Effects of Mixed Carbon Content on Spark Plasma Sintering of Binder-free Nanostructured WC Cemented Carbides AITranslate
Abstract AITranslate
<Abstrcat>Study is made on the effects of mixed carbon content on the spark plasma sintering binder-free nanostructured WC cemented carbides in respect of the sintering behavior,phase make-up,densification,hardness and grain size.The results showed that direct sintering of pure nano-WC resulted in 300~400 nm sample with high densification and hardness,but the main phase changed into WC1-x and W_2C.With 0.05~0.25% carbon mixed,there is a little WC1-x.With 0.4% carbon mixed,correct phase can be got.With 0.5% carbon mixed,free carbon appears.After ball mixing,the powder can be sintered at lower temperature and when sintering at 1 800 ℃ the grain grows rapidly and unevenly.
KeyWords AITranslate
1Shuichi Imasato,et al.Properties of ultra-fine grain binderless cemented carbide"RCCFN"[J].Internation Journal.of Refractory Metals & Hard Materials,1995,13:305.
2张久兴,刘科高,周美玲.放电等离子烧结技术的发展和应用[J].粉末冶金技术,2002,20(3):129-134. 被引量:142
1张梅琳,朱世根,朱守星.超细及纳米硬质合金中碳含量的变化及对组织性能的影响[J].材料导报,2006,20(8):65-68. 被引量:24
2刘祥庆,林涛,郭志猛,李会谦,罗骥,郝俊杰.无粘结剂硬质合金的研究进展[J].粉末冶金技术,2007,25(4):293-296. 被引量:2
3罗锴,陈强,蔡一湘.放电等离子烧结制备超细碳化钨材料[J].材料研究与应用,2010,4(4):534-537. 被引量:6
4娄静,易健宏,鲍瑞,彭元东,张浩泽.碳含量对微波烧结亚微米硬质合金组织与性能的影响[J].中国钨业,2011,26(1):30-33. 被引量:4
5张立,陈述,黄方杰,单成,程鑫,马鋆.微量钴对无金属粘结相WC硬质合金烧结致密化与WC晶粒生长行为的影响[J].硬质合金,2011,28(5):271-275. 被引量:6
6高建祥,范景莲.无粘结相WC基硬质合金研究进展[J].中国钨业,2011,26(6):22-26. 被引量:5
7周腾,夏铁锋,高立新,张大全.超细无粘结相WC基陶瓷的研究进展[J].硬质合金,2014,31(2):120-124. 被引量:6
8郑虎春,范景莲,杨文华,张忠健,刘涛.VC/Cr_3C_2及配碳量对WC-0.5Co超细硬质合金组织与性能的影响[J].稀有金属材料与工程,2015,44(4):912-917. 被引量:6
9刘璐超,娄丽,吴胜男,杨丽观.无粘结剂硬质合金研究进展与制备[J].材料开发与应用,2015,30(4):93-97. 被引量:1
10张太全,聂洪波,李文强,郑文庆,蔡晓康.无粘结相硬质合金研究进展与应用[J].中国钨业,2018,33(5):64-70. 被引量:9
1刘书祯.超细晶硬质合金晶粒长大抑制剂的研究[J].稀有金属与硬质合金,2007,35(4):51-56. 被引量:21
2吴悦梅,熊计,赖人铭.碳含量对WC-Co硬质合金显微组织的影响及其控制[J].硬质合金,2008,25(3):179-185. 被引量:25
3郑建智,承新,郑勇,严永林,赵能伟.烧结工艺和碳加入量对Mo_2FeB_2基金属陶瓷显微组织和力学性能的影响[J].机械工程材料,2009,33(3):31-34. 被引量:8
4李壮,王家君,林晨光,崔舜.WC-Co超细硬质合金微观结构对其性能的影响[J].硬质合金,2009,26(3):188-193. 被引量:22
5宗霞,鲁玉祥.稀土硬质合金的发展现状[J].矿山机械,2010,38(22):1-6. 被引量:7
6SUN Lan,YANG Tian'en,JIA Chengchang,XIONG Ji.Effects of graphite on the microstructure and properties of ultrafine WC-11Co composites by spark plasma sintering[J].稀有金属:英文版,2011,30(1):63-67. 被引量:1
7刘芳,严峰,张勇,杨贺,陆兴.热压烧结制备无粘结剂碳化钨硬质合金[J].大连交通大学学报,2011,32(1):56-60. 被引量:2
8严峰,吴博,陆兴.一种超细无粘结相WC硬质合金的制备[J].大连交通大学学报,2012,33(4):66-70. 被引量:5
9陈颢,李剑波,羊建高.硬质合金回收研究进展及发展趋势[J].有色金属科学与工程,2012,3(5):18-22. 被引量:17
10秦琴.稀土Y_2O_3对WC-6%Co超细硬质合金组织及性能的影响[J].硬质合金,2013,30(1):14-18. 被引量:12
1张同山.利用回归分析实现烧结生产控制方案的优化组合[J].柳钢科技,1998,0(S1):73-77.
