds . 2008 (1)

2Yigang Yan,Yungui Chen,Hao Liang,Chaoling Wu,Mingda Tao,Tu Mingjing.Effect of Al on hydrogen storage properties of V 30 Ti 35 Cr 25 Fe 10 alloy[J]. Journal of Alloys and Compounds . 2006 (1)

3M.V. Lototsky,V.A. Yartys,I.Yu. Zavaliy.Vanadium-based BCC alloys: phase-structural characteristics and hydrogen sorption properties[J]. Journal of Alloys and Compounds . 2005

4M. Okada,T. Kuriiwa,T. Tamura,H. Takamura,A. Kamegawa.Ti–V–Cr b.c.c. alloys with high protium content[J]. Journal of Alloys and Compounds . 2002

5H Itoh,H Arashima,K Kubo,T Kabutomori.The influence of microstructure on hydrogen absorption properties of Ti–Cr–V alloys[J]. Journal of Alloys and Compounds . 2002

6M Tsukahara,K Takahashi,A Isomura,T Sakai.Influence of oxygen on hydrogen storage and electrode properties for micro-designed V-based battery alloys[J]. Journal of Alloys and Compounds . 1998 (1)

7Kei Nomura,Etsuo Akiba.H 2 Absorbing-desorbing characterization of the TiVFe alloy system[J]. Journal of Alloys and Compounds . 1995 (1)

1尚德礼,吕春风,康磊.钛脱氧钢中夹杂物的形成规律及其对组织的影响[J].钢铁钒钛,2013,34(6):60-64. 被引量:1

2谢大海,王兴庆,陈发允.熔盐电脱氧制备金属铌的研究[J].上海金属,2011,33(2):23-27.

3胡小锋,许茜,李海滨,马青梅,任东琦.熔盐电脱氧法制备金属Ti的最新研究进展[J].材料导报,2006,20(8):101-103. 被引量:10

4周保仓.利用新开发的分析方法研究热处理过程中马氏体不锈钢夹杂物成分的改变[J].不锈,2014,0(4):14-22.

5王斌,刘奎仁,陈建设,高腾跃,何季麟.金属热还原法制备V-Ti-Fe中间合金(英文)[J].中国有色金属学报:英文版,2012,22(6):1507-1512. 被引量:5

6李晴宇,杜继红,奚正平.金属锆的熔盐电脱氧制备[J].稀有金属材料与工程,2007,36(A03):390-393. 被引量:14

7王斌,杜金晶,刘奎仁,朱军,李林波.V-Ti-Fe储氢合金的真空精炼[J].有色金属:冶炼部分,2015(6):67-71. 被引量:1

8邹祥宇,廖先杰,卫学玲,夏鹏举,徐峰,罗清威.Al_3Sc的FFC法制备和第一性原理计算研究[J].材料与冶金学报,2014,13(4):284-287. 被引量:1

9徐越兰,王克鸿,王建平,李鸿谋.稀土钇及硼在3.5%镍电焊条中的行为[J].焊接学报,1997,18(3):141-145.

10朱靖,曹吉林,王明涌,王岭,戴磊.熔盐电脱氧法制备ZrCr_2储氢合金的研究[J].人工晶体学报,2016,45(3):834-839. 被引量:1

Basic Information:

DOI:

Chinese Library Classification Number:TG139.7[一般工业技术—材料科学与工程]

Citation Information:

Molten salt electrolysis was done on V-Ti-Fe alloy prepared by metallothermic reduction,and deoxidation process of the alloy was studied.The influence of electrolysis time on deoxidation degree was investigated.The results show that most of oxygen in V-Ti-Fe alloy can be removed by molten salt electrolysis.With the increase of electrolysis time,oxygen content in the alloy gradually decreases to about 0.2%after 240 min electrolysis.Hydrogen absorption and desorption performances of V-Ti-Fe alloy are improved by electro-deoxidation in molten salt.With the increase of electrolysis time,both the maximum hydrogen absorption capacity and the effective hydrogen desorption capacity increase as high as 2.65% and 1.01%,respectively.

quote

GB/T 7714-2015 [1] WANG Bin, LIU Kui-ren, DU Jin-jing, et al. Research on Deoxidation of V-Ti-Fe Hydrogen Storage Alloy by Molten Salt Electrolysis[J]. Rare Metals and Cemented Carbides, 2015(5): 34-38.
MLA [1] WANG Bin, et al., "Research on Deoxidation of V-Ti-Fe Hydrogen Storage Alloy by Molten Salt Electrolysis." Rare Metals and Cemented Carbides, no. 5, 2015, pp. 34-38.
APA [1] WANG Bin, LIU Kui-ren, DU Jin-jing, ZHU Jun, & LI Lin-bo. (2015). Research on Deoxidation of V-Ti-Fe Hydrogen Storage Alloy by Molten Salt Electrolysis. Rare Metals and Cemented Carbides(5), 34-38.
IEEE [1] WANG Bin, LIU Kui-ren, DU Jin-jing, ZHU Jun, and LI Lin-bo, "Research on Deoxidation of V-Ti-Fe Hydrogen Storage Alloy by Molten Salt Electrolysis," Rare Metals and Cemented Carbides, no. 5, pp. 34-38, 2015. keywords: {V-Ti-Fe hydrogen storage alloy;deoxidation;molten salt electrolysis;hydrogen storage capacity}