Study on Installation Depth Optimization of the Agitator in the Rare Earth Extraction Tank without Baffles AITranslate
Abstract AITranslate
Using a 200 L front chamber extraction tank without batiles as the model,and based on the dis- tance of the original agitator from the bottom of the mixing chamber (installation depth) b= 60 mm, the mixing process of feed liquid and P507 in the rare earth mixing chamber was simulated at 5 mm intervals through fluid dynamics Fluent software. Suction pressure, suction flow velocity and agitating power were used as evaluation criteria to analyze the effect of installation depth on suction performance of the agitator through the simulation analysis with different agitator installation depth. The optimized installation depth b = 50 mm is determined,which provides theoretical guidance for on-site debugging and installation of agita- tors. The results from simulation analysis show that when the installation depth keeps 50 mm,the suction negative pressure is --140.2 Pa, the suction flow velocity is 1.25 m/s,and the agitating power is 105.68 W. The results of simulation analysis are successfully applied in the factory, and the consistency between the simulation analysis conclusions and the on-site test results is verified at the same time.
KeyWords AITranslate
1Mohsen Ostad Shabani,Ali Mazahery,Mehdi Alizadeh,Ali Asghar Tofigh,Mohammad Reza Rahimipour,Mansour Razavi,Alireza Kolahi.Computational fluid dynamics(CFD) simulation of effect of baffles on separation in mixer settler[J].矿业科学技术学报:英文版,2012,22(5):703-706. 被引量:11
2逄启寿,曾文星.稀土萃取三层搅拌桨不同插入深度对搅拌的影响[J].湿法冶金,2013,32(1):61-63. 被引量:8
3吴富姬.搅拌混合槽内混合过程的数值模拟[J].湿法冶金,2014,33(4):328-331. 被引量:7
4逄启寿,谢明春.萃取混合澄清槽混合过程的数值模拟[J].有色金属:冶炼部分,2012(6):44-46. 被引量:11
5徐金,逄启寿,郜飘飘,罗松.双层桨搅拌槽的混合过程研究[J].中国有色冶金,2017,46(1):46-49. 被引量:7
6逄启寿,邓华军.三层桨搅拌槽内三维流场的数值模拟[J].有色金属:冶炼部分,2012(7):40-43. 被引量:10
7徐水太.赣州稀土产业可持续发展的问题与对策研究[J].江西理工大学学报,2014,35(4):47-51. 被引量:26
1闫光礼,冯羽生,逄启寿.搅拌桨叶距槽底距离对导流筒稀土搅拌槽搅拌特性的影响分析[J].有色金属:选矿部分,2019,0(6):82-88. 被引量:2
2冯羽生,严少卿.管式稀土萃取槽中搅拌桨转速优选研究[J].现代矿业,2021,37(4):149-151. 被引量:1
1冯羽生,严少卿.管式稀土萃取槽中搅拌桨转速优选研究[J].现代矿业,2021,37(4):149-151. 被引量:1
2逄启寿,万福兴,王高平.档板结构对重稀土圆筒式萃取槽三维流场的影响[J].厦门大学学报:自然科学版,2022,61(2):207-214.
1堡盟:绝对值编码器EAL580[J].今日制造与升级,2018,0(8):57-57.
2屈彬彬,张莉,王富华.考虑真空泵变工况影响的凝汽器性能数值计算[J].动力工程学报,2018,38(8):640-644. 被引量:3
3郏国有.关于盐水精制的佳化工艺[J].中国氯碱,1987,0(11):25-25.
4何达,汪琳,刘如铁,王铸博,熊翔,邹俭鹏.烧结铜基多孔毛细芯的孔隙特征及性能[J].粉末冶金材料科学与工程,2018,23(4):389-397. 被引量:4
5李龙贤,林奇燕,丁振晓.诱导轮空化流场数值计算及实验研究[J].真空与低温,2018,24(4):251-258. 被引量:3
Basic Information:
DOI:
Chinese Library Classification Number:TF804.2[冶金工程—有色金属冶金]
Citation Information:
Using a 200 L front chamber extraction tank without batiles as the model,and based on the dis- tance of the original agitator from the bottom of the mixing chamber (installation depth) b= 60 mm, the mixing process of feed liquid and P507 in the rare earth mixing chamber was simulated at 5 mm intervals through fluid dynamics Fluent software. Suction pressure, suction flow velocity and agitating power were used as evaluation criteria to analyze the effect of installation depth on suction performance of the agitator through the simulation analysis with different agitator installation depth. The optimized installation depth b = 50 mm is determined,which provides theoretical guidance for on-site debugging and installation of agita- tors. The results from simulation analysis show that when the installation depth keeps 50 mm,the suction negative pressure is --140.2 Pa, the suction flow velocity is 1.25 m/s,and the agitating power is 105.68 W. The results of simulation analysis are successfully applied in the factory, and the consistency between the simulation analysis conclusions and the on-site test results is verified at the same time.
quote
| GB/T 7714-2015 | [1] FENG Yu-sheng, PANG Qi-shou, YUAN Juan-di. Study on Installation Depth Optimization of the Agitator in the Rare Earth Extraction Tank without Baffles[J]. Rare Metals and Cemented Carbides, 2018(5): 13-17. |
| MLA | [1] FENG Yu-sheng, et al., "Study on Installation Depth Optimization of the Agitator in the Rare Earth Extraction Tank without Baffles." Rare Metals and Cemented Carbides, no. 5, 2018, pp. 13-17. |
| APA | [1] FENG Yu-sheng, PANG Qi-shou, & YUAN Juan-di. (2018). Study on Installation Depth Optimization of the Agitator in the Rare Earth Extraction Tank without Baffles. Rare Metals and Cemented Carbides(5), 13-17. |
| IEEE | [1] FENG Yu-sheng, PANG Qi-shou, and YUAN Juan-di, "Study on Installation Depth Optimization of the Agitator in the Rare Earth Extraction Tank without Baffles," Rare Metals and Cemented Carbides, no. 5, pp. 13-17, 2018. keywords: {rare earth extraction tank;agitator;installation depth;suction performance;numerical simulation;Fluent software} |