Preparation of Y_2O_3:Eu3+ Red Phosphor by Microwave Radiation AITranslate

Hunan Rare Earth Metal Material Research Institute;Hunan Rare Earth Metal Material Research Institute;Hunan Rare Earth Metal Material Research Institute;Hunan Rare Earth Metal Material Research Institute;Hunan Rare Earth Metal Material Research Institute
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Y2O3∶Eu3+ red phosphor was prepared by microwave radiation,and orthogonal experiments were carried out to determine the optimal technological conditions,where heating rate is 20 ℃/min,calcination temperature 1 240 ℃,and holding time 60 min.The sample prepared under the above conditions is of 107.0% relative brightness.The phase structure,granularity and spectra of the sample were analyzed,and the results show that the sample is composed of a single pure phase of Y2O3,and it has uniform particle size of D50=3.28 μm.The maximum peak in the emission spectrum of the sample locate at 607 nm,and the color coordinates of the sample are x=0.653 3、y=0.342 4.

KeyWords AITranslate

Y2O3∶Eu3+ red phosphor microwave radiation orthogonal experiment

1朱伟长,王露.彩色等离子显示器用红色荧光粉的研究现状[J].安徽工业大学学报:自然科学版,2007,24(2):137-139. 被引量:7

2李军建,成建波,刘诗逸,赵纯经.超细Y_2O_3∶Eu荧光粉的制备及其阴极射线发光研究[J].真空科学与技术,2002,22(3):213-216. 被引量:5

3戴德昌,李沅英,蔡少华,谢驭洲,何汉波.(Ce_(0.67)Tb_(0.33))MgAl_(11)O_(19)和BaMgAl_(10)O_(17)∶Eu^(2+)荧光体的微波辐射合成及其发光性能[J].中国稀土学报,1998,16(3):284-287. 被引量:24

1文小强,王玉香,赖华生.微波辐射法合成Gd_(2)O_(2)SO_(4)∶Eu^(3+)发光材料及性能研究[J].稀土,2021(1):105-110.

2杨锦瑜,曾晓岛,朱莉萍,赵建.Eu^(3+)掺杂YPO_4荧光材料的柠檬酸辅助溶胶-凝胶法合成及其荧光性能研究[J].稀有金属与硬质合金,2014,42(4):41-45. 被引量:3

3张彦杰,胡泽青,寇晶,于晶杰,邹念育.(Sr,Ca)AlSiN_3:Eu^(2+)荧光粉的常压合成及其LED封装性能研究[J].照明工程学报,2017,28(1):10-14.

1覃利琴,陶萍芳,王荣芳,陆发权.Tb^(3+)掺杂稀土YPO_4的溶剂热合成及其荧光性能[J].玉林师范学院学报,2015,36(2):45-50. 被引量:1

2孟晓燕,彭思艳,王学军,罗伟,孙宇杰,杨流赛.YPO_4:Ln^(3+)(Ln=Eu,Tb)球形荧光粉的合成及其发光性能优化[J].光电子.激光,2018,29(11):1187-1193. 被引量:5

3郑义,付兵.Sr^(2+)共掺杂LaPO_(4):Tb^(3+)发光材料的水热合成与性能[J].山东化工,2023,52(10):50-53.

1宁小飞,李曼菲,吴杰,焦庆周,柴多里.微波辅助超强酸催化合成乳酸丁酯的研究[J].合肥工业大学学报:自然科学版,2012,35(11):1550-1553. 被引量:3

2张跃文,任跃红,董金龙.微波辐射法合成N-苯基马来酰亚胺[J].光谱实验室,2009,26(2):387-390. 被引量:3

3李西安,马荣萱,刘江飞.微波辐射法合成对羟基苯甲酸丁酯[J].化学与生物工程,2010,27(8):33-35. 被引量:3

4郭超,高俊斌,赵如松,靳广洲.大比表面积惰性Al_2O_3的合成及其载镍催化剂的评价[J].石油炼制与化工,2014,45(10):57-62. 被引量:1

5王涛涛,魏贤勇,齐行振,宗志敏.合成气直接制备低碳烯烃的铁基催化剂的改性[J].化工时刊,2011,25(7):16-18. 被引量:9

6王永秋,何晓玲,黄殊.微波辐射法合成聚天门冬氨酸的研究[J].淮北煤炭师范学院学报:自然科学版,2004,25(4):37-40. 被引量:1

7温燕梅,李思东,钟杰平,陈洪,章超桦.微波辐射法制备N-亚水杨基壳聚糖Schiff碱及其吸附性能的研究[J].应用化学,2006,23(8):892-896. 被引量:2

8张亚男,唐有根,肖方明.微波辐射法合成4-氨基邻苯二甲酰亚胺[J].广州化学,2010,35(2):43-47.

9张博,马飞,白丽丽.微波辐射法合成7-羟基-4-甲基香豆素[J].广东化工,2015,42(4):20-20. 被引量:2

10李丕高,刘彦利.微波辐射法合成对硝基苯苄醚[J].石油化工,2006,35(8):754-756. 被引量:8

Basic Information:

DOI:

Chinese Library Classification Number:TQ133.3[化学工程—无机化工]

Citation Information:

Y2O3∶Eu3+ red phosphor was prepared by microwave radiation,and orthogonal experiments were carried out to determine the optimal technological conditions,where heating rate is 20 ℃/min,calcination temperature 1 240 ℃,and holding time 60 min.The sample prepared under the above conditions is of 107.0% relative brightness.The phase structure,granularity and spectra of the sample were analyzed,and the results show that the sample is composed of a single pure phase of Y2O3,and it has uniform particle size of D50=3.28 μm.The maximum peak in the emission spectrum of the sample locate at 607 nm,and the color coordinates of the sample are x=0.653 3、y=0.342 4.

quote

GB/T 7714-2015 [1] WANG Yan-qi, LIU Yu-hui, OU Yang-yu-ping, et al. Preparation of Y_2O_3:Eu3+ Red Phosphor by Microwave Radiation[J]. Rare Metals and Cemented Carbides, 2011(1): 36-38.
MLA [1] WANG Yan-qi, et al., "Preparation of Y_2O_3:Eu3+ Red Phosphor by Microwave Radiation." Rare Metals and Cemented Carbides, no. 1, 2011, pp. 36-38.
APA [1] WANG Yan-qi, LIU Yu-hui, OU Yang-yu-ping, YU Rong-min, & HUANG Mei-song. (2011). Preparation of Y_2O_3:Eu3+ Red Phosphor by Microwave Radiation. Rare Metals and Cemented Carbides(1), 36-38.
IEEE [1] WANG Yan-qi, LIU Yu-hui, OU Yang-yu-ping, YU Rong-min, and HUANG Mei-song, "Preparation of Y_2O_3:Eu3+ Red Phosphor by Microwave Radiation," Rare Metals and Cemented Carbides, no. 1, pp. 36-38, 2011. keywords: {Y2O3∶Eu3+;red phosphor;microwave radiation;orthogonal experiment}