Influence Law of Solution pH on Separation of Vanadium and Tungsten by Ion Exchange Adsorption AITranslate
Abstract AITranslate
Abstract.Selective separation of vanadium and tungsten from the simulated NaOH leaching solution of waste SCR denitration catalyst by anion exchange resin was studied. The effect of solution pH change on adsorption behavior of vanadium and tungsten onto the resin was investigated. The experimental results show that solution pH change has little influence on W adsorption under the alkaline condition,but has re- markable influence on V adsorption. When pH increases from 8 to 12, the main ion form of V is trans- formed from V4O12^4- to HVO4^2- , resulting in greatly reduced adsorption ability of V onto the resin. When pH increases from 12 to 14,the increase of OH^- concentration becomes the main factor affecting the ad- sorption of V and W. Due to the adsorption capacity of WO4^2-〉VO4^3-〉OH^- ,the inhibition effect of in- creased OH^- concentration on V adsorption is more obvious,resulting in further weakening of V adsorp- tion. As pH increases from 8 to 14,W/V separation coefficient increases from 0. 146 to 2.36. When pH is equal to 14 and the loaded resin is eluted with a mixed solution of 1 mol/L NaOH + 2 mol/L NaCl,the maximum desorption concentration of W can reach 84 g/L,while the maximum value of V is not more than 2 g/L. As a result,the separation of tungsten and vanadium is achieved to some extent,tungsten is enriched to a certain extent,and the desorbed liquid can be used as a mother liquid for the subsequent calcium pre- cipitation or crystallization process.
KeyWords AITranslate
1陈其颢,朱林.SCR失效催化剂及其处置与再利用技术[J].电力科技与环保,2012,28(3):27-28. 被引量:11
2李化全,郭传华.废弃脱硝催化剂中有价元素钛钒钨的综合利用研究[J].无机盐工业,2014,46(5):52-54. 被引量:20
3李俊峰,张兵兵,李翼然.基于钒钛基SCR法废脱硝催化剂的回收利用[J].广州化工,2014,42(24):130-132. 被引量:18
4张家靓,赵中伟.W(Ⅵ)-V(Ⅴ)-H_2O体系钨钒分离的热力学分析[J].中国有色金属学报,2014,24(6):1656-1662. 被引量:11
5刘茂盛,孙培梅,李运姣,李洪桂.关于钨冶炼离子交换工艺除杂效果的探讨[J].稀有金属与硬质合金,1990(2):8-15. 被引量:8
6宋阜,朱宾权.离子交换法分离富集钨酸钠溶液中的钒[J].稀有金属与硬质合金,2006,34(3):5-7. 被引量:14
7张云,范必威,林海玲,马江舟,陆世银,王海平,吕树环.D290树脂从石煤酸浸液中吸附钒的工艺[J].矿物岩石,2000,20(4):95-98. 被引量:19
8郝喜才,胡斌杰,邱永宽.离子交换法回收废钒催化剂中钒的研究[J].无机盐工业,2007,39(2):52-54. 被引量:23
1杨丽娜,成宝海,李青芸,徐乔楚.用201×7离子交换树脂从石煤含钒浸出液中提钒的研究[J].化学工程与装备,2021(6):7-9. 被引量:2
2韩桂洪,王旱雨,苏胜鹏,黄艳芳,刘兵兵.溶解态钨钒选择性分离技术研究进展及探讨[J].中国有色金属学报,2021,31(11):3380-3395. 被引量:3
3肖露萍,陈星宇,刘旭恒,赵中伟.采用水合氧化铁吸附钨酸钠溶液中的钒及其吸附特性[J].中南大学学报:自然科学版,2022,53(6):1998-2006.
1韩桂洪,王静雯,刘兵兵,孙虎,黄艳芳.湿法炼锌净化钴渣回收钴技术进展及展望[J].贵州大学学报:自然科学版,2022,39(2):1-6. 被引量:1
2程倩,赵笑益,王望泊,宁新霞,周丽萍,曹欢,康敏,王勇.用D201树脂从石煤钒矿酸浸液中提钒[J].有色金属:冶炼部分,2022(5):38-44. 被引量:1
3贾蓝波,王玲,郭紫璇,熊雨婷,夏亮亮,王龙,聂轶苗,刘淑贤.含钒溶液萃取分离富集钒的研究进展[J].中国有色金属学报,2022,32(11):3489-3504. 被引量:1
4赖永传,杨鑫龙,孙建之,尚鹤,莫晓兰,温建康.石煤含氟酸浸液中V(Ⅴ)-Fe(Ⅲ)-F-H_(2)O系钒铁分离热力学研究[J].中南大学学报:自然科学版,2023,54(5):1703-1712.
5王泽玮,张伟光,梁新星,刘远,喻亮,曹雪娇,蔡震雷,胡磊.拜耳循环母液中钒的选择性吸附性能及机理[J].有色金属科学与工程,2023,14(4):460-466.
