daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

The Latest Development of Preparation Technologies of YAG:Ce3+ Phosphor AITranslate

School of Chemistry, Central South University;School of Chemistry, Central South University;School of Chemistry, Central South University;School of Chemistry, Central South University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The latest development of different preparation technologies of YAG∶Ce3+ yellow phosphor used in white LED is summarized.These technologies include solid reaction method,sol-gel method,spray method,flash combustion method,coprecipitation method,coprecipitation-molten salt method and so on.Their advantages and disadvantages are compared,and their development trends are also pointed out.

KeyWords AITranslate

YAG∶Ce3+ phosphor white LED preparation technology the latest development

1李东平,缪春燕,刘丽芳,夏威.白光LED用YAG∶Ce^(3+)荧光粉的研究进展[J].液晶与显示,2005,20(6):526-531. 被引量:30

2吴作贵,张旭东,何文,任晓辉.白光LED用YAG:Ce^(3+)荧光粉制备技术的研究进展[J].山东陶瓷,2007,30(1):28-30. 被引量:12

3Xiong Zhaoxian Song Chunxiao Wu Wei Qiu Hong.Effect of Sintering Time on Luminescent Properties of YAG: Ce3+ Phosphors[J].稀土学报:英文版,2004(z1):137-139. 被引量:6

4Ruan Shen-kang, Zhou Jian-guo, Zhong Ai-min, et al. Synthesis of Y3 Al5 O12 : Eu3+ phosphor by sol-gel meth- od and its luminescence behavior[J]. Journal of Alloys and Compounds, 1998,275-277 : 72-75.

5Li Xia,Liu Hong,Wang Ji-yang,et al. YAG : Ce nano- sized phosphor particles prepared by a solvothermal method[J]. Materials Research Bulletin, 2004,39 ( 12 ): 1 923-1 930.

6Yuan Fang-li. Ce-doped YAG phosphor powders pre pared by co-precipitation and heterogeneous precipitation [J].Materials Science & Engineering B, 2004,107 : 14-18.

7Pham-Thi M,Morell A. Process optimization and char- acterization of the red no-mill phosphor Y2 03 S : Eu[J].Electrochem,1991,138:1 100-1 103.

8Williams D K, Bihari B, Brian M. Tissue, preparation and fluorescence spectroscopy of bulk monoelinic[J]. Phys Chem B, 1998,102 (6) : 916-920.

9Esquivias L. Advanced materials from gel[J].NonCrystalline Solide, 1992,148:597-602.

10Shea L E, McKittrick J. Predicting and modeling the low-voltage eathodolumineseent efficiency of oxide phosphors[J]. Electrochem Soc, 1998,145(9):3 165-3170.

1张辉,邸永江,晁明明,侯强.YAG:Ce^(3+)荧光粉的溶胶-凝胶法制备工艺研究进展[J].中国照明电器,2014(6):5-7.

2陈鸿,张丽,陈清松,凌启淡.一种新型黄色荧光类水滑石复合物的制备及表征[J].应用化学,2013,30(7):776-781. 被引量:2

3李兆,江元汝,徐克,赵西成,赵亚娟.不同形貌Al_2O_3粉体的制备及对YAG:Ce^(3+)光学性能的影响[J].兵器材料科学与工程,2013,36(4):6-9. 被引量:7

4李聪明,谭劲,郑水林,马米,孙夏微.含硼助熔剂对YAG∶Ce荧光粉晶相、形貌及发光性能的影响[J].人工晶体学报,2013,42(11):2235-2240. 被引量:1

5童义平,黄伟传.燃烧法制备YAG∶Ce^(3+)荧光粉的研究[J].中国陶瓷,2014,50(1):9-12. 被引量:1

6钟莲云,邵媛媛,蒯洪湘,蓝平,李眉.共沉淀法制备Nd:YAG纳米粉体的研究[J].兵器材料科学与工程,2019,0(5):98-101. 被引量:2

7蒋立朋,肖雨,李宁,李思远,张希艳.YAG:Ce^(3+)荧光粉的制备工艺及发光性能研究[J].长春理工大学学报:自然科学版,2017,40(5):82-86. 被引量:1

8肖青辉,宋碧清,杨军,李子成,游维雄,夏李斌.高Eu^(3+)浓度掺杂硼铋钙红光玻璃的制备与发光性能[J].有色金属科学与工程,2018,9(5):90-96.

1李兆,赵西成,孙强强,江元汝,赵亚娟,陈利君.蓝光转换型白光LED用YAG:Ce^(3+)荧光粉改性研究新进展[J].化工新型材料,2014,42(8):34-36. 被引量:3

2江元汝,苗波波,郭卫华,刘德尧,赵亚娟,陈利君.微波诱导燃烧法制备SrAl_2O_4:Pr^(3+)荧光粉及其发光性能研究[J].兵器材料科学与工程,2014,37(5):15-19. 被引量:2

3陈良哲,朱海娣,赵璇,周秀华,陈鸿,凌启淡.黄光类水滑石的制备、表面改性及应用[J].无机化学学报,2015,31(10):1919-1928. 被引量:2

4侯青月,李金凯,段广彬,刘宗明.白光发光二极管用荧光粉的研究进展[J].中国粉体技术,2015,21(5):44-47. 被引量:2

5李宏林,李明玲,澎湃,王耀,常靖宇,方海燕.均匀共沉淀法制备荧光水滑石的结构及性能[J].材料导报:纳米与新材料专辑,2016,30(2):269-271. 被引量:2

6李兆,吴坤尧,王永锋,曹静.Dy,Tb,Mn,Bi元素微量掺杂对Ca_(10)(Si_2O_7)_3Cl_2∶Ce^(3+)荧光粉发光性能的影响[J].化工新型材料,2017,45(3):196-198.

