Direct-Ink Writing Processing of High-k Poly(vinylidene fluoride-trifluoroethylene-chlorofluoroethylene) and Its Integration into an All-Printed Capacitive Touch-Sensing Device Direct-Ink Writing Processing of High-k Poly(vinylidene fluoride-trifluoroethylene-chlorofluoroethylene) and Its Integration into an All-Printed Capacitive Touch-Sensing Device AITranslate

University of Minho; University of Minho; University of Minho;BCMaterials, Basque Center for Materials; University of Minho; LapMET University of Minho
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Direct-ink writing (DIW) printing technology represents a suitable and efficient additive manufacturing technique for producing intricate designs and structures directly on the application surface. This work has demonstrated the potential of combining DIW and screen printing to fabricate an all-printed 7 × 7 capacitive touch sensor based on high dielectric constant (high-k) poly(vinylidene fluoride-trifluoroethylene-chlorofluoroethylene)─P(VDF-TrFE-CFE). The printed device allows a maximum detection signal-to-noise ratio (SNR) of 20 dB, a large touch sensitivity that demonstrates the touch sensor’s ability to detect and respond precisely to user input. Furthermore, by demonstrating the processability of P(VDF-TrFE-CFE) with DIW printing, this research also opens the way for the low-cost fabrication and integration of sensing devices based on this high dielectric constant polymer.

KeyWords AITranslate

directink writing capacitive sensor touch sensing printed electronics P(VDFTrFECFE)
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.3c00962

Chinese Library Classification Number:

Citation Information:

Direct-ink writing (DIW) printing technology represents a suitable and efficient additive manufacturing technique for producing intricate designs and structures directly on the application surface. This work has demonstrated the potential of combining DIW and screen printing to fabricate an all-printed 7 × 7 capacitive touch sensor based on high dielectric constant (high-k) poly(vinylidene fluoride-trifluoroethylene-chlorofluoroethylene)─P(VDF-TrFE-CFE). The printed device allows a maximum detection signal-to-noise ratio (SNR) of 20 dB, a large touch sensitivity that demonstrates the touch sensor’s ability to detect and respond precisely to user input. Furthermore, by demonstrating the processability of P(VDF-TrFE-CFE) with DIW printing, this research also opens the way for the low-cost fabrication and integration of sensing devices based on this high dielectric constant polymer.

quote

GB/T 7714-2015 [1] Nelson Pereira, Rafael S. Pinto, Renato Gonçalves, et al. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.3c00962.
MLA [1] Nelson Pereira, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.3c00962.
APA [1] Nelson Pereira, Rafael S. Pinto, Renato Gonçalves, Carmen R. Tubio, Carlos M. Costa, & Senentxu LancerosMendez. (2023). ACS Applied Electronic Materials(5). https://doi.org/10.1021/acsaelm.3c00962
IEEE [1] Nelson Pereira, Rafael S. Pinto, Renato Gonçalves, Carmen R. Tubio, Carlos M. Costa, and Senentxu LancerosMendez, ACS Applied Electronic Materials, no. 5, 2023, doi: 10.1021/acsaelm.3c00962. keywords: {directink writing capacitive sensor touch sensing printed electronics P(VDFTrFECFE)}