daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Highly Uniform Activation of Carbon Fiber Reinforced Thermoplastics by Low-Temperature Plasma AITranslate

Washington University; Washington University;The Boeing Company, Saint Louis;The Boeing Company;The Boeing Company, Saint Louis; Washington University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Nonequilibrium plasma treatments of carbon fiber reinforced thermoplastic (CFRTP) composites can activate the robust, chemically inert material into a nonequilibrium state that can be used to fabricate bonded structural assemblies with high toughness. The nonequilibrium surface is unstable; thus, the development of nondestructive characterization techniques is of paramount importance to assess the material before use. Herein, a discovery is reported that plasma-activated CFRTP surfaces are characterized by a sharp, well-defined surface potential distribution, the width of which is correlated to the fracture toughness of bonded assemblies. The activated surface has a maximum lifetime on the order of days to weeks and is hypothesized to be composed of metastable radical-ion complexes. The hypothesis is consistent with several independent pieces of evidence, including Kelvin probe force microscopy, contact angle measurements, magnetic force microscopy, and radical probe experiments.

KeyWords AITranslate

plasma treatment carbon fiber polymermatrix composites (PMCs) surface modification oxygen plasma activation scanning probe microscopy
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.9b00532

Chinese Library Classification Number:

Citation Information:

Nonequilibrium plasma treatments of carbon fiber reinforced thermoplastic (CFRTP) composites can activate the robust, chemically inert material into a nonequilibrium state that can be used to fabricate bonded structural assemblies with high toughness. The nonequilibrium surface is unstable; thus, the development of nondestructive characterization techniques is of paramount importance to assess the material before use. Herein, a discovery is reported that plasma-activated CFRTP surfaces are characterized by a sharp, well-defined surface potential distribution, the width of which is correlated to the fracture toughness of bonded assemblies. The activated surface has a maximum lifetime on the order of days to weeks and is hypothesized to be composed of metastable radical-ion complexes. The hypothesis is consistent with several independent pieces of evidence, including Kelvin probe force microscopy, contact angle measurements, magnetic force microscopy, and radical probe experiments.

quote

GB/T 7714-2015 [1] Trey Oldham, Kirby Simon, Daniel R. Ferriell, et al. ACS Applied Polymer Materials, 2019(1). DOI:10.1021/acsapm.9b00532.
MLA [1] Trey Oldham, et al., ACS Applied Polymer Materials, no. 1, 2019, https://doi.org/10.1021/acsapm.9b00532.
APA [1] Trey Oldham, Kirby Simon, Daniel R. Ferriell, Marcus A. Belcher, Alexander Rubin, & Elijah Thimsen. (2019). ACS Applied Polymer Materials(1). https://doi.org/10.1021/acsapm.9b00532
IEEE [1] Trey Oldham, Kirby Simon, Daniel R. Ferriell, Marcus A. Belcher, Alexander Rubin, and Elijah Thimsen, ACS Applied Polymer Materials, no. 1, 2019, doi: 10.1021/acsapm.9b00532. keywords: {plasma treatment;carbon fiber;polymermatrix composites (PMCs);surface modification;oxygen plasma activation;scanning probe microscopy}