Research into EDM of Cemented Carbide Dies AITranslate

Hunan Zhuzhou Vocational and Technical College
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Experiments and research have been carried out on the electric parameters of EDM of cemented carbide dies, the tool electrode materials and its size calculation Analysis is made of the factors affecting the EDM and the influence of the EDM on the service life of the dies. The paper points out that it is necessary to use CAD/CAM for shape complicated tool electrodes machining;and NC EDM can be used for shape complicated dies.

KeyWords AITranslate

cemented carbide die EDM research

1李沐山.八十年代世界硬质合金技术进展[M].株州:《硬质合金》编辑部,1991,9..

2何云.硬质合金电火花加工效率研究[J].硬质合金,1998,15(4):253-256. 被引量:6

3蔡复之.实用数控加工技术[M].北京:兵器工业出版社,1995,4..

4全国数控培训网络天津分中心.数控编程[M].北京:机械工业出版社,1996,5..

1雍耀维,郭常宁,胡德金.不同电极电火花加工硬质合金的效率研究[J].电加工与模具,2004(6):4-6. 被引量:6

2汤辉.硬质合金电火花加工设备的选型和应用[J].稀有金属与硬质合金,2013,41(6):58-62. 被引量:2

3姚晨佼,李亮,何宁,赵国龙,吴贤.脉冲光纤激光诱导氧化硬质合金的温度场分布[J].中国机械工程,2017,28(3):334-339.

4张乾坤,李苏望,孙红丁,贺跃辉,江垚,陈豫章,肖逸锋.高效加工硬质合金沉孔用新型金刚石工具与工艺研究[J].金刚石与磨料磨具工程,2018,38(2):47-50.

1杨建明,乔斌,李化强.电火花加工用工具电极材料的研究进展[J].工具技术,2007(8):13-16. 被引量:14

2杨雄,冉小丰,帅玉妹,陈松.GT35钢结硬质合金电火花加工工艺试验[J].硬质合金,2009,26(4):236-239. 被引量:5

3文武,王西彬,龙震海,朱朝阳.4Cr5MoVSi电火花加工试验特征规律研究[J].工具技术,2010,44(1):29-31.

4雍耀维,唐博.电极材料对极间放电电压及加工特性影响[J].机械设计与制造,2012(6):103-105. 被引量:9

5宋满仓,解廷利,于超,王华,王敏杰.电火花线切割加工铜钨合金切缝宽度及加工精度影响因素研究[J].电加工与模具,2012(4):5-8. 被引量:3

6雍耀维,郭常宁.铜钨电极材料的电加工性能实验研究[J].机床与液压,2016,44(11):84-87. 被引量:1

7吴海会,王彤,王俊棋,尹洪石.基于Cr12MoV模具钢水雾中电火花线切割工艺研究[J].硬质合金,2017,34(2):120-128.

8吴海会,王彤,王俊棋,尹洪石.超声水雾中电火花线切割精加工特性研究[J].硬质合金,2017,34(3):179-185. 被引量:1

1郭生涛.五轴加工中心在汽车模具制造中的应用[J].金属加工:冷加工,2013(10):25-26. 被引量:3

2吴利红.细长平行面的铣削方法[J].科技视界,2014(6):245-246.

3龙燕.面铣削质量分析[J].科技致富向导,2011(11):93-93. 被引量:1

4名词解释[J].制造技术与机床,2016,0(7):129-129.

5李新,薛强.色选机滑槽专用抛光机的设计[J].机械设计,2009(1):74-75. 被引量:1

6冬雪.森精机GV-503/5A五轴联动立式加工中心[J].世界制造技术与装备市场,2003(1):55-55.

7杨佩旋,王成勇,廖艳培,袁慧.微磨料浆体射流抛光技术[J].金刚石与磨料磨具工程,2008,28(3):19-25. 被引量:6

8张雷,周锦进.电化学磁力复合加工工艺的试验研究[J].电加工与模具,2000(5):38-40. 被引量:4

9姬书得,方洪渊,刘雪松,孟庆国.混流式水轮机转轮焊接过程数值模拟的特殊性分析[J].焊接学报,2005,26(7):71-74. 被引量:4

10刘丽宏.大气腐蚀的研究和应用——《大气腐蚀》书评[J].表面工程资讯,2005,5(4):57-58.

Basic Information:

DOI:

Chinese Library Classification Number:TG661[金属学及工艺—金属切削加工及机床];TG135.5[一般工业技术—材料科学与工程]

Citation Information:

Experiments and research have been carried out on the electric parameters of EDM of cemented carbide dies, the tool electrode materials and its size calculation Analysis is made of the factors affecting the EDM and the influence of the EDM on the service life of the dies. The paper points out that it is necessary to use CAD/CAM for shape complicated tool electrodes machining;and NC EDM can be used for shape complicated dies.

quote

GB/T 7714-2015 [1] HU Huang-qing. Research into EDM of Cemented Carbide Dies[J]. Rare Metals and Cemented Carbides, 2000(1): 9-14.
MLA [1] HU Huang-qing. "Research into EDM of Cemented Carbide Dies." Rare Metals and Cemented Carbides, no. 1, 2000, pp. 9-14.
APA [1] HU Huang-qing. (2000). Research into EDM of Cemented Carbide Dies. Rare Metals and Cemented Carbides(1), 9-14.
IEEE [1] HU Huang-qing, "Research into EDM of Cemented Carbide Dies," Rare Metals and Cemented Carbides, no. 1, pp. 9-14, 2000. keywords: {cemented carbide die;EDM;research}