Ionic-Liquid-Based Electroactive Polymer Composites for Muscle Tissue Engineering AITranslate
Abstract AITranslate
As an electromechanically active tissue, muscle regeneration takes advantage of active scaffolds providing mechanoelectrical stimuli and a biomimetic microenvironment. Thus, this study reports on the preparation of ionic electroactive materials based on ionic liquids (ILs) and poly(vinylidene fluoride) (PVDF). IL/PVDF composites with 10, 20, and 40% wt. of 1-butyl-3-methylimidazolium chloride [Bmim][Cl] and 2-hydroxyethyl-trimethylammonium dihydrogen phosphate [Ch][DHP] were prepared by solvent casting. It is shown that the inclusion of [Bmim][Cl] and [Ch][DHP] both improves the electrical conductivity and induces the PVDF crystallization in the polar β-phase. Further, the introduction of the IL also influences the thermal stability of the composites. [Bmim][Cl]/PVDF composites show larger Young moduli and a larger increase of the electrical conductivity than the [Ch][DHP]/PVDF composites. It is also shown that [Bmim][Cl] composites show a piezoresistive response, with gauge factors from 1 to 2.5, allowing them therefore to work as electromechanical sensors in biomechanical applications. The noncytotoxicity of the IL/PVDF composite films and C2C12 cell proliferation demonstrates the applicability of the composites as a suitable platform for muscle regeneration strategies.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.9b00566
Chinese Library Classification Number:
Citation Information:
As an electromechanically active tissue, muscle regeneration takes advantage of active scaffolds providing mechanoelectrical stimuli and a biomimetic microenvironment. Thus, this study reports on the preparation of ionic electroactive materials based on ionic liquids (ILs) and poly(vinylidene fluoride) (PVDF). IL/PVDF composites with 10, 20, and 40% wt. of 1-butyl-3-methylimidazolium chloride [Bmim][Cl] and 2-hydroxyethyl-trimethylammonium dihydrogen phosphate [Ch][DHP] were prepared by solvent casting. It is shown that the inclusion of [Bmim][Cl] and [Ch][DHP] both improves the electrical conductivity and induces the PVDF crystallization in the polar β-phase. Further, the introduction of the IL also influences the thermal stability of the composites. [Bmim][Cl]/PVDF composites show larger Young moduli and a larger increase of the electrical conductivity than the [Ch][DHP]/PVDF composites. It is also shown that [Bmim][Cl] composites show a piezoresistive response, with gauge factors from 1 to 2.5, allowing them therefore to work as electromechanical sensors in biomechanical applications. The noncytotoxicity of the IL/PVDF composite films and C2C12 cell proliferation demonstrates the applicability of the composites as a suitable platform for muscle regeneration strategies.
quote
| GB/T 7714-2015 | [1] R. M. Meira, D. M. Correia, S. Ribeiro, et al. ACS Applied Polymer Materials, 2019(1). DOI:10.1021/acsapm.9b00566. |
| MLA | [1] R. M. Meira, et al., ACS Applied Polymer Materials, no. 1, 2019, https://doi.org/10.1021/acsapm.9b00566. |
| APA | [1] R. M. Meira, D. M. Correia, S. Ribeiro, P. Costa, A. C. Gomes, F. M. Gama, S. LancerosMéndez, & C. Ribeiro. (2019). ACS Applied Polymer Materials(1). https://doi.org/10.1021/acsapm.9b00566 |
| IEEE | [1] R. M. Meira, D. M. Correia, S. Ribeiro, P. Costa, A. C. Gomes, F. M. Gama, S. LancerosMéndez, and C. Ribeiro, ACS Applied Polymer Materials, no. 1, 2019, doi: 10.1021/acsapm.9b00566. keywords: {electroactive;ionic liquid;PVDF;smart materials;tissue engineering} |