Experimental Study on Milling Stainless Steel by Cemented Carbide Tools with Different Matrix AITranslate

Zhuzhou Cemented Carbide Cutting Tools Co.,Ltd.;Zhuzhou Cemented Carbide Cutting Tools Co.,Ltd.;Zhuzhou Cemented Carbide Cutting Tools Co.,Ltd.;Zhuzhou Cemented Carbide Cutting Tools Co.,Ltd.
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Dry milling tests were conducted for 1 Cr18 Ni9 Ti stainless steel by using cemented carbide tools with different matrix materials.The tools with different milling time were observed before and after corrosion by SEM and EDS,and the tool life and failure mechanism were compared and analyzed to obtain the basis for tool matrix material selection in dry milling of 1 Cr18 Ni9 Ti stainless steel.The experimental results show that adhesive wear,oxidation wear,thermal fatigue and boundary wear are the main failure mechanisms of the tools.The cutting condition of intermittent cutting and grinding chips in stainless steel milling is the basic reason for thermal fatigue of the tool.The cemented carbide tools with the three kinds of matrix show the same characteristics of thermal fatigue.There is a good corresponding relationship between the boundary wear of the tool and the toughness of the matrix.The worse the toughness,the more serious the boundary wear.When choosing the tools for dry milling of stainless steel,the single index of toughness or hardness can not be used as the basis for selecting tool matrix,while the matrix material with appropriate comprehensive mechanical properties can be selected.

KeyWords AITranslate

cemented carbide tool matrix material stainless steel milling failure mechanism

1王庭俊,周建华.1Cr18Ni9Ti不锈钢的切削加工[J].工具技术,2009,43(7):63-67. 被引量:21

2程志青,范君艳,梁良.WC-Ni3Al硬质合金切削奥氏体不锈钢的切削力及磨损研究[J].工具技术,2020,54(3):24-27. 被引量:4

3张好强,庞思勤,王西彬,程剑兵,李慎旺.不同晶粒度硬质合金刀具切削不锈钢的试验研究[J].稀有金属与硬质合金,2016,44(2):76-80. 被引量:3

4何光春,王丽娟.超细硬质合金刀具YW2A车削06Cr19Ni10不锈钢的切削性能[J].机床与液压,2014,42(2):33-35. 被引量:3

5尹飞,陈康华,王社权.基体的梯度结构对涂层硬质合金性能的影响[J].中南大学学报:自然科学版,2005,36(5):776-779. 被引量:15

6王社权,陈康华,徐银超,祝昌军,谢灿强,陈响明.基体梯度结构对TiN涂层硬质合金力学和切削性能的影响[J].中国有色金属学报,2011,21(4):804-809. 被引量:6

7周建涛,邓建新,李友生.高速铣削69111不锈钢的硬质合金刀具磨损机理研究[J].制造技术与机床,2010(9):94-96. 被引量:3

8金鹏,彭文.硬质合金导热系数的研究[J].硬质合金,2015,32(5):300-305. 被引量:8

9何耿煌,吴冲浒,刘献礼,张守全,邹伶俐.断续切削过程硬质合金可转位刀片破损行为研究[J].金刚石与磨料磨具工程,2015,35(3):10-16. 被引量:11

10罗学全,于涛,蒋双双,江爱胜.TC4钛合金高速铣削加工刀具失效机理研究[J].工具技术,2019,53(9):43-46. 被引量:6

1李文辉,温学杰,李秀红,张演.整体叶盘抛磨技术研究现状及其发展趋势[J].航空制造技术,2022,65(17):88-102.

1周明佳,孙艳茹,逄崇雁.刀具磨损对屑形变化的影响分析[J].科学技术创新,2021(6):180-181. 被引量:1

2张杰翔,张伟,李志永,闫方清,刘俨后,赵玉刚.切削参数对子午线轮胎模具侧板切削比能及表面粗糙度的影响研究[J].机床与液压,2021,49(14):36-40.

3宋文刚,刘战强,吕文军.工件初始表面几何状态对铣削力及表面形貌的影响[J].工具技术,2021,55(7):28-32. 被引量:2

4赵雪峰,秦浩,杨勇,李辉.双磁盘磁力钝化参数对刀具刃口的影响[J].组合机床与自动化加工技术,2021(8):52-56. 被引量:1

5一种纳织构原子层沉积二硫化钼软涂层刀具及其制备方法[J].中国钼业,2021,45(4):29-29.

6马利云,金建會.表面处理对38CrMoAlA和ZQSn10⁃2⁃3摩擦副性能的影响[J].机床与液压,2021,49(16):55-59. 被引量:1

7庞俊忠,牛苜森.高速铣削3Cr2Mo钢时硬度对表面粗糙度的影响规律[J].工具技术,2021,55(8):57-60.

8鲍久圣,董慧丽,阴妍,郭超勋,赵少迪,艾俊伟.交变磁场对制动器摩擦噪声抑制的试验研究[J].振动工程学报,2021,34(4):838-848. 被引量:4

9沈明学,秦涛,李圣鑫,彭金方,熊光耀,朱旻昊.宽温域下高速轮轨界面粘着与车轮表面损伤行为[J].交通运输工程学报,2021,21(3):269-278. 被引量:4

Basic Information:

DOI:

Chinese Library Classification Number:TG135.5[一般工业技术—材料科学与工程]

Citation Information:

Dry milling tests were conducted for 1 Cr18 Ni9 Ti stainless steel by using cemented carbide tools with different matrix materials.The tools with different milling time were observed before and after corrosion by SEM and EDS,and the tool life and failure mechanism were compared and analyzed to obtain the basis for tool matrix material selection in dry milling of 1 Cr18 Ni9 Ti stainless steel.The experimental results show that adhesive wear,oxidation wear,thermal fatigue and boundary wear are the main failure mechanisms of the tools.The cutting condition of intermittent cutting and grinding chips in stainless steel milling is the basic reason for thermal fatigue of the tool.The cemented carbide tools with the three kinds of matrix show the same characteristics of thermal fatigue.There is a good corresponding relationship between the boundary wear of the tool and the toughness of the matrix.The worse the toughness,the more serious the boundary wear.When choosing the tools for dry milling of stainless steel,the single index of toughness or hardness can not be used as the basis for selecting tool matrix,while the matrix material with appropriate comprehensive mechanical properties can be selected.

quote

GB/T 7714-2015 [1] LUO Xue-quan, YU Tao, WEN Guang-hua, et al. Experimental Study on Milling Stainless Steel by Cemented Carbide Tools with Different Matrix[J]. Rare Metals and Cemented Carbides, 2021(4): 87-93.
MLA [1] LUO Xue-quan, et al., "Experimental Study on Milling Stainless Steel by Cemented Carbide Tools with Different Matrix." Rare Metals and Cemented Carbides, no. 4, 2021, pp. 87-93.
APA [1] LUO Xue-quan, YU Tao, WEN Guang-hua, & WANG She-quan. (2021). Experimental Study on Milling Stainless Steel by Cemented Carbide Tools with Different Matrix. Rare Metals and Cemented Carbides(4), 87-93.
IEEE [1] LUO Xue-quan, YU Tao, WEN Guang-hua, and WANG She-quan, "Experimental Study on Milling Stainless Steel by Cemented Carbide Tools with Different Matrix," Rare Metals and Cemented Carbides, no. 4, pp. 87-93, 2021. keywords: {cemented carbide tool;matrix material;stainless steel;milling;failure mechanism}