For the first time, the pinning effect of small spheroid particles with aspect ratios 1, 2 and 3 on grain growth in polycrystalline structures was studied by three-dimensional phase-field simulations. This was possible by using an efficient parallel sparse bounding box algorithm. Simulation results for different volume fractions of the second-phase particles show that distributions of particles with higher aspect ratios have a stronger pinning effect, since grain boundaries have the tendency to align with the largest cross-section of the particles. The number of particles at triple, quadruple or higher order junctions increases with volume fraction, and with aspect ratio. Nevertheless, the final grain size has a volume fraction dependence of the form 1 / f V 0.93 , following theoretical predictions assuming random intersections between grain boundaries and particles. A generalised Zener relation with a prefactor depending on the aspect ratio is proposed.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1016/j.commatsci.2010.05.020
Chinese Library Classification Number:
Citation Information:
For the first time, the pinning effect of small spheroid particles with aspect ratios 1, 2 and 3 on grain growth in polycrystalline structures was studied by three-dimensional phase-field simulations. This was possible by using an efficient parallel sparse bounding box algorithm. Simulation results for different volume fractions of the second-phase particles show that distributions of particles with higher aspect ratios have a stronger pinning effect, since grain boundaries have the tendency to align with the largest cross-section of the particles. The number of particles at triple, quadruple or higher order junctions increases with volume fraction, and with aspect ratio. Nevertheless, the final grain size has a volume fraction dependence of the form 1 / f V 0.93 , following theoretical predictions assuming random intersections between grain boundaries and particles. A generalised Zener relation with a prefactor depending on the aspect ratio is proposed.
quote
| GB/T 7714-2015 | [1] Liesbeth Vanherpe, Nele Moelans, Bart Blanpain, et al. Computational Materials Science, 2010(49). DOI:10.1016/j.commatsci.2010.05.020. |
| MLA | [1] Liesbeth Vanherpe, et al., Computational Materials Science, no. 49, 2010, https://doi.org/10.1016/j.commatsci.2010.05.020. |
| APA | [1] Liesbeth Vanherpe, Nele Moelans, Bart Blanpain, & Stefan Vandewalle. (2010). Computational Materials Science(49). https://doi.org/10.1016/j.commatsci.2010.05.020 |
| IEEE | [1] Liesbeth Vanherpe, Nele Moelans, Bart Blanpain, and Stefan Vandewalle, Computational Materials Science, no. 49, 2010, doi: 10.1016/j.commatsci.2010.05.020. |