2周卫,徐光,侯悦.无粘结剂冷压成型的天然石墨模具[J].新技术新工艺,1999(4):43-44. 被引量:2
3高海燕,曹顺华.机械合金化制备纳米晶硬质合金粉的进展[J].粉末冶金技术,2003,21(6):355-358. 被引量:6
4罗骥,方哲成,郭志猛,邵慧萍.含V和Cr纳米W粉碳化热力学分析及实验[J].材料热处理学报,2011,32(2):26-29.
5亓家钟.粉末冶金文摘[J].粉末冶金技术,2005,23(6):472-473.
6傅小明.纳米碳化钨的制备技术及研究现状[J].稀有金属与硬质合金,2011,39(1):57-60. 被引量:4
7罗骥,郭志猛,林涛,胡学晟.纳米WC粉氢处理脱除游离碳的研究[J].材料热处理学报,2007,28(1):38-41. 被引量:2
8雷纯鹏,刘刚,唐建成,张方.氧化钨形貌结构对纳米WC粉及其烧结性能的影响[J].稀有金属与硬质合金,2013,41(2):53-57. 被引量:1
9果世驹,李明怡,林涛,赵燕斌,李森蓉,刘广敏,张海波.无粘结剂铁粉的温压工艺研究[J].粉末冶金工业,1996,6(6):5-9. 被引量:10
10果世驹,林涛,魏延萍,蒋龙琴,李森蓉,刘广敏,张海波.细磷铁粉的制备及其对铁粉温压行为的影响[J].粉末冶金技术,1997,15(1):14-17. 被引量:9
Basic Information:
DOI:
Chinese Library Classification Number:TF125.3[冶金工程—粉末冶金]
Citation Information:
<Abstrcat>Study is made on the effects of mixed carbon content on the spark plasma sintering binder-free nanostructured WC cemented carbides in respect of the sintering behavior,phase make-up,densification,hardness and grain size.The results showed that direct sintering of pure nano-WC resulted in 300~400 nm sample with high densification and hardness,but the main phase changed into WC1-x and W_2C.With 0.05~0.25% carbon mixed,there is a little WC1-x.With 0.4% carbon mixed,correct phase can be got.With 0.5% carbon mixed,free carbon appears.After ball mixing,the powder can be sintered at lower temperature and when sintering at 1 800 ℃ the grain grows rapidly and unevenly.
quote
| GB/T 7714-2015 | [1] ZHANG Guo-zhen, WANG Che, ZHANG Jiu-xing, et al. Effects of Mixed Carbon Content on Spark Plasma Sintering of Binder-free Nanostructured WC Cemented Carbides[J]. Rare Metals and Cemented Carbides, 2005(2): 12-15. |
| MLA | [1] ZHANG Guo-zhen, et al., "Effects of Mixed Carbon Content on Spark Plasma Sintering of Binder-free Nanostructured WC Cemented Carbides." Rare Metals and Cemented Carbides, no. 2, 2005, pp. 12-15. |
| APA | [1] ZHANG Guo-zhen, WANG Che, ZHANG Jiu-xing, ZHOU Mei-ling, & ZHONG Tao-xing. (2005). Effects of Mixed Carbon Content on Spark Plasma Sintering of Binder-free Nanostructured WC Cemented Carbides. Rare Metals and Cemented Carbides(2), 12-15. |
| IEEE | [1] ZHANG Guo-zhen, WANG Che, ZHANG Jiu-xing, ZHOU Mei-ling, and ZHONG Tao-xing, "Effects of Mixed Carbon Content on Spark Plasma Sintering of Binder-free Nanostructured WC Cemented Carbides," Rare Metals and Cemented Carbides, no. 2, pp. 12-15, 2005. keywords: {SPS;mixed carbon comtent;nanostructured cemented carbides;binder-free cemented carbides} |