1赵华轩,郎印海.磁性生物炭对水中CIP和OFL的吸附行为和机制[J].环境科学,2018,39(8):3729-3735. 被引量:14
2庄艾春,肖红新.碱熔-等离子体发射光谱法快速测定钽铌矿中钽和铌[J].广东化工,2018,45(9):222-223. 被引量:3
3王乐乐,何川,王凯,潘力,熊加林,孔凡海,宋玉宝,雷嗣远.SCR脱硝催化剂低负荷运行评估技术研究与应用[J].热力发电,2018,47(10):24-30. 被引量:14
4陈书锐,马兰,杨绍利.废钛基SCR脱硝催化剂回收处理研究现状及发展趋势[J].化学工程与技术,2018,8(4):233-241. 被引量:2
5陈良健.氮气吸附法与压汞法测量SCR脱硝催化剂孔容孔径的应用[J].化工管理,2018(28):195-197. 被引量:2
6赵恒勤,宁阳坤,王威,张博,刘红召,任保增.D314树脂吸附钼的试验研究[J].矿冶工程,2018,38(1):81-83. 被引量:5
7杨展鸿,王伟辉,吴川,黄钧宜,阮小林,董明.固体吸附管采样-离子色谱法测定工作场所空气中二氧化氮[J].中国职业医学,2018,45(5):606-608. 被引量:5
8钱如胜,张云升,张宇,杨永敢.水泥-粉煤灰体系早龄期液相离子浓度与电导率的关系[J].材料导报,2018,32(12):2066-2071. 被引量:3
9刘金璐,雷永平,王晓林,钟方丽.刺玫果总皂苷的纯化工艺及体外活性研究[J].吉林化工学院学报,2018,35(9):16-23. 被引量:1
10张颖,杨双双,王蕾,付嘉伟,李瑞,张杏,薛越文,刘璐瑶.Arthrobacter sp.JQ-1菌株胞外聚合物对DEHP吸附特性研究[J].东北农业大学学报,2018,49(10):34-42. 被引量:1
Basic Information:
DOI:
Chinese Library Classification Number:TF804.3[冶金工程—有色金属冶金]
Citation Information:
Abstract.Selective separation of vanadium and tungsten from the simulated NaOH leaching solution of waste SCR denitration catalyst by anion exchange resin was studied. The effect of solution pH change on adsorption behavior of vanadium and tungsten onto the resin was investigated. The experimental results show that solution pH change has little influence on W adsorption under the alkaline condition,but has re- markable influence on V adsorption. When pH increases from 8 to 12, the main ion form of V is trans- formed from V4O12^4- to HVO4^2- , resulting in greatly reduced adsorption ability of V onto the resin. When pH increases from 12 to 14,the increase of OH^- concentration becomes the main factor affecting the ad- sorption of V and W. Due to the adsorption capacity of WO4^2-〉VO4^3-〉OH^- ,the inhibition effect of in- creased OH^- concentration on V adsorption is more obvious,resulting in further weakening of V adsorp- tion. As pH increases from 8 to 14,W/V separation coefficient increases from 0. 146 to 2.36. When pH is equal to 14 and the loaded resin is eluted with a mixed solution of 1 mol/L NaOH + 2 mol/L NaCl,the maximum desorption concentration of W can reach 84 g/L,while the maximum value of V is not more than 2 g/L. As a result,the separation of tungsten and vanadium is achieved to some extent,tungsten is enriched to a certain extent,and the desorbed liquid can be used as a mother liquid for the subsequent calcium pre- cipitation or crystallization process.
quote
| GB/T 7714-2015 | [1] LIU Ding-ding, SONG Hao, WU Wei-hong, et al. Influence Law of Solution pH on Separation of Vanadium and Tungsten by Ion Exchange Adsorption[J]. Rare Metals and Cemented Carbides, 2018(5): 7-12. |
| MLA | [1] LIU Ding-ding, et al., "Influence Law of Solution pH on Separation of Vanadium and Tungsten by Ion Exchange Adsorption." Rare Metals and Cemented Carbides, no. 5, 2018, pp. 7-12. |
| APA | [1] LIU Ding-ding, SONG Hao, WU Wei-hong, ZHENG Cheng-hang, QIU Kun-zan, & GAO Xiang. (2018). Influence Law of Solution pH on Separation of Vanadium and Tungsten by Ion Exchange Adsorption. Rare Metals and Cemented Carbides(5), 7-12. |
| IEEE | [1] LIU Ding-ding, SONG Hao, WU Wei-hong, ZHENG Cheng-hang, QIU Kun-zan, and GAO Xiang, "Influence Law of Solution pH on Separation of Vanadium and Tungsten by Ion Exchange Adsorption," Rare Metals and Cemented Carbides, no. 5, pp. 7-12, 2018. keywords: {waste SCR denitration eatalyst;separation of vanadium and tungsten;ion exchange;pH;ion form} |