Study on Optimization of Chemical Composition of the Adhesive Phase in Cemented Carbide Roll Ring for Low Temperature Rolling AITranslate
Abstract AITranslate
Study on optimization of chemical composition of the adhesive phase in cemented carbide roll ring was emphatically carried out.The results of the first-principle calculation show that increasing the nickel content in the adhesive phase can stabilize the face-centered cubic structure of the adhesive phase,weaken the bondability and reduce the magnetic properties,thereby significantly improving the fracture toughness and ductility of the cemented carbide.The experimental results show that the fracture toughness of the cemented carbide is increased by 29%after all the cobalt in the adhesive phase is replaced with nickel.The new series of high-nickel cemented carbide roll ring products,which is developed according this achievement,has significantly reduced cracking phenomenon during low-temperature rolling of rebar steel.
KeyWords AITranslate
1龙坚战,彭文.高线辊环精轧过程中热疲劳行为研究[J].硬质合金,2010,27(6):344-348. 被引量:4
2郭圣达,张正富.WC-Co类硬质合金疲劳特性研究现状[J].材料导报,2009,23(11):69-72. 被引量:20
3完卫国,李祥才.棒线材低温轧制技术发展[J].中国冶金,2005,15(1):11-16. 被引量:19
4马靳江,周民,陈莹卷.线材减定径关键工艺装备技术的研究与开发[J].钢铁技术,2018(2):19-23. 被引量:1
5苟复钢,王运良,蔡虎情.控制轧制和控制冷却在棒材轧制中的应用[J].中国金属通报,2018(1):91-91. 被引量:2
6谭智.高速线材轧制用WC辊环的应用与碎辊原因分析[J].硬质合金,1999,16(3):166-169. 被引量:8
7方晴,王忆民.硬质合金轧辊的使用失效及其原因分析[J].硬质合金,2007,24(4):219-225. 被引量:14
8金益民.粘结相强化及其在辊环中的应用[J].硬质合金,2011,28(2):126-129. 被引量:4
9白佳声,封志奎,张鹤年,沈树亭.粘结剂中加入镍、铬对辊环用硬质合金材质性能影响的研究[J].粉末冶金技术,1993,11(1):43-46. 被引量:5
10陶辉锦,陈伟民,王赫男.镍晶格稳定性的第一性原理研究[J].材料导报,2009,23(18):83-85. 被引量:1
1刘和平,阳湘琳,彭秧锡,周颖,谢长青,赵勇.硬质合金辊环的高温法回收与循环利用[J].硬质合金,2021,38(6):434-440. 被引量:2
2柯鹏,刘豪,朱立荣,曹群,廖子剑,王海涛,龙坚战.钢材低温轧制技术研发现状与展望[J].硬质合金,2023,40(4):319-327.
1刘海军,伍文辉,汪巍,金鹏,孔德方,龙坚战,谭立群.不同粘结剂成分WC-30%(Co-Ni-Cr)粗晶硬质合金高温氧化行为的研究[J].硬质合金,2022,39(3):182-188. 被引量:2
2刘豪,孟湘君,管玉明,曹群,崔亮亮,夏艳萍,蒋甘澍.硬质合金辊环材料研究现状与发展趋势[J].硬质合金,2022,39(6):505-512. 被引量:3
1马生花,解玉龙,王万玺.富镍三元正极材料的改性研究进展[J].化工新型材料,2021,49(7):42-46.
2何栋梁,成彦惠.基于“1+X证书”制度的土建类专业成人高等 教育的课程体系设计[J].知识经济,2021(15):124-125.
3贺毅强,苏前航,徐虎林,任昌旭,徐苏,穆昱学,刘勇.AlxFeNiSiTi高熵合金的显微组织与力学性能研究[J].稀有金属与硬质合金,2021,49(4):71-75.
4王红军,石宇,侯强.着色探伤在碳化钨辊环上的应用[J].设备管理与维修,2021(15):114-115.
5吴磊,浦娟,吴铭方,龙伟民,钟素娟,胡庆贤,蓝阳.不同碳化钨含量对等离子弧熔覆镍基碳化钨涂层组织及性能的影响[J].材料导报,2021,35(16):16111-16114. 被引量:1
6崔桂梅,刘伟,张帅,王磊.基于差分进化支持向量机的轧制力预测[J].中国测试,2021,47(8):83-88. 被引量:4
7范金辉,李鹏飞,梁晓军,梁建平,徐长征,蒋力,叶祥熙,李志军.镍-不锈钢复合板轧制过程中界面的结合机制[J].材料研究学报,2021,35(7):493-500. 被引量:2
8吕建勋.桁架梁用热轧盘条焊接失效断裂原因分析[J].金属制品,2021,47(4):47-50.
Basic Information:
DOI:
Chinese Library Classification Number:TG135.5[一般工业技术—材料科学与工程]
Citation Information:
Study on optimization of chemical composition of the adhesive phase in cemented carbide roll ring was emphatically carried out.The results of the first-principle calculation show that increasing the nickel content in the adhesive phase can stabilize the face-centered cubic structure of the adhesive phase,weaken the bondability and reduce the magnetic properties,thereby significantly improving the fracture toughness and ductility of the cemented carbide.The experimental results show that the fracture toughness of the cemented carbide is increased by 29%after all the cobalt in the adhesive phase is replaced with nickel.The new series of high-nickel cemented carbide roll ring products,which is developed according this achievement,has significantly reduced cracking phenomenon during low-temperature rolling of rebar steel.
quote
| GB/T 7714-2015 | [1] LIU He-ping, LI Jin, ZHOU Ying, et al. Study on Optimization of Chemical Composition of the Adhesive Phase in Cemented Carbide Roll Ring for Low Temperature Rolling[J]. Rare Metals and Cemented Carbides, 2021(4): 81-86. |
| MLA | [1] LIU He-ping, et al., "Study on Optimization of Chemical Composition of the Adhesive Phase in Cemented Carbide Roll Ring for Low Temperature Rolling." Rare Metals and Cemented Carbides, no. 4, 2021, pp. 81-86. |
| APA | [1] LIU He-ping, LI Jin, ZHOU Ying, PENG Yang-xi, XIE Chang-qing, & ZHAO Yong. (2021). Study on Optimization of Chemical Composition of the Adhesive Phase in Cemented Carbide Roll Ring for Low Temperature Rolling. Rare Metals and Cemented Carbides(4), 81-86. |
| IEEE | [1] LIU He-ping, LI Jin, ZHOU Ying, PENG Yang-xi, XIE Chang-qing, and ZHAO Yong, "Study on Optimization of Chemical Composition of the Adhesive Phase in Cemented Carbide Roll Ring for Low Temperature Rolling," Rare Metals and Cemented Carbides, no. 4, pp. 81-86, 2021. keywords: {cemented carbide;roll ring;adhesive phase;nickel content;low temperature rolling;first-principle calculation} |