7周玲玲,汪蓓蓓,王磊,巩振虎.不同晶型氧化铝的YAG:Ce^(3+)荧光粉的制备、结构与性能研究[J].化学研究与应用,2017,29(4):547-550.

8蒋立朋,肖雨,李宁,李思远,张希艳.YAG:Ce^(3+)荧光粉的制备工艺及发光性能研究[J].长春理工大学学报:自然科学版,2017,40(5):82-86. 被引量:1

9侯芹芹,江元汝,甘俊羊,赵亚娟,赵彬,韩彤.溶剂热法合成La1.9Y0.06Mo2O9∶Eu3+Sm3+荧光粉及其能量传递机理[J].材料导报,2019,33(12):1939-1944. 被引量:1

10王林香,孙德方,李晴,王霞.Dy3+和Ce3+共掺Y3Al5O12荧光粉的制备及发光性质[J].发光学报,2020,41(2):160-167. 被引量:5

1冯子好,李杨,张梅,郭敏.含钛电炉熔分渣浸出废液合成莫来石晶须及热稳定性研究[J].人工晶体学报,2015,44(11):3005-3013.

2陈宏,李凯,郭亚军,王华,司宝财.Ti-Mn-Cu替代的M-型钡铁氧体的制备和表征[J].化学与粘合,2007,29(4):248-250. 被引量:1

3王立开,赵丰华,黄慧民,王媚,潘家辉,林涛.YAG:Ce^(3+)黄色荧光粉的不同合成方法及其发光性能的研究[J].化工新型材料,2013,41(11):111-114. 被引量:1

4刘建安,刘月兰.共沉淀-熔盐法制备六方磁铅石型钡铁氧体[J].电子元件与材料,2008,27(9):45-47. 被引量:3

5赵文晓,聂海宁,王志强.硼酸、Li^+掺杂对YAG:Ce^(3+)荧光粉的影响[J].大连工业大学学报,2015,34(4):275-277. 被引量:1

6李友凤,刘国清,漆斌,周虎,姜绮梦.EDTA络合溶胶-凝胶法合成YAG:Ce黄色荧光粉及其性能[J].中国有色金属学报,2014,24(4):1001-1007. 被引量:2

7李兆,赵西成,江元汝,徐克,赵亚娟.白光LED用片状α-A1_2O_3粉体的控制合成及应用研究[J].功能材料,2013,44(18):2663-2667. 被引量:12

8刘天用,雷小敏,徐玲,王晓,罗伟,王轶哲,赵战勇,焦桓.有机酸后处理对YAG:Ce^(3+)荧光粉发光特性的影响[J].中国稀土学报,2014,32(2):156-163. 被引量:2

9黄燕,赵勤,阎建辉,张建策,龚升高.熔盐法对黄粉YAG:Ce^(3+)表面改性的探讨[J].应用化工,2011,40(3):425-427. 被引量:1

10刘全生,郝新焱,许国锋,赵丽,曹丹丹,王瑞,张希艳,孙海鹰.Sr3SiO5∶Eu^2+荧光粉的微波合成及性能研究[J].无机化学学报,2010(7):1303-1306. 被引量:2

Basic Information:

DOI:

Chinese Library Classification Number:TQ133.3[化学工程—无机化工]

Citation Information:

The latest development of different preparation technologies of YAG∶Ce3+ yellow phosphor used in white LED is summarized.These technologies include solid reaction method,sol-gel method,spray method,flash combustion method,coprecipitation method,coprecipitation-molten salt method and so on.Their advantages and disadvantages are compared,and their development trends are also pointed out.

quote

GB/T 7714-2015 [1] HAN Kai, YE Hong-qi, XIE Ying, et al. The Latest Development of Preparation Technologies of YAG:Ce3+ Phosphor[J]. Rare Metals and Cemented Carbides, 2011(1): 30-35.
MLA [1] HAN Kai, et al., "The Latest Development of Preparation Technologies of YAG:Ce3+ Phosphor." Rare Metals and Cemented Carbides, no. 1, 2011, pp. 30-35.
APA [1] HAN Kai, YE Hong-qi, XIE Ying, & LI You-feng. (2011). The Latest Development of Preparation Technologies of YAG:Ce3+ Phosphor. Rare Metals and Cemented Carbides(1), 30-35.
IEEE [1] HAN Kai, YE Hong-qi, XIE Ying, and LI You-feng, "The Latest Development of Preparation Technologies of YAG:Ce3+ Phosphor," Rare Metals and Cemented Carbides, no. 1, pp. 30-35, 2011. keywords: {YAG∶Ce3+;phosphor;white LED;preparation technology;the latest development}