Study of Two-step Carbonization for the Production of Fine grained Taed Carbide AITranslate

Zhuzhou Cemented Carbide Factory Tantalum Niobium Products Branch
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Study is made of two step carbonization for the production of fine grained Ta carbide. The main factors affecting the product particle size and quality have been investigated.The powder preparation by cemented carbide lined ball mill (use cemented carbide balls as medium),instead of the high capacity pulverizers,will result in smaller particle size and lower Fe content. The Ta carbide from the serial production with the new technological parameters features finer particle size and lower impurity content.The product's quality is satisfactory for the cemented carbide industry.

KeyWords AITranslate

two step carbonization fine grained Ta carbide technological study

1周菊秋,黄列如,谭日善,张同桂,李光辉,曾芳屏.中国钽、铌碳化物的生产和应用[J].稀有金属材料与工程,1998,27(1):26-31. 被引量:14

2王肇信.钽铌冶金学[M].稀有金属冶金学会、钽铌冶金专业委员会,1998..

1王时光.难熔金属碳化物调配的精准计算[J].稀有金属与硬质合金,2006,34(4):32-39. 被引量:2

2张浩,朱芳.钽、铌碳化物制备技术的研究进展[J].稀有金属与硬质合金,2009,37(2):47-49. 被引量:8

3梁昌明.硬质合金用超细碳化铌(钽)粉生产工艺条件及质量控制的探讨[J].稀有金属与硬质合金,2012,40(4):63-67. 被引量:1

4李成晨,宋珂.原位扩散反应制备细TaC颗粒的研究[J].稀有金属与硬质合金,2013,41(1):32-34.

5黄云红,白掌军,王强,暴怀乾.超细碳化铌制备工艺的研究[J].宁夏工程技术,2018,17(3):211-213.

1张浩,朱芳.钽、铌碳化物制备技术的研究进展[J].稀有金属与硬质合金,2009,37(2):47-49. 被引量:8

2姜爱民,蒋显全,陈巧旺,陈异.晶粒长大抑制剂在硬质合金中的应用概况[J].硬质合金,2010,27(4):252-257. 被引量:13

3梁昌明.硬质合金用超细碳化铌(钽)粉生产工艺条件及质量控制的探讨[J].稀有金属与硬质合金,2012,40(4):63-67. 被引量:1

4李力,张崇才,陈慧,王权.烧结温度对WC-16TiC-4TaC-9Co硬质合金微观组织与性能的影响[J].重庆文理学院学报:社会科学版,2013,32(5):4-7.

5刘玉宝,李麟,张先恒,赵二雄.碳化铌的合成方法及应用研究进展[J].稀有金属与硬质合金,2014,42(1):66-69. 被引量:4

6陈慧,彭玲玲,姜中涛,邓莹,涂铭旌.真空烧结温度对WC-TiC-TaC-Co硬质合金组织和性能的影响[J].粉末冶金工业,2015,25(3):33-36. 被引量:9

7爨炳辰,谢征芳.碳化钽陶瓷材料制备方法的研究进展[J].陶瓷,2017,0(4):38-42. 被引量:1

8黄云红,白掌军,王强,暴怀乾.超细碳化铌制备工艺的研究[J].宁夏工程技术,2018,17(3):211-213.

9陈军强,孙青竹,万桂林,吕雯,杨芮.添加剂对Ti(C,N)基金属陶瓷的力学性能影响[J].科技资讯,2020,18(4):54-54.

10杨家富,陈伟鹏,赵增武,郑坤灿,庞雅丹,赵光进.真空碳热还原制备碳化钛和碳化铌粉体的研究[J].稀有金属与硬质合金,2020,48(4):28-32. 被引量:1

1Schas.,E,李新华.碳化钽技术[J].国外难熔金属与硬质材料,1992,8(1):13-20. 被引量:1

2魏圆良,刘利斌,李书巍.硬质合金衬板浸润焊技术研究及试验[J].金属加工:热加工,2013(10):39-41. 被引量:1

3刘多鹏,吴志华,周兰志,李强雄.一种长寿命高炉布料溜槽耐磨衬板[J].安徽冶金科技职业学院学报,2017,27(1):34-36. 被引量:2

4V.A.Falkovsky,张外平,李仁琼.复合碳化物硬质合金[J].国外难熔金属与硬质材料,2004,20(2):1-3.

5朱泽华.硬质合金中碳化锆铌替代碳化钽的研究[J].稀有金属与硬质合金,1993,21(S1):384-388.

6徐磊.爆炸成型法制备碳化钽陶瓷[J].机械工程材料,2010,34(9):57-59.

7于仁波,王庆柱,冯义平.高炉上料系统设备故障分析及改进[J].山东冶金,2011,33(4):79-79. 被引量:1

8V.A.Falkovsky,陈满元.多元碳化物硬质合金[J].国外难熔金属与硬质材料,2002,18(1):1-3. 被引量:1

Basic Information:

DOI:

Chinese Library Classification Number:TF123.3[冶金工程—粉末冶金]

Citation Information:

Study is made of two step carbonization for the production of fine grained Ta carbide. The main factors affecting the product particle size and quality have been investigated.The powder preparation by cemented carbide lined ball mill (use cemented carbide balls as medium),instead of the high capacity pulverizers,will result in smaller particle size and lower Fe content. The Ta carbide from the serial production with the new technological parameters features finer particle size and lower impurity content.The product's quality is satisfactory for the cemented carbide industry.

quote

GB/T 7714-2015 [1] TANG Ren-zhong. Study of Two-step Carbonization for the Production of Fine grained Taed Carbide[J]. Rare Metals and Cemented Carbides, 2000(1): 5-9.
MLA [1] TANG Ren-zhong. "Study of Two-step Carbonization for the Production of Fine grained Taed Carbide." Rare Metals and Cemented Carbides, no. 1, 2000, pp. 5-9.
APA [1] TANG Ren-zhong. (2000). Study of Two-step Carbonization for the Production of Fine grained Taed Carbide. Rare Metals and Cemented Carbides(1), 5-9.
IEEE [1] TANG Ren-zhong, "Study of Two-step Carbonization for the Production of Fine grained Taed Carbide," Rare Metals and Cemented Carbides, no. 1, pp. 5-9, 2000. keywords: {two step carbonization;fine grained Ta carbide;technological study}